| Zr-Al-Ni-Cu块体非晶合金的成分设计与微结构表征 |
| 陈伟荣 王英敏 羌建兵 董闯 |
| 大连理工大学材料工程系;大连116024 |
|
引用本文:
陈伟荣; 王英敏; 羌建兵; 董闯 . Zr-Al-Ni-Cu块体非晶合金的成分设计与微结构表征[J]. 金属学报, 2002, 38(4): 421-426 .
[1] Inoue A, Zhang T, Masumoto T. Mater Trans JIM, 1990;31: 177 [2] Inoue A, Zhang T. Mater Trans JIM. 1996; 37: 185 [3] Zhang T, Inoue A. Mater Trons JIM, 1998; 39: 857 [4] Inoue A, Zhang T, Masumoto T. J Non Cryst Solids,1993; 156-158: 473 [5] Johnson W L. Mater Sci Forum, 1996; 225-227: 35 [6] Desre P J. Mater Trans JIM, 1997; 38: 583 [7] Nagel S R, Tauc J. Phys Reu Lett, 1975; 35. 380 [8] Dong C, Perrot A, Dubois J M, Belin E. Mater Sci Forum,1994; 150-151: 403 [9] Koster U, Meinhardt J, Roos S, Busch R. Mater Sci Eng,1997; 226-228A: 995 [10] Shek C H, Wang Y M, Dong C. Mater Sci Eng, 2000;291A: 78 [11] Pettifor D G. J Phys F: Metal Phys, 1977; 7: 613 [12] Wang Y M. Qiang J B, Xu W P, Dong C, Wong C H,Shek C H. J Mater Res. in press [13] Zhang T, Inoue A, Masumoto T. Mater Trans JIM, 1991;32: 1005 [14] Chen H S. Acta Metall, 1974; 22: 1505 [15] Inoue A, Zhang T, Nishiyama N, Ohba K. Masumoto T.Mater Trans JIM, 1993: 34. 1234 [16] Inoue A, Zhang T, Kim Y H. Mater Trans JIM, 1997: 38:749 [17] Zhang T, Inoue A. Mater Trans JIM. 1998: 39. 1230M |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|