| Fe-B-Si三元系熔体的热力学 Ⅱ.1450℃时硼的活度及活度交互作用系数 |
| 冀春霖;俞荣祥;刘素兰 |
| 东北工学院;东北工学院;东北工学院冶金物化教研室;讲师;沈阳市南湖 |
|
| THERMODYNAMICS OF TERNARY Fe-B-Si MELTS AT 1450℃ Ⅱ. ACTIVITY OF B AND ITS INTERACTION COEFFICIENTS |
| JI Chunlin;YU Rongxiang Northeast University of Technology;LIU Sulan Leeturer;Department of Metallurgtcal Physicat Chemistry;Northeast University of Technotogy;Shenyang |
引用本文:
冀春霖;俞荣祥;刘素兰. Fe-B-Si三元系熔体的热力学 Ⅱ.1450℃时硼的活度及活度交互作用系数[J]. 金属学报, 1988, 24(2): 161-165.
,
,
.
THERMODYNAMICS OF TERNARY Fe-B-Si MELTS AT 1450℃ Ⅱ. ACTIVITY OF B AND ITS INTERACTION COEFFICIENTS[J]. Acta Metall Sin, 1988, 24(2): 161-165.
1 Darken L S. J Amer Chem Soc, 1950; 72: 2909 2 Wagner C. Thermodynamics of Alloys, Reading Mass: Addison-Wesley, 1952: 19 3 Makay H A C. Trans Faraday Soc, 1953; 49: 237 4 Schuhmann R Jr. Acta Metall, 1955; 3: 219 5 Gokcen N A. J Phys Chem, 1960; 64: 401 6 周国治.中国科学,1977;(5) :456 7 王之昌,周国治.中国科学,1984;(10) :959 8 冀春霖,俞荣祥,刘素兰.金属学报,1988;24:B87 9 Evans D B. Pehlke R D. Trans Metall Soc AIME. 1964; 230. 1657 10 Ball D L. Trans Metall Soc AIME, 1967; 239: 31 11 Schenck H, Steinmetz E. Arch Eisenhuettenwes, 1968; 39: 255 12 Fruehan R J. Metall Trans, 1970; 1: 2083 13 Lupis C H P, Elliott J F. Acta Metall, 1966; 14: 529 14 Darken L S. Trans Metall Soc AIME, 1967; 239: 80 |
|