| 原位激光定向能量沉积NiTi形状记忆合金的微观结构和力学性能 |
陈斐1,2,3( ), 邱鹏程1, 刘洋1,2, 孙兵兵4, 赵海生4, 沈强1 |
1.武汉理工大学 材料复合新技术国家重点实验室 武汉 430070 2.武汉理工大学 材料科学与工程国际化示范学院(材料与微电子学院) 武汉 430070 3 湖北隆中实验室 襄阳 441000 4 航发优材(镇江)增材制造有限公司 镇江 212132 |
|
| Microstructure and Mechanical Properties of NiTi Shape Memory Alloys by In Situ Laser Directed Energy Deposition |
CHEN Fei1,2,3( ), QIU Pengcheng1, LIU Yang1,2, SUN Bingbing4, ZHAO Haisheng4, SHEN Qiang1 |
1.State Key Laboratory of Advance e Technology for Materials Synthesis and Processing, Wuhan University of Technology, Wuhan 430070, China 2.International School of Materials Science and Engineering (School of Materials and Microelectronics), Wuhan University of Technology, Wuhan 430070, China 3 Hubei Longzhong Laboratory, Xiangyang 441000, China 4 HFYC (Zhenjiang) Additive Manufacturing Co., Ltd., Zhenjiang 212132, China |
引用本文:
陈斐, 邱鹏程, 刘洋, 孙兵兵, 赵海生, 沈强. 原位激光定向能量沉积NiTi形状记忆合金的微观结构和力学性能[J]. 金属学报, 2023, 59(1): 180-190.
Fei CHEN,
Pengcheng QIU,
Yang LIU,
Bingbing SUN,
Haisheng ZHAO,
Qiang SHEN.
Microstructure and Mechanical Properties of NiTi Shape Memory Alloys by In Situ Laser Directed Energy Deposition[J]. Acta Metall Sin, 2023, 59(1): 180-190.
| 1 |
Elahinia M H, Hashemi M, Tabesh M, et al. Manufacturing and processing of NiTi implants: A review [J]. Prog. Mater. Sci., 2012, 57: 911
doi: 10.1016/j.pmatsci.2011.11.001
|
| 2 |
Marattukalam J J, Singh A K, Datta S, et al. Microstructure and corrosion behavior of laser processed NiTi alloy [J]. Mater. Sci. Eng., 2015, C57: 309
|
| 3 |
Cho G B, Kim K W, Ahn H J, et al. Applications of Ti-Ni alloys for secondary batteries [J]. J. Alloys Compds., 2008, 449: 317
doi: 10.1016/j.jallcom.2006.01.129
|
| 4 |
Lu B W, Cui X F, Liu E B, et al. Influence of microstructure on phase transformation behavior and mechanical properties of plasma arc deposited shape memory alloy [J]. Mater. Sci. Eng., 2018, A736: 130
|
| 5 |
Krishna B V, Bose S, Bandyopadhyay A. Laser processing of net-shape NiTi shape memory alloy [J]. Metall. Mater. Trans., 2007, 38A: 1096
|
| 6 |
Yao C, Yin F X, Ji P G, et al. Effects of grain refinement on the microstructures and damping behaviors of a Cu-Al-Ni-Mn-Ti shape memory alloy [J]. Intermetallics, 2021, 138: 107315
doi: 10.1016/j.intermet.2021.107315
|
| 7 |
Marattukalam J J, Balla V K, Das M, et al. Effect of heat treatment on microstructure, corrosion, and shape memory characteristics of laser deposited NiTi alloy [J]. J. Alloys Compds., 2018, 744: 337
doi: 10.1016/j.jallcom.2018.01.174
|
| 8 |
Haberland C, Elahinia M, Walker J M, et al. On the development of high quality NiTi shape memory and pseudoelastic parts by additive manufacturing [J]. Smart Mater. Struct., 2014, 23: 104002
doi: 10.1088/0964-1726/23/10/104002
|
| 9 |
Otubo J, Rigo O D, Neto C M, et al. The effects of vacuum induction melting and electron beam melting techniques on the purity of NiTi shape memory alloys [J]. Mater. Sci. Eng., 2006, A438-440: 679
|
| 10 |
Saedi S, Turabi A S, Andani M T, et al. Thermomechanical characterization of Ni-rich NiTi fabricated by selective laser melting [J]. Smart Mater. Struct., 2016, 25: 035005
|
| 11 |
Zhao C Y, Liang H L, Luo S C, et al. The effect of energy input on reaction, phase transition and shape memory effect of NiTi alloy by selective laser melting [J]. J. Alloys Compds., 2020, 817: 153288
doi: 10.1016/j.jallcom.2019.153288
|
| 12 |
Zhang D Z, Li Y Z, Wang H, et al. Ultrasonic vibration-assisted laser directed energy deposition in-situ synthesis of NiTi alloys: Effects on microstructure and mechanical properties [J]. J. Manuf. Processes, 2020, 60: 328
doi: 10.1016/j.jmapro.2020.10.058
|
| 13 |
Frazier W E. Metal additive manufacturing: A review [J]. J. Mater. Eng. Perform., 2014, 23: 1917
doi: 10.1007/s11665-014-0958-z
|
| 14 |
Beyer C. Strategic implications of current trends in additive manufacturing [J]. J. Manuf. Sci. Eng., 2014, 136: 064701
|
| 15 |
Guo N N, Leu M C. Additive manufacturing: Technology, applications and research needs [J]. Front. Mech. Eng., 2013, 8: 215
doi: 10.1007/s11465-013-0248-8
|
| 16 |
Hassan M R, Mehrpouya M, Dawood S. Review of the machining difficulties of nickel-titanium based shape memory alloys [J]. Appl. Mech. Mater., 2014, 564: 533
doi: 10.4028/www.scientific.net/AMM.564.533
|
| 17 |
Kaynak Y. Machining and phase transformation response of room-temperature austenitic NiTi shape memory alloy [J]. J. Mater. Eng. Perform., 2014, 23: 3354
doi: 10.1007/s11665-014-1058-9
|
| 18 |
Liang X L, Liu Z Q, Wang B. State-of-the-art of surface integrity induced by tool wear effects in machining process of titanium and nickel alloys: A review [J]. Measurement, 2019, 132: 150
doi: 10.1016/j.measurement.2018.09.045
|
| 19 |
Kaynak Y, Karaca H E, Noebe R D, et al. The effect of active phase of the work material on machining performance of a NiTi shape memory alloy [J]. Metall. Mater. Trans., 2015, 46A: 2625
|
| 20 |
Kaynak Y, Huang B, Karaca H E, et al. Surface characteristics of machined NiTi shape memory alloy: The effects of cryogenic cooling and preheating conditions [J]. J. Mater. Eng. Perform., 2017, 26: 3597
doi: 10.1007/s11665-017-2791-7
|
| 21 |
Venkatalaxmi A, Padmavathi B S, Amaranath T. A general solution of unsteady Stokes equations [J]. Fluid Dyn. Res., 2004, 35: 229
doi: 10.1016/j.fluiddyn.2004.06.001
|
| 22 |
Bormann T, Schumacher R, Müller B, et al. Tailoring selective laser melting process parameters for NiTi implants [J]. J. Mater. Eng. Perform., 2012, 21: 2519
doi: 10.1007/s11665-012-0318-9
|
| 23 |
Bandyopadhyay A, Krishna B V, Xue W C, et al. Application of laser engineered net shaping (LENS) to manufacture porous and functionally graded structures for load bearing implants [J]. J. Mater. Sci. Mater. Med., 2009, 20(suppl.1) : S29
|
| 24 |
Vamsi Krishna B, Xue W C, Bose S, et al. Functionally graded Co-Cr-Mo coating on Ti-6Al-4V alloy structures [J]. Acta Biomater., 2008, 4: 697
pmid: 18054298
|
| 25 |
Lu H Z, Yang C, Luo X, et al. Ultrahigh-performance TiNi shape memory alloy by 4D printing [J]. Mater. Sci. Eng., 2019, A763: 138166
|
| 26 |
Hassanin H, Abena A, Elsayed M A, et al. 4D printing of NiTi auxetic structure with improved ballistic performance [J]. Micromachines (Basel), 2020, 11: 745
|
| 27 |
Wang C, Tan X P, Du Z, et al. Additive manufacturing of NiTi shape memory alloys using pre-mixed powders [J]. J. Mater. Process. Technol., 2019, 271: 152
doi: 10.1016/j.jmatprotec.2019.03.025
|
| 28 |
Walker J M, Haberland C, Taheri Andani M, et al. Process development and characterization of additively manufactured nickel-titanium shape memory parts [J]. J. Intell. Mater. Syst. Struct., 2016, 27: 2653
doi: 10.1177/1045389X16635848
|
| 29 |
Shayesteh Moghaddam N, Saghaian S E, Amerinatanzi A, et al. Anisotropic tensile and actuation properties of NiTi fabricated with selective laser melting [J]. Mater. Sci. Eng., 2018, A724: 220
|
| 30 |
Saedi S, Shayesteh Moghaddam N, Amerinatanzi A, et al. On the effects of selective laser melting process parameters on microstructure and thermomechanical response of Ni-rich NiTi [J]. Acta Mater., 2018, 144: 552
doi: 10.1016/j.actamat.2017.10.072
|
| 31 |
Zhang B C, Chen J, Coddet C. Microstructure and transformation behavior of in-situ shape memory alloys by selective laser melting Ti-Ni mixed powder [J]. J. Mater. Sci. Technol., 2013, 29: 863
doi: 10.1016/j.jmst.2013.05.006
|
| 32 |
Wang X B, Kustov S, Van Humbeeck J. A short review on the microstructure, transformation behavior and functional properties of NiTi shape memory alloys fabricated by selective laser melting [J]. Materials (Basel), 2018, 11: 1683
doi: 10.3390/ma11091683
|
| 33 |
Ma J, Franco B, Tapia G, et al. Spatial control of functional response in 4D-printed active metallic structures [J]. Sci. Rep., 2017, 7: 46707
doi: 10.1038/srep46707
pmid: 28429796
|
| 34 |
Saedi S, Turabi A S, Andani M T, et al. The influence of heat treatment on the thermomechanical response of Ni-rich NiTi alloys manufactured by selective laser melting [J]. J. Alloys Compds., 2016, 677: 204
doi: 10.1016/j.jallcom.2016.03.161
|
| 35 |
Otsuka K, Ren X. Physical metallurgy of Ti-Ni-based shape memory alloys [J]. Prog. Mater. Sci., 2005, 50: 511
doi: 10.1016/j.pmatsci.2004.10.001
|
| 36 |
Li S, Hassanin H, Attallah M M, et al. The development of TiNi-based negative Poisson's ratio structure using selective laser melting [J]. Acta Mater., 2016, 105: 75
doi: 10.1016/j.actamat.2015.12.017
|
| 37 |
Taheri Andani M, Haberland C, Walker J M, et al. Achieving biocompatible stiffness in NiTi through additive manufacturing [J]. J. Intell. Mater. Syst. Struct., 2016, 27: 2661
doi: 10.1177/1045389X16641199
|
| 38 |
Fan G L, Chen W, Yang S, et al. Origin of abnormal multi-stage martensitic transformation behavior in aged Ni-rich Ti-Ni shape memory alloys [J]. Acta Mater., 2004, 52: 4351
doi: 10.1016/j.actamat.2004.06.002
|
| 39 |
Jiang S Y, Zhang Y Q. Microstructure evolution and deformation behavior of as-cast NiTi shape memory alloy under compression [J]. Trans. Nonferrous Met. Soc. China, 2012, 22: 90
doi: 10.1016/S1003-6326(11)61145-X
|
| 40 |
Taheri Andani M, Saedi S, Turabi A S, et al. Mechanical and shape memory properties of porous Ni50.1Ti49.9 alloys manufactured by selective laser melting [J]. J. Mech. Behav. Biomed. Mater., 2017, 68: 224
doi: 10.1016/j.jmbbm.2017.01.047
|
| 41 |
Kim J I, Miyazaki S. Effect of nano-scaled precipitates on shape memory behavior of Ti-50.9at.%Ni alloy [J]. Acta Mater., 2005, 53: 4545
doi: 10.1016/j.actamat.2005.06.009
|
| 42 |
Kim Y W, Do D. Shape memory characteristics of highly porous Ti-rich TiNi alloys [J]. Mater. Lett., 2016, 162: 1
doi: 10.1016/j.matlet.2015.09.101
|
| 43 |
Mohd Jani J, Leary M, Subic A, et al. A review of shape memory alloy research, applications and opportunities [J]. Mater. Des., 2014, 56: 1078
doi: 10.1016/j.matdes.2013.11.084
|
| 44 |
Sam J, Franco B, Ma J, et al. Tensile actuation response of additively manufactured nickel-titanium shape memory alloys [J]. Scr. Mater., 2018, 146: 164
doi: 10.1016/j.scriptamat.2017.11.013
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|