| Ni-W-Cu-P沉积机制及在酸性溶液中的腐蚀行为* |
方信贤1,2( ),薛亚军1,戴玉明1,王章忠1,2 |
1 南京工程学院江苏省先进结构材料与应用技术重点实验室, 南京 211167 2 南京工程学院材料工程学院, 南京 211167 |
|
| DEPOSITION MECHANISM OF Ni-W-Cu-P COATING AND ITS CORROSION BEHAVIOR IN ACID SOLUTION |
Xinxian FANG1,2( ),Yajun XUE1,Yuming DAI1,Zhangzhong WANG1,2 |
1 Jiangsu Key Laboratory of Advanced Structural Materials and Application Technology, Nanjing Institute of Technology, Nanjing 211167, China 2 School of Materials Engineering, Nanjing Institute of Technology, Nanjing 211167, China; |
引用本文:
方信贤,薛亚军,戴玉明,王章忠. Ni-W-Cu-P沉积机制及在酸性溶液中的腐蚀行为*[J]. 金属学报, 2016, 52(11): 1432-1440.
Xinxian FANG,
Yajun XUE,
Yuming DAI,
Zhangzhong WANG.
DEPOSITION MECHANISM OF Ni-W-Cu-P COATING AND ITS CORROSION BEHAVIOR IN ACID SOLUTION[J]. Acta Metall Sin, 2016, 52(11): 1432-1440.
| [1] | Fang X X, Zhen R, Xue Y J, Wang Z Z.Chin J Mater Res, 2011; 25: 172 | | [1] | (方信贤, 甄睿, 薛亚军, 王章忠. 材料研究学报, 2011; 25: 172) | | [2] | Fang X X, Ba Z X, Zhen R, Wang Z Z.Trans Mater Treat, 2014; 35: 180 | | [2] | (方信贤, 巴志新, 甄睿, 王章忠. 材料热处理学报, 2014; 35: 180) | | [3] | Abdel Salam H, Shoeib M A, Hady H, Abdel Salam O F.Surf Coat Technol, 2007; 202: 162 | | [4] | Nalaraju J B, Ezhil Selvi V, William Grips V K, Rajam K S.Electrochim Acta, 2006; 52: 1064 | | [5] | Song J F, Guo K M, Zhao Z H.Chin J Nonferrous Met, 1998; 8: 379 | | [5] | (宋锦福, 郭凯铭, 赵子辉. 中国有色金属学报, 1998; 8: 379) | | [6] | Gao Y, Zheng Z J, Zhu M, Lu C P.Mater Sci Eng, 2004; A381: 98 | | [7] | Tien S K, Duh J G. Thin Solid Films#/magtechI#, 2004; 469-170: 268 | | [8] | Balaraju J N, Millath Jahan S, Rajam K S.Surf Coat Technol, 2006; 201: 507 | | [9] | Palaniappa M, Seshadri S K.Wear, 2008; 265: 735 | | [10] | He F J, Fang Y Z, Jin S J.Wear, 2014; 311: 14 | | [11] | Palaniappa M, Seshadri S K. Mater Sci Eng#/magtechI#, 2007; A460-461: 638 | | [12] | He S Z, Huang X M, Zheng H M, Li P, Lin Z P, Shan C L.Tribology, 2009; 29: 362 | | [12] | (何素珍, 黄新民, 郑华明, 李鹏, 林志平, 单传丽. 摩擦学学报, 2009; 29: 362) | | [13] | Fang X X, Bai Y Q, Wang Z Z.Acta Metall Sin, 2010; 46: 239 | | [13] | (方信贤, 白允强, 王章忠. 金属学报, 2010; 46: 239) | | [14] | Liu G C, Yang L J, Wang L D, Wang S L, Liu C Y, Wang J.Surf Coat Technol, 2010; 204: 3382 | | [15] | Balaraju J N, Rajam K S.Surf Coat Technol, 2005; 195: 154 | | [16] | Nee C C, Weil R.Surf Technol, 1985; 25: 7 | | [17] | Balaraju J N, Kalavati, Rajam K S.Surf Coat Technol, 2010; 205: 575 | | [18] | Fang X X, Zhou H Z, Xue Y J.Trans Nonferrous Met Soc China, 2015; 25: 2594 | | [19] | He S Z, Huang X M.Trans Mater Treat, 2010; 31: 133 | | [19] | (何素珍, 黄新民. 材料热处理学报, 2010; 31: 133) | | [20] | Liu H, Guo R X, Li S, Zong Y, He B Q.Chin J Nonferrous Met, 2011; 21: 1936 | | [20] | (刘宏, 郭荣新, 李莎, 宗云, 何冰清. 中国有色金属学报, 2011; 21: 1936) | | [21] | Liu H, Guo R X, Liu Y, Thompson G E, Liu Z.Surf Coat Technol, 2012; 206: 3350 | | [22] | Liu H, Viejo F, Guo R X, Glenday S, Liu S.Surf Coat Technol, 2010; 204: 1549 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|