| 基于晶粒长大拓扑依赖性的准稳态三维晶粒尺寸分布 |
| 王 超;刘国权;于海波 |
| 北京科技大学材料科学与工程学院; 北京 100083 |
|
| QUASI-STATIONARY THREE-DIMENSIONAL GRAIN SIZE DISTRIBUTION WITH TOPOLOGY DEPENDENCY OF GRAIN GROWTH |
| WANG Chao; LIU Guoquan; YU Haibo |
| School of Materials Science & Engineering; University of Science &Technology Beijing; Beijing 100083 |
引用本文:
王超; 刘国权; 于海波 . 基于晶粒长大拓扑依赖性的准稳态三维晶粒尺寸分布[J]. 金属学报, 2004, 40(12): 1233-1237 .
,
,
.
QUASI-STATIONARY THREE-DIMENSIONAL GRAIN SIZE DISTRIBUTION WITH TOPOLOGY DEPENDENCY OF GRAIN GROWTH[J]. Acta Metall Sin, 2004, 40(12): 1233-1237 .
[1] Hillert M. Acta Metall, 1965; 13: 227 [2] Atkinson H V. Acta Metall, 1988; 36: 469 [3] Mullins W W. J Appl Phys, 1956; 27: 900 [4] Fradkov V E, Udler D. Adv Phys,1994;43:739 [5] Yu H B. PhD Thesis, University of Science and Technology Beijing, 1997 (于海波.北京科技大学博士学位论文,1997) [6] Yu H B, Liu G Q. Chin Sci Bull, 1996; 41: 2000 (于海波,刘国权.科学通报,1996;41:2000) [7] Liu G Q, Yu H B, Song X Y, Qin X G. Mater Design,2001; 22: 33 [8] Wang C, Liu G Q. Sci Chin, 2004;47E:112 [9] Brown L C. Acta Metall, 1989; 37:71 [10] Coughlan S D, Fortes M A. Scr Metall Mater, 1993; 28:1471 [11] Weygand D, Brechet Y. Philos Mag, 1999; 79B: 703 [12] Wakai F, Enomoto N, Ogawa H. Acta Mater, 2000; 48:1297 [13] Krill C E, Chen L Q. Acta Mater, 2002; 50: 3057 [14] Song X Y, Liu G Q, Gu N J. Scr Mater, 2000; 43: 355T |
|