| 等离子体熔融钛与羟基磷灰石混合粉颗粒的形态和相组成 |
| 吕宇鹏 李士同 梁栋科 朱瑞富 李木森 雷廷权 |
| 山东大学材料科学与工程学院;济南250061 |
|
引用本文:
吕宇鹏; 李士同; 梁栋科; 朱瑞富; 李木森; 雷廷权 . 等离子体熔融钛与羟基磷灰石混合粉颗粒的形态和相组成[J]. 金属学报, 2002, 38(12): 1292-1294 .
[1] Ducheyne P. J Biomed Mater Res: Appl Biomater, 1987;21: 219 [2] Gross K A, Berndt C C. Key Eng Mater, 1991; 53-55: 124 [3] Lacefield W R, Hench L L. Biomaterials, 1986; 7: 104 [4] Barth E, Hero H. Biomaterials, 1986; 7: 273 [5] Ellies L G, Nelson D G A, Featherstone J D B. Biomaterials, 1992; 13: 313 [6] Lamy D, Pierre A C, Heimann R B. J Mater Res, 1996;11: 680 [7] Kyeck S, Pemer P. Mater Sci Forum, 1999; 308-311: 368 [8] Tsui Y C, Doyle C, Clyne T W. Biomaterials, 1998; 19: 2015A |
|