| Al-Cu-Zn合金单相凝固过程中的溶质截留 |
| 陈福义 介万奇 |
| 西北工业大学凝固技术国家重点实验室; 西安710072 |
|
引用本文:
陈福义; 介万奇 . Al-Cu-Zn合金单相凝固过程中的溶质截留[J]. 金属学报, 2003, 39(9): 943-947 .
[1] Aziz M J. J Appl Phys, 1982; 53: 1158 [2] Aziz M J. Metall Mater Trans, 1996; 27A: 671 [3] Kar A, Mazumder J. Acta Metall Mater, 1992; 40: 1873 [4] Aziz M J, Kaplan T. Acta Metall, 1988; 36: 2335 [5] Aziz M J, Boettinger W J. Acta Metall Mater, 1994; 42:527 [6] Aziz M J. Mater Sci Eng, 1997; A226: 255 [7] Kittl J A, Aziz M J, Brunco D P, Thompson M O. J CrystGrowth, 1995; 148: 172 [8] Smith P M, Aziz M J. Acta Meatll Mater, 1994; 42: 3515 [9] Carrard M, Gremaud M, Zimmermann, Kurz W. ActaMetall Mater, 1992; 40: 983 [10] Boettinger W J, Coriell S R, Sekerka R F. Mater Sci Eng,1984; 65: 27 [11] Chen F, Jie W. Acta Metall Sin, 2003; 39: 597(陈福义,介万奇.金属学报, 2003;39:597) [12] Livio B, Carlo A, Marcello B. J Alloys Comp, 1997; 247: 172 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|