金属学报  2026, Vol. 62 Issue (5): 905-922    DOI: 10.11900/0412.1961.2025.00323
  综述 本期目录 | 过刊浏览 |
纯Mo及钼基可降解金属材料的研究现状与发展趋势
郑玉峰(), 谌雨农
北京大学 材料科学与工程学院 北京 100871
Research Status and Future Directions of Pure Mo and Mo-Based Biodegradable Metals
ZHENG Yufeng(), SHEN Yunong
School of Materials Science and Engineering, Peking University, Beijing 100871, China
引用本文:

郑玉峰, 谌雨农. 纯Mo及钼基可降解金属材料的研究现状与发展趋势[J]. 金属学报, 2026, 62(5): 905-922.
Yufeng ZHENG, Yunong SHEN. Research Status and Future Directions of Pure Mo and Mo-Based Biodegradable Metals[J]. Acta Metall Sin, 2026, 62(5): 905-922.

全文: PDF(3727 KB)   HTML
摘要: 

Mo是人体所必需的微量元素之一,金属纯Mo因其优异的力学性能、均匀的降解行为和良好的生物相容性,成为心脑血管支架、心脏起搏器、肠胃吻合钉和可穿戴生物电子器械等多种植/介入医疗器械潜在的候选材料。钼基金属材料已有一些合金体系和复合材料应用于航空航天、电子和化工等领域,但作为可降解金属用于医疗领域的研究尚处于起步阶段,诸多关键科学问题尚未厘清。本文聚焦纯Mo及钼基金属材料的材料本性,借鉴其在工程领域的制造路径和性能优势,梳理其在生理环境中的腐蚀行为和降解产物的潜在生物学效应,基于材料生物降解性和生物相容性的双重筛选原则,并结合可降解金属器械的服役需求,提出新型钼基可降解金属材料的合金成分设计、微观组织、塑性变形、增材制造和生物医学性能提升策略,展望其未来可能在生物医学领域的应用前景及发展方向。

关键词 : Mo,  可降解金属,  力学性能,  降解行为,  生物相容性    
Abstract:

Mo, a trace element in the human body, has attracted increasing attention owing to its excellent mechanical properties, uniform degradation behavior, and favorable biocompatibility. The highlighted features make it a promising candidate for various biodegradable medical devices, including cardiovascular and neurovascular stents, cardiac pacemakers, gastrointestinal anastomotic staples, and wearable bioelectronic devices. Currently, Mo and its alloys have been developed as industrial materials and are well-established in aerospace, electronics, and chemical engineering. However, research on Mo and its alloys as biomaterials is an emerging field of study and faces several critical scientific challenges. In this review, we highlight Mo's intrinsic material characteristics, summarize traditional manufacturing methods and performance advantages, and outline its degradation mechanisms and biological responses in physiological environments. Furthermore, we propose design strategies for Mo-based biodegradable metals that consider biodegradability, biocompatibility, and the functional requirements of biodegradable implants, focusing on composition, microstructure, plastic deformation, and additive manufacturing. Finally, we discuss the future applications and developmental directions of Mo-based biodegradable metals in the field of biomaterials.

Key words: Mo    biodegradable metal    mechanical property    biodegradation behavior    biocompatibility
收稿日期: 2025-10-20     
ZTFLH:  TG146  
基金资助:国家自然科学基金重点项目(52531008)
通讯作者: 郑玉峰,yfzheng@pku.edu.cn,主要从事生物医用金属材料研究
Corresponding author: ZHENG Yufeng, professor, Tel: (010)62767411, E-mail: yfzheng@pku.edu.cn
作者简介: 郑玉峰,男,1973年生,教授,博士
图1  可降解金属纯Mo的腐蚀行为研究:Mo-H2O体系的Pourbaix图[36];纯Mo在生理环境及模拟炎症条件下的生物降解行为示意图[36];选区激光熔化和旋锻纯Mo随浸泡时间演化的腐蚀机理及过程对比[37];Mo在去离子水中溶解时的表面化学状态和显微组织演变[38]
图2  金属纯Mo在血管内植入后的研究结果:EDS分析证实了腐蚀产物层的形成[73];免疫荧光染色显示在Mo和Pt植入物周围存在内皮细胞(CD31)和平滑肌肌动蛋白(α-SMA)的反应[73];X光片、微型CT及取出物观察结果显示植入物可保留并在体内维持血管整合长达12个月[74];苏木精-伊红(H&E)染色和Masson染色证实了大鼠腹主动脉内的血管组织反应[16];SEM观察(BSE模式)显示在3个月时出现支架支杆的在体降解并可见明显的降解产物[16];对降解产物的表征[16];Mo丝编织支架和弹簧圈在颅内缺血性和出血性卒中治疗中的应用及用于评估钼基神经植入物的组织病理学和功能安全性的流程示意图[75];编织支架Mo丝对体内神经功能的影响[75];及二维Mo弹簧圈的体内生物安全性[75]
图3  含Mo薄膜的暂态电子学器件:可吸收的温度和压力传感器实物图及构成传感区域的蛇形Si-纳米膜结构的OM像[77];大鼠脑内可吸收传感器系统的示意图[77];一种用于高分辨率皮层脑电图(ECoG)的有源多路复用全可吸收传感器装置的爆炸透视示意图及处于不同制造阶段的两个单元的OM像和整个系统的实物照片[79];可弯曲的生态可吸收/生物可吸收微机电系统(eb-MEMS)平台的示意图[80];及一种暂时性、无线、无电池的电刺激装置附着在足部创口上的示意图[81]
图4  可降解钼合金的候选合金化元素
图5  常见生物安全的可降解颗粒的熔点-硬度关系图[88]
图6  含Mo生物材料应用于骨科器械的实验结果:实物照片和Micro-CT分析显示7.5Mo-BGC (生物活性玻璃陶瓷)支架在第12周相较于空白组和BGC组具有更优的骨软骨修复效果[89];第12周的番红O染色结果显示7.5Mo-BGC组形成了更多透明软骨样组织[89];Micro-CT及三维重建证实在第1和第8周支架的保留、新骨形成及新骨向Mo支架内的长入[90];组织学染色显示新形成的骨-牙周膜-牙骨质复合体[91];免疫荧光结果提示在再生牙周膜内有成纤维连接蛋白骨膜蛋白的表达[92];组织学测量分析显示牙周再生相关参数得到改善[91];免疫荧光进一步显示在骨-牙周膜及牙周膜-牙根界面处存在神经标志物(CGRP、TRPV、TRPM8)的表达[91];RAW 264.7细胞在Mmp9抑制剂(Ilomastat)处理下的免疫荧光图像[92];及巨噬细胞对可降解钼植入物降解产物炎症反应的示意图[92]
图7  纯Mo及钼基合金、其他可降解金属及其合金及CoCr合金体系的力学性能总结图[87,93~95];钼基可降解金属材料的潜在医学应用预测
[1] Lasheen T A, El-Ahmady M E, Hassib H B, et al. Molybdenum metallurgy review: Hydrometallurgical routes to recovery of molybdenum from ores and mineral raw materials [J]. Miner. Process. Extr. Metall. Rev., 2015, 36: 145
doi: 10.1080/08827508.2013.868347
[2] Novotny J A, Peterson C A. Molybdenum [J]. Adv. Nutr., 2018, 9: 272
doi: 10.1093/advances/nmx001 pmid: 29767695
[3] Outteridge T, Kinsman N, Ronchi G, et al. Editorial: Industrial relevance of molybdenum in China [J]. Adv. Manuf., 2020, 8: 35
doi: 10.1007/s40436-019-00270-5
[4] Braithwaite E R, Haber J. Molybdenum: An Outline of Its Chemistry and Uses: Vol.19[M]. Amsterdam: Elsevier, 2013: 13
[5] Morales R, Aune R E, Seetharaman S, et al. The powder metallurgy processing of refractory metals and alloys [J]. JOM, 2003, 55(10): 20
[6] Lalik E. Kinetic analysis of reduction of MoO3 to MoO2 [J]. Catal. Today, 2011, 169: 85
doi: 10.1016/j.cattod.2010.09.013
[7] Tkachenko S, Oliver-Urrutia C, Ksenzova O, et al. Production of spherical Mo and Mo-Si powders by spray drying of Si suspension in a water-soluble Mo precursor [J]. Adv. Powder Technol., 2024, 35: 104313
doi: 10.1016/j.apt.2023.104313
[8] Garg P, Park S J, German R M. Effect of die compaction pressure on densification behavior of molybdenum powders [J]. Int. J. Refract. Met. Hard Mater., 2007, 25: 16
doi: 10.1016/j.ijrmhm.2005.10.014
[9] Solodkyi I, Petrusha V, Grigoroscuta M A, et al. Efficient sintering of Mo matrix composites—A study of temperature dependences and the use of the sinter additive Ni [J]. Metals, 2023, 13: 1715
doi: 10.3390/met13101715
[10] Huang H S, Hwang K S. Deoxidation of molybdenum during vacuum sintering [J]. Metall. Mater. Trans., 2002, 33A: 657
[11] Tanvir G, Karim M A, Jadhav S, et al. Effect of hot isostatic pressing on porosity of wire-arc directed energy deposited TZM/NbZr1 bimetallic structure [J]. Virtual Phys. Prototy., 2024, 19: e2404989
doi: 10.1080/17452759.2024.2404989
[12] Atkinson H V, Davies S. Fundamental aspects of hot isostatic pressing: An overview [J]. Metall. Mater. Trans., 2000, 31A: 2981
[13] Mouawad B, Soueidan M, Fabrègue D, et al. Full densification of molybdenum powders using spark plasma sintering [J]. Metall. Mater. Trans., 2012, 43A: 3402
[14] Liu Z W, Wang A Q, Zhang Q F, et al. Microstructure evolution and process optimization of molybdenum rods during loose tooling forging [J]. Int. J. Refract. Met. Hard Mater., 2022, 108: 105926
doi: 10.1016/j.ijrmhm.2022.105926
[15] Primig S, Clemens H, Knabl W, et al. Orientation dependent recovery and recrystallization behavior of hot-rolled molybdenum [J]. Int. J. Refract. Met. Hard Mater., 2015, 48: 179
doi: 10.1016/j.ijrmhm.2014.09.008
[16] Bian D, Tong Z P, Gong G C, et al. Additive manufacturing of biodegradable molybdenum—From powder to vascular stent [J]. Adv. Mater., 2024, 36: 2401614
doi: 10.1002/adma.v36.32
[17] Zhao C, Shi B, Chen S L, et al. Laser melting modes in metal powder bed fusion additive manufacturing [J]. Rev. Mod. Phys., 2022, 94: 045002
[18] Wang D Z, Yu C F, Ma J, et al. Densification and crack suppression in selective laser melting of pure molybdenum [J]. Mater. Des., 2017, 129: 44
doi: 10.1016/j.matdes.2017.04.094
[19] Ramakrishnan T, Espiritu E R L, Kwon S, et al. Laser powder bed fusion additive manufacturing of molybdenum using a nitrogen build atmosphere [J]. Int. J. Refract. Met. Hard Mater., 2024, 119: 106555
doi: 10.1016/j.ijrmhm.2024.106555
[20] Leclercq A, Mouret T, Brailovski V. Laser powder bed fusion of molybdenum: Density, structure and mechanical properties at room and elevated temperatures [J]. Mater. Sci. Eng., 2025, A929: 148004
[21] Rebesan P, Ballan M, Bonesso M, et al. Pure molybdenum manufactured by laser powder bed fusion: Thermal and mechanical characterization at room and high temperature [J]. Add. Manuf., 2021, 47: 102277
[22] Yan A R, Atif A M, Wang X B, et al. The microstructure and cracking behaviors of pure molybdenum fabricated by selective laser melting [J]. Materials, 2022, 15: 6230
doi: 10.3390/ma15186230
[23] Fu Z W, Körner C. Actual state-of-the-art of electron beam powder bed fusion [J]. Eur. J. Mater., 2022, 2: 54
[24] Dejene N D, Lemu H G. Current status and challenges of powder bed fusion-based metal additive manufacturing: Literature review [J]. Metals, 2023, 13: 424
doi: 10.3390/met13020424
[25] Böhm J, Breuning C, Markl M, et al. A new approach of preheating and powder sintering in electron beam powder bed fusion [J]. Int. J. Adv. Manuf. Technol., 2024, 133: 3769
doi: 10.1007/s00170-024-13966-1
[26] Fernandez-Zelaia P, Ledford C, Ellis E A I, et al. Crystallographic texture evolution in electron beam melting additive manufacturing of pure molybdenum [J]. Mater. Des., 2021, 207: 109809
doi: 10.1016/j.matdes.2021.109809
[27] Di Sturco S, Marchese G, Bondioli F, et al. Understanding the processability, microstructure, and mechanical properties of molybdenum processed by electron beam powder bed fusion [J]. Int. J. Refract. Met. Hard Mater., 2025, 129: 107091
doi: 10.1016/j.ijrmhm.2025.107091
[28] Gröger R, Bailey A G, Vitek V. Multiscale modeling of plastic deformation of molybdenum and tungsten: I. Atomistic studies of the core structure and glide of 1/2<111> screw dislocations at 0 K [J]. Acta Mater., 2008, 56: 5401
doi: 10.1016/j.actamat.2008.07.018
[29] Gröger R, Vitek V. Multiscale modeling of plastic deformation of molybdenum and tungsten. III. Effects of temperature and plastic strain rate [J]. Acta Mater., 2008, 56: 5426
doi: 10.1016/j.actamat.2008.07.027
[30] Kraych A, Clouet E, Dezerald L, et al. Non-glide effects and dislocation core fields in BCC metals [J]. npj Comput. Mater., 2019, 5: 109
doi: 10.1038/s41524-019-0247-3
[31] Zhang G, Chen G Q, Panwisawas C, et al. First-principles study of oxygen segregation and its effect on the embrittlement of molybdenum symmetrical tilt grain boundaries [J]. Acta Mater., 2023, 261: 119387
doi: 10.1016/j.actamat.2023.119387
[32] Mueller A J, Bianco R, Buckman R W. Evaluation of oxide dispersion strengthened (ODS) molybdenum and molybdenum-rhenium alloys [J]. Int. J. Refract. Met. Hard Mater., 2000, 18: 205
doi: 10.1016/S0263-4368(00)00028-7
[33] Tammas-Williams S, Withers P J, Todd I, et al. The influence of porosity on fatigue crack initiation in additively manufactured titanium components [J]. Sci. Rep., 2017, 7: 7308
doi: 10.1038/s41598-017-06504-5 pmid: 28779073
[34] Cockeram B V. The role of stress state on the fracture toughness and toughening mechanisms of wrought molybdenum and molybdenum alloys [J]. Mater. Sci. Eng., 2010, A528: 288
[35] Pourbaix M. Atlas of Electrochemical Equilibria in Aqueous Solutions [M]. Brussels: Pergamon Press, 1966: 272
[36] Shen Y N, Cheng Y, Zheng Y F. Insight into the biodegradation behavior of pure molybdenum under simulated inflammatory condition [J]. Corros. Sci., 2024, 228: 111816
doi: 10.1016/j.corsci.2023.111816
[37] Tong Z P, Gong G C, Huang H, et al. In vitro corrosion and biocompatibility of additively manufactured biodegradable molybdenum [J]. Acta Biomater., 2025, 191: 66
doi: 10.1016/j.actbio.2024.11.019 pmid: 39572309
[38] Yin L, Cheng H Y, Mao S M, et al. Dissolvable metals for transient electronics [J]. Adv. Funct. Mater., 2014, 24: 645
doi: 10.1002/adfm.v24.5
[39] Hixson H, Sherwood P M A. Valence-band and core photoelectron spectroscopic studies of molybdenum aqueous oxidation and the influence of argon-ion etching [J]. J. Chem. Soc., Faraday Trans., 1995, 91: 3593
[40] Okonkwo I A, Doff J, Baron-Wiecheć A, et al. Oxidation states of molybdenum in oxide films formed in sulphuric acid and sodium hydroxide [J]. Thin Solid Films, 2012, 520: 6318
doi: 10.1016/j.tsf.2012.05.031
[41] Petrova M, Bojinov M, Zanna S, et al. Mechanism of anodic oxidation of molybdenum in nearly-neutral electrolytes studied by electrochemical impedance spectroscopy and X-ray photoelectron spectroscopy [J]. Electrochim. Acta, 2011, 56: 7899
doi: 10.1016/j.electacta.2010.12.022
[42] Novotny J A, Turnlund J R. Molybdenum intake influences molybdenum kinetics in men [J]. J. Nutr., 2007, 137: 37
doi: 10.1093/jn/137.1.37 pmid: 17182798
[43] Institute of Medicine. Dietary Reference Intakes for Vitamin A, Vitamin K, Arsenic, Boron, Chromium, Copper, Iodine, Iron, Manganese, Molybdenum, Nickel, Silicon, Vanadium, and Zinc [M]. Washington: National Academies Press, 2001: 420
[44] Novotny J A. Molybdenum nutriture in humans [J]. J. Evid. Based Complementary Altern. Med., 2011, 16: 164
doi: 10.1177/2156587211406732
[45] Brewer G J, Askari F, Dick R B, et al. Treatment of Wilson’s disease with tetrathiomolybdate: V. Control of free copper by tetrathiomolybdate and a comparison with trientine [J]. Transl. Res., 2009, 154: 70
doi: 10.1016/j.trsl.2009.05.002
[46] Harrison R. Structure and function of xanthine oxidoreductase: Where are we now? [J]. Free Radical Biol. Med., 2002, 33: 774
doi: 10.1016/S0891-5849(02)00956-5
[47] Polito L, Bortolotti M, Battelli M G, et al. Xanthine oxidoreductase: A leading actor in cardiovascular disease drama [J]. Redox Biol., 2021, 48: 102195
doi: 10.1016/j.redox.2021.102195
[48] Battelli M G, Bortolotti M, Polito L, et al. The role of xanthine oxidoreductase and uric acid in metabolic syndrome [J]. Biochim. Biophys. Acta Mol. Basis Dis., 2018, 1864: 2557
doi: 10.1016/j.bbadis.2018.05.003
[49] Kelley E E. Biochemistry of molybdopterin nitrate/nitrite reductases [A]. Nitric Oxide: Biology and Pathobiology [M]. London: Elsevier, 2017: 173
[50] Terao M, Romão M J, Leimkühler S, et al. Structure and function of mammalian aldehyde oxidases [J]. Arch. Toxicol., 2016, 90: 753
doi: 10.1007/s00204-016-1683-1 pmid: 26920149
[51] Shintani Y, Maruoka S, Gon Y, et al. Nuclear factor erythroid 2-related factor 2 (Nrf2) regulates airway epithelial barrier integrity [J]. Allergol. Int., 2015, 64(suppl.) : S54
[52] Shaw S, Jayatilleke E. The role of aldehyde oxidase in ethanol-induced hepatic lipid peroxidation in the rat [J]. Biochem. J., 1990, 268: 579
pmid: 2363695
[53] Burzlaff A, Beevers C, Pearce H, et al. New studies on the in vitro genotoxicity of sodium molybdate and their impact on the overall assessment of the genotoxicity of molybdenum substances [J]. Regul. Toxicol. Pharm., 2017, 86: 279
doi: 10.1016/j.yrtph.2017.03.018
[54] Barceloux D G, Barceloux D. Molybdenum [J]. J. Toxicol.: Clin. Toxicol., 1999, 37: 231
doi: 10.1081/CLT-100102422
[55] Vyskočil A, Viau C. Assessment of molybdenum toxicity in humans [J]. J. Appl. Toxicol., 1999, 19: 185
pmid: 10362269
[56] Murray F J, Sullivan F M, Tiwary A K, et al. 90-day subchronic toxicity study of sodium molybdate dihydrate in rats [J]. Regul. Toxicol. Pharm., 2014, 70: 579
doi: 10.1016/j.yrtph.2013.09.003
[57] Bandyopadhyay S K, Chatterjee K, Tiwari R K, et al. Biochemical studies on molybdenum toxicity in rats: Effects of high protein feeding [J]. Int. J. Vitam. Nutr. Res., 1981, 51: 401
pmid: 7327862
[58] Bompart G, Pécher C, Prévot D, et al. Mild renal failure induced by subchronic exposure to molybdenum: urinary kallikrein excretion as a marker of distal tubular effect [J]. Toxicol. Lett., 1990, 52: 293
doi: 10.1016/0378-4274(90)90039-o pmid: 1975134
[59] Ott H C, Prior C, Herold M, et al. Respiratory symptoms and bronchoalveolar lavage abnormalities in molybdenum exposed workers [J]. Wien. Klin. Wochenschr., 2004, 116(suppl.): 25
[60] National Toxicology Program. Toxicology and carcinogenesis studies of molybdenum trioxide [R]. Research Triangle Park, NC: U.S. Dept. of Health and Human Services, Public Health Service, National Institutes of Health, 1997
[61] Shiue I, Hristova K. Higher urinary heavy metal, phthalate and arsenic concentrations accounted for 3-19% of the population attributable risk for high blood pressure: US NHANES, 2009-2012 [J]. Hypertens. Res., 2014, 37: 1075
doi: 10.1038/hr.2014.121 pmid: 25077919
[62] Schroeder H A, Kraemer L A. Cardiovascular mortality, municipal water, and corrosion [J]. Arch. Environ. Health: Int. J., 1974, 28: 303
doi: 10.1080/00039896.1974.10666497
[63] Bortolotti M, Polito L, Battelli M G, et al. Xanthine oxidoreductase: One enzyme for multiple physiological tasks [J]. Redox Biol., 2021, 41: 101882
doi: 10.1016/j.redox.2021.101882
[64] He W L, Kwesiga M P, Gebreyesus E, et al. Nitric oxide and oxidative stress-mediated cardiovascular functionality: From molecular mechanism to cardiovascular disease [A]. Vascular Biology-Selection of Mechanisms and Clinical Applications [M]. London: IntechOpen, 2019: 78
[65] Byon C H, Heath J M, Chen Y B. Redox signaling in cardiovascular pathophysiology: A focus on hydrogen peroxide and vascular smooth muscle cells [J]. Redox Biol, 2016, 9: 244
doi: S2213-2317(16)30126-4 pmid: 27591403
[66] Beckman J S, Koppenol W H. Nitric oxide, superoxide, and peroxynitrite: The good, the bad, and ugly [J]. Am. J. Physiol. Cell Physiol., 1996, 271: C1424
doi: 10.1152/ajpcell.1996.271.5.C1424
[67] White C R, Brock T A, Chang L Y, et al. Superoxide and peroxynitrite inatherosclerosis. [J]. Proc. Natl. Acad. Sci. USA, 1994, 91: 1044
pmid: 8302829
[68] Leeuwenburgh C, Hardy M M, Hazen S L, et al. Reactive nitrogen intermediates promote low density lipoprotein oxidation in human atherosclerotic intima [J]. J. Biol. Chem., 1997, 272: 1433
doi: 10.1074/jbc.272.3.1433 pmid: 8999808
[69] Patetsios P, Song M, Shutze W P, et al. Identification of uric acid and xanthine oxidase in atherosclerotic plaque [J]. Am. J. Cardiol., 2001, 88: 188
pmid: 11448423
[70] Nomura J, Busso N, Ives A, et al. Xanthine oxidase inhibition by febuxostat attenuates experimental atherosclerosis in mice [J]. Sci. Rep., 2014, 4: 4554
doi: 10.1038/srep04554 pmid: 24686534
[71] Koval’Skii V V, Iarovaia G A, Shmavonian D M. Modification of human and animal purine metabolism in conditions of various molybdenum bio-geochemical areas [J]. Zh. Obshch. Biol., 1961, 22: 179
[72] Yan Z Y, Liu Z X, Yang B W, et al. Long-term exposure of molybdenum disulfide nanosheets leads to hepatic lipid accumulation and atherogenesis in apolipoprotein E deficient mice [J]. NanoImpact, 2023, 30: 100462
doi: 10.1016/j.impact.2023.100462
[73] Sikora-Jasinska M, Morath L M, Kwesiga M P, et al. In-vivo evaluation of molybdenum as bioabsorbable stent candidate [J]. Bioact. Mater., 2022, 14: 262
doi: 10.1016/j.bioactmat.2021.11.005 pmid: 35310360
[74] Schauer A, Redlich C, Scheibler J, et al. Biocompatibility and degradation behavior of molybdenum in an in vivo rat model [J]. Materials, 2021, 14: 7776
doi: 10.3390/ma14247776
[75] Shen Y N, Huang Y M, Zhang Y, et al. Ultrafine molybdenum wire braided neurointerventional implants: Bridging biodegradability and neurovascular safety for stroke treatment [J]. Adv. Sci., 2026, 13: e11466
doi: 10.1002/advs.v13.1
[76] Curry E J, Ke K, Chorsi M T, et al. Biodegradable piezoelectric force sensor [J]. Proc. Natl. Acad. Sci. USA, 2018, 115: 909
doi: 10.1073/pnas.1710874115 pmid: 29339509
[77] Kang S K, Murphy R K J, Hwang S W, et al. Bioresorbable silicon electronic sensors for the brain [J]. Nature, 2016, 530: 71
doi: 10.1038/nature16492
[78] Yin L, Huang X, Xu H X, et al. Materials, designs, and operational characteristics for fully biodegradable primary batteries [J]. Adv. Mater., 2014, 26: 3879
doi: 10.1002/adma.v26.23
[79] Yu K J, Kuzum D, Hwang S W, et al. Bioresorbable silicon electronics for transient spatiotemporal mapping of electrical activity from the cerebral cortex [J]. Nat. Mater., 2016, 15: 782
doi: 10.1038/nmat4624
[80] Yang Q S, Liu T L, Xue Y G, et al. Ecoresorbable and bioresorbable microelectromechanical systems [J]. Nat. Electron., 2022, 5: 526
doi: 10.1038/s41928-022-00791-1
[81] Song J W, Ryu H, Bai W B, et al. Bioresorbable, wireless, and battery-free system for electrotherapy and impedance sensing at wound sites [J]. Sci. Adv., 2023, 9: eade4687
doi: 10.1126/sciadv.ade4687
[82] Hu P, Yang F, Wang K S, et al. Preparation and ductile-to-brittle transition temperature of the La-TZM alloy plates [J]. Int. J. Refract. Met. Hard Mater., 2015, 52: 131
doi: 10.1016/j.ijrmhm.2015.05.006
[83] Chen X C, Wang C, Ju H J, et al. Microstructure, room-temperature mechanical properties, and oxidation resistance of Ti-added Mo-Si-B alloys fabricated via hot pressing sintering [J]. J. Alloys Compd., 2025, 1010: 177634
doi: 10.1016/j.jallcom.2024.177634
[84] Cheng P M, Yang C, Zhang P, et al. Enhancing the high-temperature creep properties of Mo alloys via nanosized La2O3 particle addition [J]. J. Mater. Sci. Technol., 2022, 130: 53
doi: 10.1016/j.jmst.2022.04.043
[85] Hu W Q, Du Z F, Dong Z Z, et al. The synthesis of TiC dispersed strengthened Mo alloy by freeze-drying technology and subsequent low temperature sintering [J]. Scr. Mater., 2021, 198: 113831
doi: 10.1016/j.scriptamat.2021.113831
[86] Chen Y J, Fang Y, Cheng P M, et al. The origin of exceptionally large ductility in molybdenum alloys dispersed with irregular-shaped La2O3 nano-particles [J]. Nat. Commun., 2024, 15: 4105
doi: 10.1038/s41467-024-48439-2
[87] Liu Y, Zheng Y F, Chen X H, et al. Fundamental theory of biodegradable metals—Definition, criteria, and design [J]. Adv. Funct. Mater., 2019, 29: 1805402
doi: 10.1002/adfm.v29.18
[88] Ashby M F, Cebon D. Materials selection in mechanical design [J]. J. Phys. IV France, 1993, 3: C7-1
[89] Dang W T, Wang X Y, Li J Y, et al. 3D printing of Mo-containing scaffolds with activated anabolic responses and bi-lineage bioactivities [J]. Theranostics, 2018, 8: 4372
doi: 10.7150/thno.27088 pmid: 30214627
[90] Tian B M, Li X, Zhang J J, et al. A 3D-printed molybdenum-containing scaffold exerts dual pro-osteogenic and anti-osteoclastogenic effects to facilitate alveolar bone repair [J]. Int. J. Oral Sci., 2022, 14: 45
doi: 10.1038/s41368-022-00195-z
[91] He X T, Li X, Zhang M, et al. Role of molybdenum in material immunomodulation and periodontal wound healing: Targeting immunometabolism and mitochondrial function for macrophage modulation [J]. Biomaterials, 2022, 283: 121439
doi: 10.1016/j.biomaterials.2022.121439
[92] Liu D Y, Chen J H, Zhou J N, et al. Macrophage-related inflammatory responses to degradation products of biodegradable molybdenum implants [J]. Mater. Today Bio, 2025, 31: 101519
[93] Jing K, Liu R, Xie Z M, et al. Excellent high-temperature strength and ductility of the ZrC nanoparticles dispersed molybdenum [J]. Acta Mater., 2022, 227: 117725
doi: 10.1016/j.actamat.2022.117725
[94] Liu G, Zhang G J, Jiang F, et al. Nanostructured high-strength molybdenum alloys with unprecedented tensile ductility [J]. Nat. Mater., 2013, 12: 344
doi: 10.1038/nmat3544 pmid: 23353630
[95] Shi C X, Li H D, Zhou L. Materials Science and Engineering Handbook [M]. Beijing: Chemical Industry Press, 2004: 16
[95] 师昌绪, 李恒德, 周 廉. 材料科学与工程手册 [M]. 北京: 化学工业出版社, 2004: 16
[1] 吕昭平, 申耀祖, 王先珍, 陈强, 唐建国, 张晓宾, 于勇, 蒋虽合, 刘雄军, 王辉, 吴渊. 面向极端服役条件的高熵合金结构材料:性能优势、瓶颈与突破路径[J]. 金属学报, 2026, 62(5): 743-755.
[2] 陈光, 陈奉锐, 朱德民, 李贵忠, 李罗, 宋伟东, 王子特, 相恒高, 陈旸, 祁志祥. 聚片孪生功能基元序构的高性能TiAl合金[J]. 金属学报, 2026, 62(4): 541-549.
[3] 梁涛, 杜云波, 陈协辉, 潘浩波. 生物可降解纯Mg表面BA + Alg@Ca复合涂层的制备及其体外生物相容性[J]. 金属学报, 2026, 62(4): 669-684.
[4] 王建峰, 许珍木, 刘战, 高转妮, 占小红. 超声振动对TC4钛合金窄间隙激光焊接组织及强化机理的影响[J]. 金属学报, 2026, 62(3): 406-420.
[5] 蒋志达, 胥杨洋, 于佳新, 刘文才, 朱浩文, 吴国华, 尚郑平. 高温无氧轧制Cu/1060Al/Cu三层复合材料的力学和导电性能[J]. 金属学报, 2026, 62(3): 431-444.
[6] 江国龙, 周霞. 超声辅助下Mg/Mg-Zn-Al钎焊界面行为的分子动力学模拟[J]. 金属学报, 2026, 62(2): 372-382.
[7] 王启勇, 李晓博, 刘小超, 王心成, 张泰瑞, 倪中华, 陈彪. 低碳钢预制涡流搅拌摩擦焊工艺研究[J]. 金属学报, 2026, 62(1): 217-234.
[8] 张天宇, 张鹏, 肖娜, 王小海, 刘国强, 杨志刚, 张弛. 奥氏体化温度对2 GPa超高强钢显微组织和力学性能的影响[J]. 金属学报, 2025, 61(9): 1353-1363.
[9] 王洪瑛, 姚志浩, 李大禹, 郭婧, 姚凯俊, 董建新. 高 γ' 相含量粉末及变形高温合金组织和力学性能的异同性[J]. 金属学报, 2025, 61(9): 1364-1374.
[10] 吴志勇, 邵徽凡, 蔡长春, 曾敏, 王振军, 王艳丽, 陈雷, 熊博文. 斜纹碳布缝合织物结构增强铝基复合材料的高温拉伸及断裂行为[J]. 金属学报, 2025, 61(9): 1387-1402.
[11] 毕健浩男, 张艳, 王振玉, 周晟昊, 刘永跃, 张小岩, 汪爱英. Mo含量对CrAlMoN涂层微观结构、力学性能及摩擦学性能的影响[J]. 金属学报, 2025, 61(9): 1413-1424.
[12] 肖文龙, 臧晨阳, 郭锦涛, 冯佳文, 马朝利. 基于原位电阻法的7A65铝合金厚板双级时效工艺[J]. 金属学报, 2025, 61(8): 1153-1164.
[13] 刘继浩, 迟宏宵, 武会宾, 马党参, 周健, 谷金波. 喷射成形工艺对M3高速钢碳化物特征及力学性能的影响[J]. 金属学报, 2025, 61(8): 1229-1244.
[14] 葛蓬华, 张勇, 李志明. 异构FeCoNi中熵合金的软磁与力学行为[J]. 金属学报, 2025, 61(7): 1119-1128.
[15] 谢昂, 陈胜虎, 姜海昌, 戎利建. Nb含量和均质化处理对奥氏体不锈钢铸态组织和力学性能的影响[J]. 金属学报, 2025, 61(7): 1035-1048.