| 金属高Miller指数表面能的分子动力学研究 |
| 王晓春 贾 瑜 姚乾凯 王 飞 马健新 胡 行 |
| 郑州大学物理工程学院材料物理重点实验室; 郑州 450052 |
|
| Molecular Dynamics Simulation of the Surface Energies of High—Index Surfaces in Metals |
| WANG Xiaochun; JIA Yu; YAO Qiankai;WANG Fei; MA Jianxin; HU Xing |
| School of Physical Engineering and Key Laboratory of Physical Materials;Zhengzhou University; Zhengzhou 450052 |
引用本文:
王晓春; 贾瑜; 姚乾凯; 王飞; 马健新; 胡行 . 金属高Miller指数表面能的分子动力学研究[J]. 金属学报, 2004, 40(6): 589-.
,
,
,
,
,
.
Molecular Dynamics Simulation of the Surface Energies of High—Index Surfaces in Metals[J]. Acta Metall Sin, 2004, 40(6): 589-.
[1] Yi S P, Liu R S. Acta Metall Sin, 2000; 36: 1030(易双萍, 刘让苏.金属学报; 2000; 36: 1030) [2] Liang H Y, Ni X G. Acta Metall Sin, 2001; 37: 833(梁海弋, 倪向贵. 金属学报, 2001; 37: 833) [3] Li J Z, Liu H. Acta Metall Sin, 2001; 37: 1013(李忠吉, 刘辉. 金属学报,2001;37: 1013) [4] Zhuang J, Liu L. Acta Phys Sin, 1997; 46: 2418(庄军, 刘磊. 物理学报, 1997; 46: 2418) [5] Daw M, Baskes M. Phys Rev B, 1984; 29: 6443 [6] Foiles S, Baskes M, Daw M. Phys Rev B, 1986; 33: 7983 [7] Barral M A, Llois A M. Phys Rev B, 2000; 62: 12668 [8] Nakanishi S, Umezawa K. Phys Rev B, 2000; 62: 13136 [9] Kumikov V K, Khokonov Kh B. J Appl Phys, 1983; 54:1346 [10] Zhuang J, Liu L. Phy Rev B, 1999; 59: 13278 [11] Udler D, Seidman D N. Phys Rev B, 1996; 54: 11133 [12] Vitos L, Ruban A V, Skriver H L. Philos Mag B, 1998;78: 487 [13] Katagiri M, Nozue Y. Mater Sci Eng A, 1996; 217/218:112 [14] Alden M, Mirbt S. Phys Rev B, 1992; 46: 6303 [15] Rokuta E, Hasegasa Y. Surf Sci, 1999; 427-428: 97 [16] Daniel J Gaspar, Aubrey T. J Chem Phys, 1998; 109: 6947 [17] Tian Y, Lin K W, Jona F. Phys Rev B, 2000; 62: 12844 [18] Reinecke N, Reiter S, Vetter S. Appl Phys A, 2002; 75: 1 [19] Roth M, Pickel M, Wang J. Appl Phys B, 2002; 74: 661 [20] Wolf D. Surf Sci, 1990; 226: 389 [21] Mutasa B, Farkas D. Surf Sci, 1998; 415: 312 [22] Voter A, Chen S. Mater Res Soc Symp Proc, 1987; Vol.82: 175 [23] Farkas D, Mutasa B, Vailhe C. Model Simul Mater Sci Eng, 1995; 3: 201 [24] Vitos L, Ruban A V, Skriver H L, Kollar J. Surf Sci, 1998;411: 186 [25] Todd J R, Andrew E D. Phys Rev B, 1989; 39: 9967 [26] Sinnoott S B, Stave M S, Raeker T J. Phys Rev B, 1991;44: 8927 [27] Kallinteris G C, Papanicolaou N I, Evangelakis G A. Phys Rev B, 1997; 55: 2150 [28] Mishin Y, Farkas D. Phys Rev B, 1999; 59: 3393 [29] Rodriguez A M, Bozzolo G, Ferrante J. Surf Sci, 1993;289: 100 [30] Chen S P, Voter A F. Surf Sci Lett, 1991; 244: L107 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|