| 新型医用Ti-24Nb-4Zr-8Sn合金在Hanks溶液中的电化学腐蚀行为研究 |
| 白芸1, 2), 李述军1), 郝玉琳1), 杨锐1) |
1) 中国科学院金属研究所沈阳材料国家(联合)实验室, 沈阳 110016
2) 鞍山师范学院化学系, 鞍山 114005 |
|
| ELECTROCHEMICAL CORROSION BEHAVIOR OF A NEW BIOMEDICAL Ti-24Nb-4Zr-8Sn ALLOY IN HANKS SOLUTION |
| BAI Yun1, 2), LI Shujun1), HAO Yulin1), YANG Rui1) |
1) Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
2) Chemistry Department, Anshan Normal University, Anshan 114005 |
引用本文:
白芸 李述军 郝玉琳 杨锐. 新型医用Ti-24Nb-4Zr-8Sn合金在Hanks溶液中的电化学腐蚀行为研究[J]. 金属学报, 2012, 48(1): 76-84.
,
,
,
.
ELECTROCHEMICAL CORROSION BEHAVIOR OF A NEW BIOMEDICAL Ti-24Nb-4Zr-8Sn ALLOY IN HANKS SOLUTION[J]. Acta Metall Sin, 2012, 48(1): 76-84.
| [1] Fekry A M, Ei–Sherif R M. Electrochim Acta, 2009; 54: 7280[2] Mu Z Q, Liang C H. Corros Sci Prot Technol, 1998; 10: 103(牟战旗, 梁成浩. 腐蚀科学与防护技术, 1998; 10: 103)[3] Shukla A K, Balasubramaniam R, Bhargava S. Intermetallics, 2005; 13: 631[4] Cai Z, Shafer T, Watanabe L, Nunn M E, Okabe T. Biomaterials, 2003; 24: 213[5] Tamilselvi S, Murugaraj R, Rajendran N. Mater Corros, 2007; 58: 113[6] Sumner D, Gatante J. Clin Orthop Rel Res, 1992; 274: 124[7] Wang K. Mater Sci Eng, 1996; A213: 134[8] Niinomi M. Mater Sci Eng, 1998; A243: 231[9] Hao Y L, Li S J, Sun S Y. Acta Biomater, 2007; 3: 277[10] Hao Y L, Li S J, Sun S Y. Mater Sci Eng, 2006; A441: 112[11] Semlitsch M F, Weber H, Streicher R M, Schon R. Biomaterials, 1992; 13: 781[12] Gurappa I. Mater Charact, 2002; 49: 73[13] Mareci D, Ungureanu G, Aelenei D M, Rosca J CM. Mater Corros, 2007; 58: 848[14] Gonzalez J E G, Mirza–Rosca J C. J Electroanal Chem, 1999; 471: 109[15] Koike M, Cai Z, Fujii H, Brezner M, Okabe T. Biomaterials, 2003; 24: 4541[16] Choubey A, Balasubramaniam R, Basui B. J Alloy Compd, 2004; 381: 288[17] Pourbaix M. Biomaterials, 1984; 5: 122[18] Metikos–Hukovic M, Kwokal A, Piljac J. Biomaterials, 2003; 24: 3765[19] Macdonald D D. J Electrochem Soc, 1992; 139: 3434[20] Cheng Y C, Zhang C B, Hu J, Tang C B, Gao B. Chin J Conserv Dent, 2010; 20: 84(程义成, 张春宝, 胡 江, 唐长斌, 高 勃. 牙体牙髓牙周病学杂志, 2010; 20: 84)[21] Alves V A, Reis R Q, Santos J C B, Souza D G. Corros Sci, 2009; 51: 2473[22] Tamilselvi S, Rajendran N. Mater Corros, 2007; 58: 285[23] Assis S L, Costa I. Mater Corros, 2007; 58: 329[24] Zhu Z Q, Xue W B, Lu L, Du J C, Liu G J, Li W F. Acta Metall Sin, 2011; 47: 74(朱振庆, 薛文斌, 鲁亮, 杜建成, 刘贯军, 李文芳. 金属学报, 2011; 47: 74)[25] Pouilleau J, Devilliers D, Garrido F, Durand–Vidal S, Mahe E. Mater Sci Eng, 1997; B47: 235[26] Pourbaix M. Atlas of Electrochemical Equilibria in Aqueoussolution. Brussels: Pergamon Press Ltd, 1966: 49[27] Freitas M, Bulhoes L. J Appl Electrochem, 1997; 27: 612[28] Zhou B X, Li Q, Liu W Q, Yao M Y, Chu Y L. Rare Met Mater Eng, 2006; 26: 1009(周邦新, 李强, 刘文庆, 姚美意, 褚于良. 稀有金属材料工程, 2006; 26: 1009) |
|