| 界面能调控熔体中纳米颗粒分布铝热合成铁基ODS合金 |
刘建学, 席文君( ), 李能, 李树杰 |
| 北京航空航天大学材料科学与工程学院 北京 100191 |
|
| Effect of Interfacial Energy on Distribution of Nanoparticle in the Melt During the Preparation of Fe-Based ODS Alloys by Thermite Reaction |
Jianxue LIU, Wenjun XI( ), Neng LI, Shujie LI |
| School of Materials Science and Engineering, Beihang University, Beijing 100191, China |
引用本文:
刘建学, 席文君, 李能, 李树杰. 界面能调控熔体中纳米颗粒分布铝热合成铁基ODS合金[J]. 金属学报, 2017, 53(8): 1011-1017.
Jianxue LIU,
Wenjun XI,
Neng LI,
Shujie LI.
Effect of Interfacial Energy on Distribution of Nanoparticle in the Melt During the Preparation of Fe-Based ODS Alloys by Thermite Reaction[J]. Acta Metall Sin, 2017, 53(8): 1011-1017.
| [1] | Wright I G, Wilcox B A, Jaffee R I.The high-temperature oxidation of Ni-20%Cr alloys containing various oxide dispersions[J]. Oxid. Met., 1975, 9: 275 | | [2] | Nagai H, Takebayashi Y, Mitani H.Effect of dispersed oxides of rare earths and other reactive elements on the high temperature oxidation resistance of Fe-20Cr alloy[J]. Metall. Trans., 1981, 12A: 435 | | [3] | Ukai S, Harada M, Okada H, et al.Alloying design of oxide dispersion strengthened ferritic steel for long life FBRs core materials[J]. J. Nucl. Mater., 1993, 204: 65 | | [4] | Merzhanov A G.Self-propagating high-temperature synthesis: twenty years of search and findings [A]. Combustion and Plasma Synthesis of High-Temperature Materials[M]. New York: VCH Publishers, 1990: 1 | | [5] | Duan H P, Sheng Y, Liu M, et al.Stainless steel lined composite steel pipe produced by centrifugal SHS process[J]. J. Mater. Sci. Lett., 1996, 15: 1060 | | [6] | Xi W J, Yin S, Guo S J, et al.Stainless steel lined composite steel pipe prepared by centrifugal-SHS process[J]. J. Mater. Sci., 2000, 35: 45 | | [7] | Xi W J, Peng R L, Wu W, et al.Al2O3 nanoparticle reinforced Fe-based alloys synthesized by thermite reaction[J]. J. Mater. Sci., 2012, 47: 3585 | | [8] | Cui Y, Xi W J, Wang X, et al.Al2O3 nanoparticle and NiAl reinforced Fe-based ODS alloys synthesized by thermite reaction[J]. Acta Metall. Sin., 2015, 51: 791(崔跃, 席文君, 王星等. 纳米Al2O3和NiAl共同强化的铁基ODS合金的铝热合成研究[J]. 金属学报, 2015, 51: 791) | | [9] | Wang X, Xi W J, Cui Y, et al.Microstructure evolution mechanism and mechanical properties of FeNiCrAl alloy reinforced by coherent NiAl synthe-sized by thermite process[J]. Acta Metall. Sin. 2015, 51: 483(王星, 席文君, 崔跃等. 铝热合成NiAl共格强化的FeNiCrAl合金的组织演化机理和力学性能[J]. 金属学报, 2015, 51: 483) | | [10] | Wu W, Xi W J.Effect of heat decomposition process and thermal treatment for TiO2 Xerogel powder on surface organic functional groups[J]. Chin. J. Inorg. Chem., 2011, 27: 659(吴伟, 席文君. 二氧化钛干凝胶热分解及热处理对表面有机官能团变化的影响[J]. 无机化学学报, 2011, 27: 659) | | [11] | Chen R F, Liu H T.Preparation of Cr-doped TiO2/SiO2 photocatalysts and their photocatalytic properties[J]. J. Chin. Chem. Soc., 2011, 58: 947 | | [12] | Hao S M, Ishida K, Nishizawa T.Role of alloying elements in phase decomposition in alnico magnet alloys[J]. Metall. Trans., 1985, 16A: 179 | | [13] | Bradley A J.Microscopical studies on the iron-nickel-aluminium system. Part I——α+β alloys and isothermal sections of the phase equilibrium diagram[J]. J. Iron Steel Inst., 1949, 163: 19 | | [14] | Bradley A J.Microscopical studies on the iron-nickel-aluminium system. Part II——The breakdown of the body-centered cubic lattice[J]. J. Iron Steel Inst., 1951, 168: 233 | | [15] | Bradley A J.Microscopical studies on the iron-nickel-aluminium system. Part III——Transformations of the β and β' phase[J]. J. Iron Steel Inst., 1952, 171: 41 | | [16] | Hao S M, Takayama T, Ishida K, et al.Miscibility gap in Fe-Ni-Al and Fe-Ni-Al-Co systems[J]. Metall. Trans., 1984, 15A: 1819 | | [17] | Wang C P, Liu X J, Ohnuma I, et al.Thermodynamic database of the phase diagrams in Cu-Fe base ternary systems[J]. J. Phase Equilib. Diff., 2004, 25: 320 | | [18] | Baumli P, Sytchev J, Kaptay G.Perfect wettability of carbon by liquid aluminum achieved by a multifunctional flux[J]. J. Mater. Sci., 2010, 45: 5177 | | [19] | Rohrer G S.Grain boundary energy anisotropy: A review[J]. J. Mater. Sci., 2011, 46: 5881 | | [20] | Triantafyllou G, Angelopoulos G N, Nikolopoulos P.Surface and grain-boundary energies as well as surface mass transport in polycrystalline yttrium oxide[J]. J. Mater. Sci., 2010, 45: 2015 | | [21] | Nikolopoulos P, Agathopoulos S, Tsoga A.A method for the calculation of interfacial energies in Al2O3 and ZrO2/liquid-metal and liquid-alloy systems[J]. J. Mater. Sci., 1994, 29: 4393 | | [22] | Sharan A, Cramb A W.Surface tension and wettability studies of liquid Fe-Ni-O alloys[J]. Metall. Mater. Trans., 1997, 28B: 465 | | [23] | Silvain J F, Bihr J C, Douin J.Wettability, reactivity and stress relaxation of an NiAl(Ti)/Al2O3 composite[J]. Compos. Appl. Sci. Manuf., 1998, 29A: 1175 | | [24] | Nakanishi K, Soga N.Phase separation in silica sol-gel system containing polyacrylic acid I. Gel formaation behavior and effect of solvent composition[J]. J. Non-Cryst. Solids, 1992, 139: 1 | | [25] | Kaptay G.Interfacial criterion of spontaneous and forced engulfment of reinforcing particles by an advancing solid/liquid interface[J]. Metall. Mater. Trans., 2001, 32A: 993 | | [26] | K?rber C, Rau G, Cosman M D, et al.Interaction of particles and a moving ice-liquid interface[J]. J. Cryst. Growth, 1985, 72: 649 | | [27] | Uhlmann D R, Chalmers B, Jackson K A.Interaction between particles and a solid-liquid interface[J]. J. Appl. Phys., 1964, 35: 2986 | | [28] | Sen S, Dhindaw B K, Stefanescu D M, et al.Melt convection effects on the critical velocity of particle engulfment[J]. J. Cryst. Growth, 1997, 173: 574 | | [29] | Washizu T, Nagasaka T, Hino M.Viscosity of liquid Fe-Cu-Si alloy formed in new melting process for domestic waste incineration residue[J]. Mater. Trans., 2001, 42: 471 | | [30] | Huang Z Q, Ding E J.Surface Wetting and Wetting Transition [M]. Shanghai: Shanghai Science & Technical Publishers, 1994: 40(黄祖洽, 丁鄂江. 表面浸润和浸润相变 [M]. 上海: 上海科学技术出版社, 1994: 40) | | [31] | Chen Z Q, Dai M G.Colloidal Chemistry [M]. Beijing: Higher Education Press, 1984: 38(陈宗淇, 戴闽光. 胶体化学[M]. 北京: 高等教育出版社, 1984: 38) | | [32] | Wang J Y, Yuan W, Mishra R S, et al.Microstructure and mechanical properties of friction stir welded oxide dispersion strengthened alloy[J]. J. Nucl. Mater., 2013, 432: 274 | | [33] | Quadakkers W J, Holzbrecher H, Briefs K G, et al.Differences in growth mechanisms of oxide scales formed on ODS and conventional wrought alloys[J]. Oxid. Met., 1989, 32: 67 | | [34] | Klueh R L, Shingledecker J P, Swindeman R W, et al.Oxide dispersion-strengthened steels: a comparison of some commercial and experimental alloys[J]. J. Nucl. Mater., 2005, 341: 103 | | [35] | Montealegre M A, Strehl G, González-Carrasco J L, et al. Oxidation behaviour of novel ODS FeAlCr intermetallic alloys[J]. Intermetallics, 2005, 13: 896 | | [36] | Weinbruch S, Anastassiadis A, Ortner H M, et al.On the mechanism of high-temperature oxidation of ODS superalloys: significance of yttrium depletion within the oxide scales[J]. Oxid. Met., 1999, 51: 111 | | [37] | Wittenberger J D.Creep and tensile properties of several oxide-dispersion-strengthened nickel-base alloys at 1365 K [R]. Cleveland, OH, United States: NASA Lewis Research Center, 1977 | | [38] | Pint B A, Wright I G.Oxidation behavior of ODS Fe-Cr alloys[J]. Oxid. Met., 2005, 63: 193 | | [39] | Sokolov M A, Hoelzer D T, Stoller R E, et al. Fracture toughness and tensile properties of nano-structured ferritic steel 12YWT [J]. J. Nucl. Mater., 2007, 367-370: 213 |
|
|