| Al--Bi难混溶合金快速连续凝固的实验研究 |
| 何 杰 赵九洲 王晓峰 李中原 |
| 中国科学院金属研究所; 沈阳 110016 |
|
| An Experimental Study of the Rapid Continuous Solidification of Al—Bi Immiscible Alloy |
| HE Jie; ZHAO Jiuzhou; WANG Xiaofeng; LI Zhongyuan |
| Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
何杰; 赵九洲; 王晓峰; 李中原 . Al--Bi难混溶合金快速连续凝固的实验研究[J]. 金属学报, 2006, 42(1): 67-72 .
,
,
,
.
An Experimental Study of the Rapid Continuous Solidification of Al—Bi Immiscible Alloy[J]. Acta Metall Sin, 2006, 42(1): 67-72 .
[1]Guo J J,Cui H B,Su Y Q,Bi W S,Jia J,Fu H Z.Spec Cast Nonfer Alloys,2004;(1):1(郭景杰,崔红保,苏彦庆,毕维生,贾均,傅恒志.特种铸造及有色合金,2004;(1):1) [2]Zheng H X,Xie H,Chen Z L,Yang G C,Guo X F.Chin J Rare Met,2002;26(1):15(郑红星,谢辉,陈倬麟,杨根仓,郭学锋.稀有金属,2002;26(1):15) [3]Zhu D Y,Yang X H,Han X J,Wei B B.The Chin J Nonfer Met,2003;13:32(朱定一,杨晓华,韩秀君,魏炳波.中国有色金属学报,2003;13:328) [4]Rudrakshi G B,Srivastava V C,Pathak J P,Ojha S N.Mater Sci Eng,2004;A383:30 [5]Yang S,Liu W J.J Mater Sci,2001;36:5351 [6]Zhang H W,Xian A P.Acta Metall Sin,1999;35:1187(张宏闻,冼爱平.金属学报,1999;35:1187) [7]Guo J J,Liu Y,Su Y Q,Jia J,Ding H S,Zhao J Z.Mater Sci Technol,2002;18:71286 [8]Alkemper J,Ratke L.Z Metallkd,1994;85:365 [9]Wu M H,Ludwig A,Ratke L.Modell Simul Mater Sci Eng,2003;11:755 [10]Zhao J Z,Ratke L.Scr Mater,2004;50:543 [11]Ratke L,Diefenbach S.Mater Sci Eng,1995;R15:263 [12]Jia J,Zhao J Z,Guo J J,Liu Y.Immiscible Alloy and Preparation Technology.Harbin:Harbin Institute of Technology Press,2002:1(贾均,赵九洲,郭景杰,刘源.难混溶合金及其制备技术.哈尔滨:哈尔滨工业大学出版社,2002:1) [13]He J,Zhao J Z.Acta Metall Sin,2005;41:407(何杰,赵九洲.金属学报,2005;41:407) [14]He J,Zhao J Z.Mater Sci Technol,2005;21:759 [15]He J,Zhao J Z.Mater Sci Eng,2005;A404:85 [16]He J,Zhao J Z,Wang X F,Gao L L.Metall Mater Frans, ??2005;36A:2449 [17]Zhao J Z,He J,Hu Z Q,Laoke L.Z Metallkd,1998;89:241 [18]Kamio A,Kumai S,Tezuka H.Mater Sci Eng,1991;A146:105 [19]Derby B,Favier J J.Acta Metall,1983;31:1123 [20]Ratke L,Korekt G,Drees S.ESA Symposium Proceedings on Space Station Utilisation,1996:385 [21]Zhao J Z,Ratke L.Z Metallkd,1998;89:241 [22]Zhao J Z,Ratke L.Scr Mater,1998;39:181G |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|