YNi_5相及其对Ni_3Al合金性能的影响 |
王淑荷;郭建亭;李辉;孙超;谭明晖;赖万慧 |
中国科学院金属研究所;副研究员;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
ON THE YNi_5 PHASE AND ITS EFFECT UPON PROPERTIES OF Ni_3 Al ALLOY |
WANG Shuhe;GUO Jianting;LI Hui; SUN Chao;TAN Minghui;LAI Wanhui Institute of Metal Research; Academia Sinica; Shenyang |
引用本文:
王淑荷;郭建亭;李辉;孙超;谭明晖;赖万慧. YNi_5相及其对Ni_3Al合金性能的影响[J]. 金属学报, 1991, 27(6): 39-43.
,
,
,
,
,
.
ON THE YNi_5 PHASE AND ITS EFFECT UPON PROPERTIES OF Ni_3 Al ALLOY[J]. Acta Metall Sin, 1991, 27(6): 39-43.
1 青木清,和泉修,日本金属学会会志,1979;43:1190 2 郭建亭,李辉,孙超,朱耀霄.金属学报,1989;25:A406 3 Holt R T, Wallace W. Int Metall Rev, 1976; 21(1) : 1 4 Beaudry B J, Daans A H. Trans AIME, 1960; 218: 854 5 Guo Jianting, Sun Chao, Li Hui, Lai Wanhui, Tan Minghu:, Wang Shuhe. International Symposium on High-Temperature Corrosion and Protection, June 26--30. 1990, Shenyangr |
|