| 晶体取向对激光快凝重熔区组织形态的影响 |
| 杨森 黄卫东 刘文今 苏云鹏 周尧和 |
| 清华大学机械工程系;北京100084 |
|
引用本文:
杨森; 黄卫东; 刘文今; 苏云鹏; 周尧和 . 晶体取向对激光快凝重熔区组织形态的影响[J]. 金属学报, 2001, 37(6): 571-574 .
[1] Singh J. J Mater Sci, 1994; 29: 5232 [2] Zimmerman M, Carrad M, Gremaud M, Kurz W. MaterSet Eng. 1991; 134A: 1268 [3] Gill S C, Zimmerman M, Kurz W. Acta Metall Mater,1992; 40: 2895 [4] Zimmerman M, Carrad M, Kurz W. Acta Metall Mater,1990; 38: 2586 [5] Mudali U K, Dayal R K. J Mater Eng Perf,1992; 1: 341 [6] Stewart J, Wells D B, Scott P M, Bransden A S. Corro-sion,1990; 46: 618 [7] Huang W D, Mao Z Y, Zhou Y H. Acta Metall Sin, 1986;22B: 240(黄卫东,毛志英,周尧和金属学报,1986;22B:240) [8] Yang Sen, Ph.D Thesis, Xi'an: Northwestern Polytechni-cal University, 2000(杨森.西安:西北工业大学博士学位论文,2000) [9] Chong E, Wilcox W R. J Crystal Growth, 1974; 21: 135 [10] Flemings F C. Solidification Processing, New York:Mcgraw-Hill, 1974; 72 [11] Huang W D, Master Thesis, Xi'an: Northwestern Poly-technical University, 1984(黄卫东:西安:西北工业大学硕士学位论文,1984) [12] Kurz W, Fisher D J, Fundamentals of Solidification, Ae-dermannsdorf: Trans Tech Pub. 1984: 67; |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|