| 镍基单晶高温合金的蠕变损伤规律研究 |
| 岳珠峰;吕震宙;郑长卿 |
| 西北工业大学 |
|
| THE CREEP─DAMAGE BEHAVIOUR FOR SINGLE CRYSTAL NICKEL-BASE SUPERALLOY |
| YUE Zhufeng;LU Zhenzhou;ZHENG Changqing(Northwestern Polytechnical University;Xi'an 710072) |
引用本文:
岳珠峰;吕震宙;郑长卿. 镍基单晶高温合金的蠕变损伤规律研究[J]. 金属学报, 1995, 31(8): 370-375.
,
,
.
THE CREEP─DAMAGE BEHAVIOUR FOR SINGLE CRYSTAL NICKEL-BASE SUPERALLOY[J]. Acta Metall Sin, 1995, 31(8): 370-375.