Please wait a minute...
金属学报  2011, Vol. 47 Issue (7): 777-783    DOI: 10.3724/SP.J.1037.2011.00265
  综述 本期目录 | 过刊浏览 |
核反应堆压力容器的辐照脆化与延寿评估
吕铮
东北大学材料各向异性与织构教育部重点实验室, 沈阳 110819
RADIATION-NDUCED EMBRITTLEMENT AND LIFE EVALUATION OF REACTOR PRESSURE VESSELS
LU Zheng
Key Laboratory for Anisotropy and Texture of Materials, Ministry of Education, Northeastern University, Shenyang 110819
引用本文:

吕铮. 核反应堆压力容器的辐照脆化与延寿评估[J]. 金属学报, 2011, 47(7): 777-783.
. RADIATION-NDUCED EMBRITTLEMENT AND LIFE EVALUATION OF REACTOR PRESSURE VESSELS[J]. Acta Metall Sin, 2011, 47(7): 777-783.

全文: PDF(925 KB)  
摘要: 核反应堆中辐照导致压力容器钢脆化使韧脆转变温度(DBTT)升高, 从而危及压力容器安全运行, 最终导致反应堆寿命终止. 本文简要介绍了压力容器钢辐照脆化机制、在役反应堆的安全性监测、模拟预测DBTT的升高和反应堆延寿评估.
关键词 : 反应堆压力容器,  辐照损伤,  DBTT升高,  寿命评估    
Abstract:Neutron irradiation can lead to the embrittlement and the shift of ductile-brittle transition temperature (DBTT) of the reactor pressure vessel (RPV) steels, which is the potential threat to the safe operation of reactors. Surveillance program for RPVs, irradiation damage and embrittlement of RPV steels and safe evaluation of RPVs were reviewed in this paper.
Key words: reactor pressure vessel    irradiation damage    DBTT shift    life evaluation
收稿日期: 2011-04-25     
基金资助:

国家自然科学基金项目50971033和91026013, 国家重点基础研究发展计划项目2011CB610405, 中央高校基本科研业务费N100402001及教育部新世纪优秀人才支持计划项目NCET-10-0302资助

作者简介: 吕铮, 男, 1970年生, 教授
[1] Odette G R, Lucas G E. JOM, 2001; 53: 18

[2] Little E A. Proc EUROMAT 96, Conf Materials and Nuclear Power, London: Institute of Materials, 1996: 29

[3] Nanstad R K, Sokolov M A, McCabe D E. J ASTM Int, 2008; 5: JAI101346

[4] Steele L E. In: Steele L E, ed., Status of USA Nuclear Reactor Pressure Vessel Surveillance for Radiation Effects, ASTM STP 784, Philadelphia, PA: American Society for Testing and Materials, 1983: 277

[5] Wallin K. Eng Fract Mech, 2002; 69: 451

[6] Little E A. Proc Conf Dimensional Stability and Mechanical Behavior of Irradiated Metals and Alloys, London: BNES, 1984: 141

[7] Guionnet C, Robin Y, Flavier C, Lefort A, Gros D, Perdreau R. In: Kramer D, Brager H R, Perrin J S, eds., Effects of Radiation on Materials: Proceedings of the Tenth International Symposium, ASTM STP 725, Philadelphia, PA: American Society for Testing and Materials, 1981: 20

[8] Monzen R, Iguchi M, Jenkins M L. Philos Mag Lett, 2000; 80: 137

[9] Phythian W J, English C A. J Nucl Mater, 1993; 205: 162

[10] Miller M K, Russell K F, Sokolov M A, Nanstad R K. J Nucl Mater, 2003; 320: 177

[11] Faulkner R G, Lu Z, Ellis D, Williams T J. J ASTM Int, 2005; 2: 285

[12] Buswell J T, Little E A, Sinclair R N. Nucl Energy, 1998; 37: 387

[13] Schilling W, Ullmaier H. In: Cahn R W, eds., Materials Science and Technology: Nuclear Materials, Vol.10B, Germany: Wiley–VCH, 1994: 179

[14] Domain C, Becquart C S, Malerba L. J Nucl Mater, 2004; 335: 121

[15] Jenkins M L, Kirk M A. Characterisation of Radiation Damage by Transmission Electron Microscopy. Bristol and Philadelphia: IOP Publishing, 2001: 126

[16] Little E A, Harries D R. Met Sci, 1970; 4: 188

[17] English C A, Ortner S R, Gage G, Server W L, Rosinski S T. In: Rosinski S T, Grossbeck M L, Allen T R, Kumar A S, eds., Effects of Radiation on Materials: 20th International Symposium, ASTM STP 1405, West Conshohocken, PA: American Society for Testing and Materials, 2001: 151

[18] Bischler P J E, Wild R K. In: Gelles D S, Nanstad R K, Kumar A S, Little E A, eds., Effects of Radiation on Materials: 17th International Symposium, ASTM STP 1270, West Conshohocken, PA: American Society for Testing and Materials, 1996: 260

[19] Faulkner R G, Jones R B, Lu Z, Flewitt P E J. Philos Mag, 2005; 85: 2065

[20] Pechenkin V A, Konobeev Y V, Stepanov I A, Nikolaev Y A. In: Grossbeck M L, Allen T R, Lott R G, Kumar A S, eds., Effects of Radiation on Materials: 21st International Symposium, ASTM STP 1447, West Conshohocken, PA: American Society for Testing and Materials, 2004: 138

[21] Lu Z, Faulkner R G, Flewitt P E J. Mater Sci Eng, 2006; A437: 306

[22] Lu Z, Faulkner R G, Sakaguchi N, Kinoshita H, Takahashi H J, Flewitt P E. J Nucl Mater, 2006; 351: 155

[23] Brillaud C, Hedin F, Houssin B. In: Garner F A, Henager C H, Igata N, eds., Influence of Radiation on Material Properties: 13th International Symposium, ASTM STP 956, Philadelphia, PA: American Society for Testing and Materials, 1987: 420

[24] Petrequin P. A Review of Formulas for Predicting Irradiation Embrittlement of Reactors Vessel Materials, AMES Report No.6, 1996: 13

[25] Odette G R, Mader E V, Lucas G E, Phythian W J, English C A. In: Kumar A S, Gelles D S, Nanstad R K, Little E A, eds., Effects of Radiation on Materials: 16th International Symposium, ASTM STP 1175, Philadelphia, PA: American Society for Testing and Materials, 1993: 373

[26] Odette G R, Yamamoto R T, Klingensmith R D. Philos Mag, 2005; 85: 779

[27] Miller M K, Russell K F. J Nucl Mater, 2007; 37: 145

[28] Odette G R, Wirth B D. J Nucl Mater, 1998; 251: 157
[1] 刘伟, 陈婉琦, 马梦晗, 李恺伦. 聚变堆用W在等离子体作用下的辐照损伤行为研究进展[J]. 金属学报, 2023, 59(8): 986-1000.
[2] 刘悦, 汤鹏正, 杨昆明, 沈一鸣, 吴中光, 范同祥. 抗辐照损伤金属基纳米结构材料界面设计及其响应行为的研究进展[J]. 金属学报, 2021, 57(2): 150-170.
[3] 梁晋洁, 高宁, 李玉红. 体心立方Fe中微裂纹与间隙型位错环相互作用的分子动力学模拟[J]. 金属学报, 2020, 56(9): 1286-1294.
[4] 吴玉程. 核聚变堆用W及其合金辐照损伤行为研究进展[J]. 金属学报, 2019, 55(8): 939-950.
[5] 李正操, 陈良. 核能系统压力容器辐照脆化机制及其影响因素[J]. 金属学报, 2014, 50(11): 1285-1293.
[6] 黄远 孔德月 何芳 王玉林 刘文西. 辐照损伤合金化制备Mo/Ag层状复合材料[J]. 金属学报, 2012, 48(10): 1253-1259.
[7] 贺新福 杨鹏 杨文. Fe-Cu合金基体损伤的分子动力学模拟研究[J]. 金属学报, 2011, 47(7): 954-957.
[8] 韩恩厚. 核电站关键材料在微纳米尺度上的环境损伤行为研究------进展与趋势[J]. 金属学报, 2011, 47(7): 769-776.
[9] 孙超 谭军 应诗浩 李聪 彭倩 赵素琼. 辐照后N18锆合金氢致延迟开裂临界温度预测[J]. 金属学报, 2010, 46(7): 805-809.
[10] 胡本芙; 木下博嗣; 坂口纪史; 高桥平七郎 . Fe-Cr-Mn钢时效析出碳化物辐照损伤行为[J]. 金属学报, 2006, 42(3): 234-238 .
[11] 胡本芙; 高桥平七郎 . He对低活性Fe-Cr-Mn(W, V)合金辐照产生点缺陷行为的影响[J]. 金属学报, 2004, 40(9): 955-961 .
[12] 胡苯芙; 木下博嗣; 高桥平七郎 . Fe-Cr-Mn(W, V)合金焊接热影响区的辐照损伤及诱发的晶界元素偏析[J]. 金属学报, 1999, 35(10): 1090-1094 .
[13] 孙继光;陈朝庆;张希顺;田耘;单秉权;潘庆春. ODS铁素体合金抗辐照损伤性能[J]. 金属学报, 1998, 34(11): 1210-1216.
[14] 万发荣;黄学军;褚武扬;肖纪美. 铁素体钢中氢对材料辐照肿胀行为的影响[J]. 金属学报, 1995, 31(2): 69-73.
[15] 万发荣;黄学军;孔峰;褚武扬;肖纪美;高桥平七郎;北京科技大学;日本北海道大学. 氧化物弥散强化铁素体钢的电子辐照行为[J]. 金属学报, 1994, 30(22): 448-452.