| 600 MPa级Nb-Ti微合金化高成形性元宝梁用钢的强化机制 |
惠亚军1,2( ), 潘辉1, 刘锟1, 李文远1, 于洋1, 陈斌1, 崔阳1 |
| 1 首钢技术研究院薄板研究所 北京 1000432 首钢总公司绿色可循环钢铁流程北京市重点实验室 北京 100043 |
|
| Strengthening Mechanism of 600 MPa Grade Nb-Ti Microalloyed High Formability Crossbeam Steel |
Yajun HUI1,2( ), Hui PAN1, Kun LIU1, Wenyuan LI1, Yang YU1, Bin CHEN1, Yang CUI1 |
1 Sheet Metal Research Institute, Shougang Research Institute of Technology, Beijing 100043, China 2 Beijing Key Laboratory of Green Recyclable Process for Iron & Steel Production, Shougang Group, Beijing 100043, China |
引用本文:
惠亚军, 潘辉, 刘锟, 李文远, 于洋, 陈斌, 崔阳. 600 MPa级Nb-Ti微合金化高成形性元宝梁用钢的强化机制[J]. 金属学报, 2017, 53(8): 937-946.
Yajun HUI,
Hui PAN,
Kun LIU,
Wenyuan LI,
Yang YU,
Bin CHEN,
Yang CUI.
Strengthening Mechanism of 600 MPa Grade Nb-Ti Microalloyed High Formability Crossbeam Steel[J]. Acta Metall Sin, 2017, 53(8): 937-946.
| [1] | Zhang P C, Wu H B, Tang D, et al.Dissolving behaviors of carbonitrides in Nb-V-Ti and V-Ti microalloying steels[J]. Acta Metall. Sin., 2007, 43: 753(张鹏程, 武会宾, 唐荻等. Nb-V-Ti和V-Ti微合金钢中碳氮化物的回溶行为[J]. 金属学报, 2007, 43: 753) | | [2] | Speer J G, Michael J R, Hansen S S.Carbonitride precipitation in niobium/vanadium microalloyed steels[J]. Metall. Trans., 1987, 18A: 211 | | [3] | Zheng L X, Li W Y, Zhai D Y.Analysis on fracture of the ingot beam of the heavy-duty dump truck[J]. Metall. Equipm., 2010, (5): 28(郑利霞, 李文颖, 翟大勇. 自卸车元宝梁断裂分析[J]. 冶金设备, 2010, (5): 28) | | [4] | Wu C L, Ma W R, Wang S, et al. Girder shaped like shoe-shaped gold ingot and vehicle frame assembly with same [P]. China Patents, CN204341193U, 2015(吴辰龙, 马维忍, 王珊等. 一种元宝梁以及具有该元宝梁的车架总成 [P]. 中国专利, CN204341193U, 2015) | | [5] | Li Y J.Finite element analysis of static-dynamic stress of heavy truck[J]. Autom. Eng., 1989, (1): 35(李玉娟. 超重型汽车车架静动态应力的有限元分析[J]. 汽车工程, 1989, (1): 35) | | [6] | Zhang Y, Zhang L, Xu Z J, et al.Simulation of heavy vehicle frame based on assembled structures and analysis on the frame fracture[J]. Comput. Simul., 2005, 22(12): 218(张勇, 张力, 徐宗俊等. 基于组合结构的重车车架建模仿真及断裂分析[J]. 计算机仿真, 2005, 22(12): 218) | | [7] | Yu C W.Finite elements simulation and optimization of heavy-duty truck's frame structure [D]. Changchun: Jilin University, 2005(余传文. 重型载货汽车车架结构的有限元仿真及优化 [D]. 长春: 吉林大学, 2005) | | [8] | Zou L, Yu H C, Jing J H.Finite element analysis of the frame of 6×4 heavy dump truck[J]. J. Hefei Univ. Technol.(Nat. Sci), 2007, 30(Suppl.): 43(邹琳, 于海昌, 景俊鸿. 6×4重型自卸车车架有限元分析[J]. 合肥工业大学学报(自然科学版), 2007, 30(增刊): 43) | | [9] | Xu B, Shang L P, Chen X J, et al. Reinforced heavy duty car wing girder [P]. China Patents, CN202911799U, 2013(徐斌, 尚利平, 陈学军等. 一种强化重型汽车元宝梁 [P]. 中国专利, CN202911799U, 2013) | | [10] | Song W X.Metallography [M]. Beijing: Metallurgical Industry Press, 1980: 1(宋维锡. 金属学[M]. 北京: 冶金工业出版社, 1980: 1) | | [11] | Wang Y M, Li M Y, Wei G, et al.Controlled Rolling of Steel and Controlled Cooling [M]. Beijing: Metallurgical Industry Press, 1995: 1(王有铭, 李曼云, 韦光等. 钢材的控制轧制和控制冷却 [M]. 北京: 冶金工业出版社, 1995: 1) | | [12] | Yong Q L, Li Y F, Sun Z B, et al.Second-phase on grain coarsening time and temperature[J]. Iron Steel, 1993, 28(9): 45(雍岐龙, 李永福, 孙珍宝等. 第二相与晶粒粗化时间及粗化温度[J]. 钢铁, 1993, 28(9): 45) | | [13] | Smith R M, Dunne D P.Structural aspects of alloy carbonitride precipitation in microalloyed steels[J]. Mater. Forum, 1988, 11: 166 | | [14] | Hong S G, Kang K B, Park C G.Strain-induced precipitation of Nb in Nb and Nb-Ti microalloyed HSLA steels[J]. Scr. Mater., 2002, 46: 163 | | [15] | Yi H L, Du L X, Wang G D, et al.New Ti-bearing high strength steel[J]. Chin. J. Mech. Eng., 2008, 44(8): 50(衣海龙, 杜林秀, 王国栋等, 一种新型含钛高强度钢[J], 机械工程学报, 2008, 44(8): 50) | | [16] | Dutta B, Valdes E, Sellars C M.Mechanism and kinetics of strain induced precipitation of Nb(C, N) in austenite[J]. Acta Metall. Mater., 1992, 40: 653 | | [17] | Poths R M, Higginson R L, Palmiere E J.Complex precipitation behaviour in a microalloyed plate steel[J]. Scr. Mater., 2001, 44: 147 | | [18] | Craven A J, He K, Garvie L A J, et al. Complex heterogeneous precipitation in titanium-niobium microalloyed Al-killed HSLA steels——I. (Ti, Nb)(C, N) particles[J]. Acta Mater., 2000, 48: 3857 | | [19] | Thillou V.Basic metal processing research institute report [R]. Pittsburgh, PA, USA: University of Pittsburgh, 1997 | | [20] | Yong Q L.The Second Phase in Steels [M]. Beijing: Metallurgical Industry Press, 2006: 175(雍岐龙. 钢铁材料中的第二相 [M]. 北京: 冶金工业出版社, 2006: 175) | | [21] | Yong Q L, Ma M T, Wu B R.Microalloyed steel——Physical and Mechanical Metallurgy [M]. Beijing: China Machine Press, 1989: 57(雍岐龙, 马鸣图, 吴宝榕. 微合金钢——物理和力学冶金 [M]. 北京: 机械工业出版社, 1989: 57) | | [22] | Wang R Z, Zhang H T.Strengthening mechanism of Nb and Ti complex microalloyed strip steel produced by thin slab casting and direct rolling process[J]. Acta Metall. Sin., 2007, 43: 1082(王瑞珍, 章洪涛. 薄板坯连铸连轧工艺生产的Nb、Ti复合微合金化热轧带钢的强化机制[J]. 金属学报, 2007, 43: 1082) | | [23] | Pickering F B.Physical Metallurgy and the Design of Steels [M]. London: Applied Science Publishing Ltd., 1978: 63 | | [24] | Ashby M F.Strengthening Methods in Crystals[M]. London: Applied Science Publishers Ltd., 1971: 137 | | [25] | Gladman T, Dulieu D, Mclvor I D.Microalloy' 75[M]. New York: Union Carbide Corporation, 1977: 32 |
|
|