| Fe-B-Si三元系熔体的热力学 Ⅰ.1450℃时Si的活度及活度交互作用系数 |
| 冀春霖;俞荣祥;刘素兰 |
| 东北工学院;东北工学院;东北工学院冶金物化教研室;讲师;沈阳市湖东 |
|
| THERMODYNAMICS OF TERNARY Fe-B-Si MELTS AT 1450℃ Ⅰ. ACTIVITY OF Si AND ITS INTERACTION COEFFICIENTS |
| JI Chunlin;YU Rongxiang;LIU Sulan Northeast University of Technology; ShenyangLIU Sulan Lecturer;Department of Metallurgleal Phusicat Chemistry;Northeoss University of Technology;Shenyang |
引用本文:
冀春霖;俞荣祥;刘素兰. Fe-B-Si三元系熔体的热力学 Ⅰ.1450℃时Si的活度及活度交互作用系数[J]. 金属学报, 1988, 24(2): 155-160.
,
,
.
THERMODYNAMICS OF TERNARY Fe-B-Si MELTS AT 1450℃ Ⅰ. ACTIVITY OF Si AND ITS INTERACTION COEFFICIENTS[J]. Acta Metall Sin, 1988, 24(2): 155-160.
1 Wagner C. Thermodynamic of,Alloys, Reading Mass: Addison-Wesley. 1952: 51 2 Lupis C H P, Elliott J F. Acta Metall. 1966; 14: 529. 1019 3 Elliott J F, Gleiser M, Ramakrishna V. Thermochemistry for Steelmaking II, Reading Mass: Addison-Wesley, 1963: 4 Schenck H, Steinmetz E. Arch Eisenhuettenwes, 1968; 39: 255 5 松下幸雄,坂尾弘,大谷正康等,制钢反应推奖平衡值,日本学术振兴会,1968: 6 Sigworth G K,Elliott J F.Met Sci,1974;8:298 7 松下幸雄,坂尾弘,大谷正康等,制钢反应推奖平衡值,(改订增补)日本学术振兴会,1984: 8 Ball D L. Trans Metall Soc AIME, 1967; 239: 31 9 Schroeder D, Chipman J. Trans Metall Soc AIME, 1964; 230: 1492. 10 #120 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|