| 铁基非晶合金局部晶化过程中的矫顽力拐折现象 |
| 杨国斌;关志群;王双全;王润 |
| 教授;北京钢铁学院材料系;北京钢铁学院;北京钢铁学院;北京钢铁学院 |
|
| INFLECTION OF COERCIVITY DURING LOCAL CRYSTALLIZATION OF Fe-Si-B AMORPHOUS ALLOYS |
| YANG Guobin;GUAN Zhiqun;WANG Shuangquan;WANG Run Beijing University of Iron and Steel TechnologyProfessor;Department of Materials Science; Beijing University of Iron and Steel Technology |
引用本文:
杨国斌;关志群;王双全;王润. 铁基非晶合金局部晶化过程中的矫顽力拐折现象[J]. 金属学报, 1988, 24(4): 362-364.
,
,
,
.
INFLECTION OF COERCIVITY DURING LOCAL CRYSTALLIZATION OF Fe-Si-B AMORPHOUS ALLOYS[J]. Acta Metall Sin, 1988, 24(4): 362-364.
1 Kronmuller H. J Magn Magn Mater, 1981; 24: 159 2 Hasegawa R, Fish G E, Ramanan VRR V, J Magn Magn Mater, 1976; 2: 927 3 Hasegawa R, Ramanan V R V, Fish G E. J Appl Phys, 1982; 53: 2276 4 Ramanan V R V, Fish G E. J Appl Phys, 1982; 52: 2273 5 Yeh H L, Maddin R. Metall Trans, 1979; 10A: 771 6 Novak L., Potocky L, Lovas A, Kisdi-Koszo E, Takaecs J. J Magn Magn Mater, 1980; 19: 149 7 北京大学物理系.铁磁学,科学出版社,1974 |
|