| 钢圆坯连铸过程中渐开式电磁旋流水口数值模拟 |
| 李德伟,苏志坚,陈进,王强,丸川雄净,赫冀成 |
| 东北大学材料与冶金学院, 沈阳 110819 |
|
| NUMERICAL SIMULATION OF SWIRLING FLOW IN DIVERGENT SUBMERGED ENTRY NOZZLE IN ROUND BILLET CONTINUOUS CASTING OF STEEL |
| LI Dewei, SU Zhijian, CHEN Jin, WANG Qiang, MARUKAWA Katsukiyo, HE Jicheng |
| School of Materials and Metallurgy, Northeastern University, Shenyang 110819 |
引用本文:
李德伟,苏志坚,陈进,王强,丸川雄净,赫冀成. 钢圆坯连铸过程中渐开式电磁旋流水口数值模拟[J]. 金属学报, 2013, 49(7): 871-880.
LI Dewei,
SU Zhijian,
CHEN Jin,
WANG Qiang,
MARUKAWA Katsukiyo,
HE Jicheng.
NUMERICAL SIMULATION OF SWIRLING FLOW IN DIVERGENT SUBMERGED ENTRY NOZZLE IN ROUND BILLET CONTINUOUS CASTING OF STEEL[J]. Acta Metall Sin, 2013, 49(7): 871-880.
| [1] Yokoya S, Asako Y, Hara S, Szekely J. ISIJ Int, 1994; 34: 883
[2] Takagi S, Yokoya S, Iguchi M, Hara S. ISIJ Int, 1997; 10: 809
[3] Yokoya S, Takagi S, Iguchi M, Asako Y, Westoff R, Hara S. ISIJ Int, 1998; 38: 827
[4] Yokoya S, Takagi S, Iguchi M, Marukawa K, Yasugaira W, Hara S. ISIJ Int, 2000; 40: 584
[5] Kholmatov S, Takagi S, Jonsson L, Jonsson P, Yokoya S. ISIJ Int, 2007; 47: 80
[6] Tsukaguchi Y, Nakamura O, Jonsson P, Yokoya S, Tanaka T, Hara S. ISIJ Int, 2007; 47: 1436
[7] Jia H H, Yu Z, Lei Z S, Deng K, Chen J C, Hua W J, Ren Z M. Acta Metall Sin, 2008; 44: 375
(贾洪海, 于湛, 雷作胜, 邓康, 陈家昶, 华文杰, 任忠鸣. 金属学报, 2008; 44: 375)
[8] Cui X C, Liu Z C, Tian X M, Lin J B. Spec Steel, 2005; 26: 6
(崔小朝, 刘梓才, 田新明, 林金保. 特殊钢, 2005; 26: 6)
[9] Jia H H. Master Thesis, Shanghai University, 2008
(贾洪海. 上海大学硕士学位论文, 2008)
[10] Tsukaguchi Y, Hayashi H, Yokoya S, Tanaka T, Hara S. Tetsu Hagan$\acute{e$, 2007; 93: 575
(塚口友一, 林浩~史, 横谷真一郎, 田中敏宏, 原茂太. 鉄と鋼, 2007; 93: 575)
[11] Tsukaguchi Y, Hayashi H, Kurimoto H, Yokoya S, Marukawa K, Tanaka T. Tetsu Hagane, 2009; 95: 33
(塚口友一, 林浩史, 栗本英典, 横谷真一郎, 丸川雄净, 田中敏宏. 鉄と鋼, 2009; 95: 33)
[12] He J C, Katsukiyo M, Su Z J. Chin Pat, 200510047290.6, 2005
(赫冀成, 丸川雄净, 苏志坚. 中国专利, 200510047290.6, 2005)
[13] Shu Z J, Li D W, Sun L W, Katsukiyo M, He J C. Acta Metall Sin, 2010; 46: 479
(苏志坚, 李德伟, 孙立为, 丸川雄净, 赫冀成.金属学报, 2010; 46: 479)
[14] Yoneyama Y, Takeuchi E, Matsuzawa K, Sawada I, Hattori Y, Kishida Y.Nippon Steel Tech Report, 1990; 45: 30
[15] Spitzer K H, Dubke M, Schwerdtfeger K. Metall Trans, 1986; 17B: 119
[16] Thomas B G, Mika L J, Najjar F M. Metall Trans, 1990; 21B: 387 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|