| SiCp/6061Al合金复合材料的单轴循环变形行为及其时间相关特性 |
| 康国政 刘宇杰 |
| 西南交通大学应用力学与工程系; 成都 610031 |
|
| Uniaxial Cyclic Deformation of Sicp/6061Al Alloy Composites and Its Time--Dependence |
| KANG Guozheng; LIU Yujie |
| Department of Applied Mechanics and Engineering; Southwest Jiaotong University; Chengdu 610031 |
引用本文:
康国政; 刘宇杰 . SiCp/6061Al合金复合材料的单轴循环变形行为及其时间相关特性[J]. 金属学报, 2006, 42(1): 59-66 .
,
.
Uniaxial Cyclic Deformation of Sicp/6061Al Alloy Composites and Its Time--Dependence[J]. Acta Metall Sin, 2006, 42(1): 59-66 .
[1]Ruggles M D,Krempl E.J Mech Phys Solids,1990;38:575 [2]Delobelle P,Robinet P,Bocher L.Int J Plast,1995;11:295 [3]Kobayashi M,Ohno N,Igari T.Int J Plast,1998;14:355 [4]Mizuno M,Mima Y,Abdel-Karim M,Ohno N.ASME J Eng Mater Technol,2000;122(1):29 [5]Kang G Z,Gao Q,Cai LX,Yang X J,Sun Y F.Acta Metall Sin,2000;36:497(康国政,高庆,蔡力勋,杨显杰,孙亚芳.金属学报,2D00;35:497 [6]Kang G Z,Gao Q,Yang X J.Int J Mech Sci,2002;44:1645 [7]Kang G Z,Gao Q,Cai L X,Sun Y F.Nucl Eng Des,2002;216:13 [8]Kang G Z,Sun Y F,Zhang J,Kan Q H.Acta Metall Sin,2005;41:277(康国政,孙亚芳,张娟,阚前华.金属学报,2005;41:277 [9]Chaboche J L.Int J Plast,1991;7:661 [10]Ohno N,Wang J D.Int J Plast,1993;9:375 [11]Chen X,Jiao R,Kim,K S.Int J Plast,2005;21:161 [12]Ohno N,Abdel-Karim M.ASME J Eng Mater Technol,2000;122(1):35 [13]Chen X,Jiao R.Int J Plast,2004;20:871 [14]Kang G Z,Gao Q,Yang X J.Mech Mater,2002;34:521 [15]Gao Q,Kang G Z,Yang X J.Theor Appl Fract Mech,2003;40:105 [16]Kang G Z.Mech Mater,2004;36:299 [17]Han N L,Wang Z G,Yang J M,Zhang G D.Mater Sci Eng,2002;A337:140 [18]Srivatsan T S,Meslet A H,Vasudevan V K.Int J Fatigue,2005;27:357 [19]Han N L,Wang Z G,Zhang G D,Lui L.Mater Lett,1999;38(1):70 [20]Xia Z,Ellyin F.Int J Fatigue,1998;20:51 [21]Han N L,Wang Z G,Wang W L,Zhang G D,Shi C X.Comput Sci Technol,1999;59(1):147? |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|