| Ni-32.5%Sn共晶合金的净化与深过冷 |
| 魏炳波;杨根仓;周尧和 |
| 西北工业大学凝固技术国家实验室;讲师;西北工业大学;西北工业大学 |
|
| DENUCLEATION AND HIGH UNDERCOOLING OF Ni-32.5%Sn EUTECTIC ALLOY |
| WEI Bingbo;YANG Gencong;ZHOU Yaohe Northwestern Polytechnical University; Xi'an |
引用本文:
魏炳波;杨根仓;周尧和. Ni-32.5%Sn共晶合金的净化与深过冷[J]. 金属学报, 1990, 26(5): 119-124.
,
,
.
DENUCLEATION AND HIGH UNDERCOOLING OF Ni-32.5%Sn EUTECTIC ALLOY[J]. Acta Metall Sin, 1990, 26(5): 119-124.
1 Sahm P R, Jones H, Adam C M. Science and Technology of the Undercooled Melt, Dordrecht, Netherlands: Martinus Nijhoff Publishers, 1986 2 魏炳波.杨根仓.航空学报,1988;9:B589 3 Flemings M C, Shiohara Y. Mater Sci Eng, 1984; 65: 157 4 Powell G L F. J Aust Inst Met, 1965; 10: 233 5 Perepezko J H. Mater Sci Eng, 1984; 65: 125 6 Smithells C J. Metals Reference Book, 5th ed., London: Butterworths, 1976: 186, 940 7 Holloman J H, Turnbull D. Prog Met Phys, 1953; 4: 333 8 Nielsen H J V. Z Metallk, 1979; 70: 606 9 Davies H A. In: Cantor B ed, Rapidly Quenched Metals Ⅲ, Vol. Ⅰ, London: The Metals Society, 1978: 1 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|