| Ti-Al基合金中的Hall-Petch关系及影响因素分析 |
| 唐建成 黄伯云 贺跃辉 刘文胜 周科朝 |
| 中南大学粉末冶金国家重点实验室;长沙410083 |
|
引用本文:
唐建成; 黄伯云; 贺跃辉; 刘文胜; 周科朝 . Ti-Al基合金中的Hall-Petch关系及影响因素分析[J]. 金属学报, 2002, 38(4): 365-368 .
[1] Ward C M, Froes F H. JOM, 1994; 46: 28 [2] Huang S C. Scr Metall, 1988; 22: 1885 [3] Dimiduk D M, Hazzledine P M, Parthasarthy T A, Sesha-giri S, Mendiratta M G. Metall Mater Trans, 1998; 29A:37 [4] Liu C T, Schneibel J H, Maziasz P J, Wright J L, EastonD S. Intermetallics, 1996; 4: 429 [5] Morris M A, Leboeuf M. Mater Sci Eng, 1997; 224A: 1 [6] Bohn B, Klassen T, Bormann R. Acta Mater, 2001; 49:299 [7] Vasudevan V K, Court S A, Kurath P, Fraser H L. ScrMetall, 1989; 23: 467 [8] Chu W Y, Thompson A W. Scr Metall Mater, 1991; 25:641 [9] Kumpfert J, Kim Y W, Dimimduk D M. Mater Sci Eng,1995; 192/192A: 465 [10] Chen L H, Huang B Y, Qu X H. Chin J Nonferrous Met,1996: 6: 120(陈伶辉.黄伯云.曲选辉 中国有色金属学报.1996;6:120) [11] Xie Y X, Cao M Z, Xu Z J. Acta Metall Sin, 1993; 29:160(谢英秀、曹名洲.徐曾基.金属学报、1993(29:160) [12] Tang J C, Huang B Y, He Y H, Liu W S. Trans NonferrousMet Soc Chin, 2000; 10: 183 [13] Zhong J G. Error Theory and Datum Handling. Beijing:Chemical Industry Press, 1992: 342(钟继贵 误差理论与数据处理,北京:化学工业出版社.1992:342) [14] Mereer C, Soboyejo W O. Scr Mater, 1996; 35:17 [15] Yun J H, Oh M H, Nam S W, Wee D M, Inui H, Yam-aguchi M. Mater Sci Eng, 1997; 239A: 702 [16] Tang J C, Huang B Y, He Y H, Xie K. Trans NonferrousMet Soc Chin, 1999; 9: 692 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|