Please wait a minute...
金属学报  2026, Vol. 62 Issue (10): 1655-1675    DOI: 10.11900/0412.1961.2024.00428
  综述 本期目录 | 过刊浏览 |
耐事故燃料包壳用FeCrAl合金的腐蚀与辐照性能研究进展
杜东海1,2(), 林腾鸿1,2, 王辉3()
1 西北工业大学 长三角研究院 太仓 215400
2 西北工业大学 清洁能源研究院 太仓 215400
3 四川大学 材料科学与工程学院 成都 610065
Research Progress on Corrosion and Irradiation Performance of Accident-Tolerant Fuel Cladding FeCrAl Alloy
DU Donghai1,2(), LIN Tenghong1,2, WANG Hui3()
1 Yangtze River Delta Research Institute, Northwestern Polytechnical University, Taicang 215400, China
2 Institute of Clean Energy, Northwestern Polytechnical University, Taicang 215400, China
3 College of Materials Science and Engineering, Sichuan University, Chengdu 610065, China
引用本文:

杜东海, 林腾鸿, 王辉. 耐事故燃料包壳用FeCrAl合金的腐蚀与辐照性能研究进展[J]. 金属学报, 2026, 62(10): 1655-1675.
Donghai DU, Tenghong LIN, Hui WANG. Research Progress on Corrosion and Irradiation Performance of Accident-Tolerant Fuel Cladding FeCrAl Alloy[J]. Acta Metall Sin, 2026, 62(10): 1655-1675.

全文: PDF(1620 KB)   HTML
摘要: 

在日本福岛核事故中,锆合金燃料包壳在高温下与蒸汽快速反应,在短时间内发生破裂,反应产生的H2引起爆炸,导致放射性物质泄漏,给公众安全和生态环境造成灾难性后果。为提高燃料包壳在严重失水事故下的安全性,核工业界提出了开发耐事故燃料包壳替代原有锆合金包壳的思路。近十几年来,国内外针对耐事故燃料包壳的研发开展了大量工作,其中FeCrAl合金因其优异的抗高温蒸汽腐蚀性能、较好的力学性能以及良好的抗辐照性能,成为中长期内候选包壳材料的重点研究对象,合金的成分筛选、加工制备、服役性能评价已取得较大进展,全尺寸管已进入中子辐照考验的关键阶段。本文围绕核级FeCrAl合金在正常工况和事故工况下的服役性能,介绍了其在高温水中的抗均匀腐蚀和应力腐蚀性能及影响因素、在高温蒸汽中的氧化性能及影响因素,总结了辐照对合金微观组织和力学性能的影响规律,分析了辐照对均匀腐蚀和应力腐蚀的加速作用,以期为合理评价FeCrAl合金服役性能和优化合金提供参考。

关键词 : FeCrAl合金,  腐蚀,  辐照,  微观组织,  服役性能    
Abstract:

The Fukushima nuclear accident in Japan highlighted the susceptibility of zirconium alloy fuel claddings. Exposure to high temperatures caused the cladding to react rapidly with steam, resulting in the release of hydrogen and subsequent explosions. These events led to significant radioactive leakage, posing substantial risks to public and environmental safety. To mitigate these risks, accident-tolerant fuel claddings have been proposed as a replacement for traditional zirconium alloy claddings. In recent years, research has focused on developing accident-resistant cladding materials domestically and internationally. FeCrAl alloys have emerged as key materials for medium- and long-term fuel cladding solutions because of their exceptional resistance to high-temperature steam corrosion and superior performance under irradiation. Significant progress has been made in the screening of alloy compositions, the optimization of processing methods, and the evaluation of service performance. Full-scale FeCrAl tubes have progressed to the critical stage of neutron irradiation tests. This paper comprehensively reviews nuclear-grade FeCrAl alloys and evaluates their performance under normal and accident conditions. This review examines the uniform and stress-corrosion behavior of FeCrAl alloys in high-temperature water, the factors influencing these properties, and their oxidation performance in high-temperature steam. The paper also summarizes the impact of irradiation on the alloy's microstructure and mechanical properties, highlighting the role of irradiation in accelerating uniform and stress corrosion. This analysis provides significant insights into the service performance of FeCrAl alloys and offers valuable knowledge to support their continued optimization as enhanced, accident-tolerant fuel cladding materials.

Key words: FeCrAl alloy    corrosion    irradiation    microstructure    service performance
收稿日期: 2024-12-18     
ZTFLH:  TL341  
基金资助:国家自然科学基金项目(12375273);国家自然科学基金项目(52122103)
通讯作者: 杜东海,dudonghai@nwpu.edu.cn,主要从事核材料高温腐蚀研究;
王辉,qinghe5525@163.com,主要从事核材料制备和服役性能研究
Corresponding author: DU Donghai, associate professor, Tel: 18817556270, E-mail: dudonghai@nwpu.edu.cn;
WANG Hui, professor, Tel: 13709081432, E-mail: qinghe5525@163.com
作者简介: 杜东海,男,1987年生,副教授,博士
图1  FeCrAl合金在高温水中的腐蚀过程示意图[20]
图2  Fe-10Cr与Fe-18Cr合金在沸水堆(BWR)和压水堆(PWR)环境条件下的Pourbaix图[22]
图3  FeCrAl合金慢拉伸实验后样品氧化膜的表征[50]
图4  Cr与Al含量对商业和模型FeCrAl合金1200 ℃高温蒸汽氧化性能的影响[9]
图5  在1200 ℃蒸汽环境中含Y FeCrAl合金的氧化行为随时间、Y含量变化的示意图[86]
图6  FeCrAl合金的位错环尺寸以及<100>与1/2<111>位错环中值尺寸之比随辐照剂量的变化[121]
图7  辐照后不同类型FeCrAl合金中αʹ析出相的数量密度及其与Cr、Al含量的关系[79]
图8  400 keV Fe+辐照下辐照剂量和辐照温度对Laves相溶解行为的影响[146]
图9  离子辐照后FeCrAl合金纳米压痕硬度与辐照剂量的关系[124]
图10  T35Y2合金在模拟PWR环境内耦合质子辐照下的腐蚀形貌[170]
图11  辐照后ODS-FeCrAl合金Al2O3氧化膜中Y-Zr在晶界的分布[178](ODS表示氧化物弥散强化)
[1] Zinkle S J, Terrani K A, Gehin J C, et al. Accident tolerant fuels for LWRs: A perspective[J]. J. Nucl. Mater., 2014, 448: 374
doi: 10.1016/j.jnucmat.2013.12.005
[2] Terrani K A. Accident tolerant fuel cladding development: Promise, status, and challenges[J]. J. Nucl. Mater., 2018, 501: 13
doi: 10.1016/j.jnucmat.2017.12.043
[3] Yun D, Lu C Y, Zhou Z J, et al. Current state and prospect on the development of advanced nuclear fuel system materials: A review[J]. Mater. Rep. Energy, 2021, 1: 100007
[4] Savchenko A M, Karpyuk L A, Novikov V V, et al. New ATF concepts and materials: Evaluation and investigations[R]. Analysis of Options and Experimental Examination of Fuels for Water Cooled Reactors with Increased Accident Tolerance (ACTOF) IAEA-TECDOC—1921, Vienna: International Atomic Energy Agency, 2020: 155
[5] Tang C C, Stueber M, Seifert H J, et al. Protective coatings on zirconium-based alloys as accident-tolerant fuel (ATF) claddings[J]. Corros. Rev., 2017, 35: 141
doi: 10.1515/corrrev-2017-0010
[6] Liu J K, Zhang X H, Yun D. A complete review and a prospect on the candidate materials for accident-tolerant fuel claddings[J]. Mater. Rep., 2018, 32: 1757
[6] 刘俊凯, 张新虎, 恽 迪. 事故容错燃料包壳候选材料的研究现状及展望[J]. 材料导报, 2018, 32: 1757
[7] Tangirbergen A, Amangeldi N, Revankar S T, et al. A review of irradiation-induced hardening in FeCrAl alloy systems for accident-tolerant fuel cladding[J]. Nucl. Eng. Des., 2024, 429: 113659
doi: 10.1016/j.nucengdes.2024.113659
[8] Terrani K A, Zinkle S J, Snead L L. Advanced oxidation-resistant iron-based alloys for LWR fuel cladding[J]. J. Nucl. Mater., 2014, 448: 420
doi: 10.1016/j.jnucmat.2013.06.041
[9] Yamamoto Y, Pint B A, Terrani K A, et al. Development and property evaluation of nuclear grade wrought FeCrAl fuel cladding for light water reactors[J]. J. Nucl. Mater., 2015, 467: 703
doi: 10.1016/j.jnucmat.2015.10.019
[10] Colldeweih A W, Petersen P G, Matos M D, et al. Post irradiation examinations of FeCrAl cladding in PWR conditions[J]. J. Nucl. Mater., 2025, 603: 155402
doi: 10.1016/j.jnucmat.2024.155402
[11] Rebak R B. Improved and innovative accident-tolerant nuclear fuel materials considered for retrofitting light water reactors—A review[J]. Corros. Mater. Degrad., 2023, 4: 466
doi: 10.3390/cmd4030024
[12] Qian L B, Liu Y, Huang T, et al. Research progress in high-temperature thermo-mechanical behavior for modelling FeCrAl cladding under loss-of-coolant accident condition[J]. Prog. Nucl. Energy, 2023, 164: 104848
doi: 10.1016/j.pnucene.2023.104848
[13] Ukai S, Sakamoto K, Ohtsuka S, et al. Alloy design and characterization of a recrystallized FeCrAl-ODS cladding for accident-tolerant BWR fuels: An overview of research activity in Japan[J]. J. Nucl. Mater., 2023, 583: 154508
doi: 10.1016/j.jnucmat.2023.154508
[14] Wang X, Shen X P. Research progress of ODS FeCrAl alloys—A review of composition design[J]. Materials, 2023, 16: 6280
doi: 10.3390/ma16186280
[15] Qiu G X, Wei X L, Miao D J, et al. Research progress of nuclear FeCrAl cladding materials[J]. J. Iron Steel Res., 2022, 34: 884
doi: 10.13228/j.boyuan.issn1001-0963.20210342
[15] 邱国兴, 韦旭立, 缪德军 等. 核级FeCrAl包壳材料研究进展[J]. 钢铁研究学报, 2022, 34: 884
doi: 10.13228/j.boyuan.issn1001-0963.20210342
[16] Huang X, Li X Y, Fang X D, et al. Research progress in FeCrAl alloys for accident-tolerant fuel cladding[J]. J. Mater. Eng., 2020, 48(3): 19
doi: 10.11868/j.issn.1001-4381.2018.001165
[16] 黄 希, 李小燕, 方晓东 等. 容错事故燃料包壳用FeCrAl合金的研究进展[J]. 材料工程, 2020, 48(3): 19
[17] Tao X K, Huang Z G, Guo Q M, et al. Research progress of FeCrAl alloy for cladding material of new type of light water reactor[J]. Hot Work. Technol., 2018, 47(6): 23
[17] 陶小康, 黄重国, 郭青苗 等. 新型轻水反应堆包壳材料FeCrAl合金的研究进展[J]. 热加工工艺, 2018, 47(6): 23
[18] Zhou J, Qiu S Y, Du P N, et al. Research progress in the FeCrAl alloys for accident tolerant fuel cladding[J]. Mater. Rep., 2017, 31(suppl.2) : 47
[18] 周 军, 邱绍宇, 杜沛南 等. 耐事故燃料包壳用FeCrAl不锈钢的研究进展[J]. 材料导报, 2017, 31(增刊2): 47
[19] Jiang G Y, Xu D H, Feng P, et al. Corrosion of FeCrAl alloys used as fuel cladding in nuclear reactors[J]. J. Alloys Compd., 2021, 869: 159235
doi: 10.1016/j.jallcom.2021.159235
[20] Lin X D, Liang X, Li Y F, et al. Microstructural understanding of general and localized corrosion of Fe13Cr4Al2Mo1.2Nb alloy in high temperature aerated water and superheated steam[J]. Corros. Sci., 2022, 203: 110341
doi: 10.1016/j.corsci.2022.110341
[21] Rebak R B, Larsen M, Kim Y J. Characterization of oxides formed on iron-chromium-aluminum alloy in simulated light water reactor environments[J]. Corros. Rev., 2017, 35: 177
doi: 10.1515/corrrev-2017-0011
[22] Terrani K A, Pint B A, Kim Y J, et al. Uniform corrosion of FeCrAl alloys in LWR coolant environments[J]. J. Nucl. Mater., 2016, 479: 36
doi: 10.1016/j.jnucmat.2016.06.047
[23] Kim Y J, Wagenbaugh F, Jurewicz T B, et al. Environmental behavior of light water reactor accident tolerant candidate cladding materials under design conditions[A]. Proceedings of the CORROSION 2015[C]. Dallas: NACE, 2015: 5817
[24] Jiang G Y, Xu D H, Wei Y, et al. Corrosion of Zircaloy-4, Zr-1Nb and FeCrAl alloys in deaerated water at 330 oC and 14 MPa: Superior corrosion resistance and corrosion mechanism of FeCrAl alloy by experiments and molecular dynamics simulations[J]. Chem. Eng. J., 2023, 462: 142143
doi: 10.1016/j.cej.2023.142143
[25] Liao J J, Wang H, Wu J, et al. Addition of niobium in Fe-13Cr-4.5Al-2Mo alloy used as ATF cladding: Effect on high temperature water corrosion and in-situ electrochemistry[J]. Mater. Des., 2022, 220: 110854
doi: 10.1016/j.matdes.2022.110854
[26] Ning F Q, Wang X, Yang Y, et al. Uniform corrosion behavior of FeCrAl alloys in borated and lithiated high temperature water[J]. J. Mater. Sci. Technol., 2021, 70: 136
doi: 10.1016/j.jmst.2020.07.026
[27] Jiang G Y, Xu D H, Yang W P, et al. Incipient corrosion of FeCrAl alloys in H3BO3- and LiOH-containing pure water at 360 oC and 18.5 MPa[J]. J. Nucl. Mater., 2021, 557: 153299
doi: 10.1016/j.jnucmat.2021.153299
[28] Yin L, Jurewicz T B, Larsen M, et al. Uniform corrosion of FeCrAl cladding tubing for accident tolerant fuels in light water reactors[J]. J. Nucl. Mater., 2021, 554: 153090
doi: 10.1016/j.jnucmat.2021.153090
[29] Li J, Wu S J, Yang Y, et al. Study on corrosion resistance of ODS-FeCrAl tube for ATF[J]. Nucl. Power Eng., 2021, 42(4): 119
[29] 李 静, 吴飒建, 杨 英 等. ATF用ODS-FeCrAl管材的耐腐蚀性能研究[J]. 核动力工程, 2021, 42(4): 119
[30] Raiman S S, Field K G, Rebak R B, et al. Hydrothermal corrosion of 2nd generation FeCrAl alloys for accident tolerant fuel cladding[J]. J. Nucl. Mater., 2020, 536: 152221
doi: 10.1016/j.jnucmat.2020.152221
[31] Li N, Parker S S, Saleh T A, et al. Intermediate temperature corrosion behaviour of Fe-12Cr-6Al-2Mo-0.2Si-0.03Y alloy (C26M) at 300-600 °C[J]. Corros. Sci., 2019, 157: 274
doi: 10.1016/j.corsci.2019.05.029
[32] Park D J, Kim H G, Park J Y, et al. A study of the oxidation of FeCrAl alloy in pressurized water and high-temperature steam environment[J]. Corros. Sci., 2015, 94: 459
doi: 10.1016/j.corsci.2015.02.027
[33] Joyce L, Wang P, Umretiya R V, et al. Oxide layers in Ni-doped FeCrAl alloy in 320 oC radioactive hydrogenated water[J]. J. Nucl. Mater., 2024, 593: 154987
doi: 10.1016/j.jnucmat.2024.154987
[34] Nagothi B S, Qu H Z, Zhang W M, et al. Hydrothermal corrosion of latest generation of FeCrAl alloys for nuclear fuel cladding[J]. Materials, 2024, 17: 1633
doi: 10.3390/ma17071633
[35] Hu Y H, Ling Y H, Zhao X F, et al. Corrosion of FeCrAl-1Nb alloy in deaerated water at 290 oC and 7 MPa: The oxidation behavior of grain boundary[J]. Corros. Sci., 2024, 235: 112159
doi: 10.1016/j.corsci.2024.112159
[36] Hu Y H, Ling Y H, Wang W P, et al. Corrosion behavior of Laves precipitates in FeCrAl-1Nb alloy at 290 oC and 7 MPa: The size effect and critical role of pH[J]. Corros. Sci., 2024, 240: 112498
doi: 10.1016/j.corsci.2024.112498
[37] Kuang W J, Han E H, Wu X Q, et al. Microstructural characteristics of the oxide scale formed on 304 stainless steel in oxygenated high temperature water[J]. Corros. Sci., 2010, 52: 3654
doi: 10.1016/j.corsci.2010.07.015
[38] Terachi T, Arioka K. Characterization of oxide film behaviors on 316 stainless steels in high temperature water—Influence of hydrogen and oxygen considerations for initiation of SCC[A]. Proceedings of the CORROSION 2006[C]. San Diego: NACE, 2006: 06608
[39] Wright I G, Dooley R B. A review of the oxidation behaviour of structural alloys in steam[J]. Int. Mater. Rev., 2010, 55: 129
doi: 10.1179/095066010X12646898728165
[40] Robertson J. The mechanism of high temperature aqueous corrosion of stainless steels[J]. Corros. Sci., 1991, 32: 443
doi: 10.1016/0010-938X(91)90125-9
[41] Lin X D, Ma H B, Ren Q S, et al. Corrosion behaviors of Fe13Cr5Al4Mo alloy in high-temperature high-pressure water environments[J]. Acta Metall. Sin., 2022, 58: 1611
doi: 10.11900/0412.1961.2021.00574
[41] 林晓冬, 马海滨, 任啟森 等. Fe13Cr5Al4Mo合金在高温高压水环境中的腐蚀行为[J]. 金属学报, 2022, 58: 1611
doi: 10.11900/0412.1961.2021.00574
[42] Rebak R B, Jurewicz T B, Kim Y. Oxidation resistance of FeCrAl in simulated BWR and PWR water chemistries[A]. 2017 Water Reactor Fuel Performance Meeting[C]. Jeju Island, Republic of Korea, 2017
[43] Xie J Y, Ma X, Kuang W J. Improving the corrosion resistance of FeCrAl alloy in high temperature hydrogenated water through gaseous pre-oxidation[J]. Corros. Commun., 2024, 15: 36
doi: 10.1016/j.corcom.2024.03.001
[44] Rebak R B. Versatile oxide films protect FeCrAl alloys under normal operation and accident conditions in light water power reactors[J]. JOM, 2018, 70: 176
doi: 10.1007/s11837-017-2705-z
[45] Qu H J, Abouelella H, Chikhalikar A S, et al. Effect of nickel on the oxidation behavior of FeCrAl alloy in simulated PWR and BWR conditions[J]. Corros. Sci., 2023, 216: 111093
doi: 10.1016/j.corsci.2023.111093
[46] Rebak R B, Yin L, Zhang W M, et al. Effect of the redox potential on the general corrosion behavior of industrial nuclear alloys[J]. J. Nucl. Mater., 2023, 576: 154257
doi: 10.1016/j.jnucmat.2023.154257
[47] Rebak R B, Jurewicz T B, Larsen M, et al. Zinc water chemistry reduces dissolution of FeCrAl for nuclear fuel cladding[J]. Corros. Sci., 2022, 198: 110156
doi: 10.1016/j.corsci.2022.110156
[48] Xue C C, Zhang Z Y, Tan J B, et al. Effects of Zn injection on corrosion behavior and crud deposition of FeCrAl fuel cladding under subcooled nuclear boiling condition in high-temperature pressurized water[J]. Corros. Sci., 2023, 211: 110909
doi: 10.1016/j.corsci.2022.110909
[49] Rebak R B, Yin L, Andresen P L. Resistance of ferritic FeCrAl alloys to stress corrosion cracking for light water reactor fuel cladding applications[J]. Corrosion, 2020, 76: 3632
[50] Xie J Y, Zhang S H, Dong J Y, et al. Insights into the superior stress corrosion cracking resistance of FeCrAl alloy in high temperature hydrogenated water: the critical role of grain boundary oxidation[J]. Corros. Sci., 2022, 208: 110668
doi: 10.1016/j.corsci.2022.110668
[51] Sakamoto K, Miura Y, Ukai S, et al. Development of accident tolerant FeCrAl-ODS fuel cladding for BWRs in Japan[J]. J. Nucl. Mater., 2021, 557: 153276
doi: 10.1016/j.jnucmat.2021.153276
[52] Xiao T, Xiao J, Chen Y, et al. Stress corrosion behavior of FeCrAl ferrite stainless steel under PWR water deviation condition[J]. At. Energy Sci. Technol., 2019, 53: 414
[52] 肖 婷, 肖 军, 陈 勇 等. FeCrAl铁素体不锈钢在压水堆水化学偏离工况下的应力腐蚀行为[J]. 原子能科学技术, 2019, 53: 414
[53] Kim C, Tang C C, Grosse M, et al. Oxidation mechanism and kinetics of nuclear-grade FeCrAl alloys in the temperature range of 500-1500 oC in steam[J]. J. Nucl. Mater., 2022, 564: 153696
doi: 10.1016/j.jnucmat.2022.153696
[54] Qian Y, Sun R R, Zhang W H, et al. Effect of Nb on microstructure and corrosion resistance of Fe22Cr5Al3Mo alloy[J]. Acta Metall. Sin., 2020, 56: 321
doi: 10.11900/0412.1961.2019.00276
[54] 钱 月, 孙蓉蓉, 张文怀 等. Nb对Fe22Cr5Al3Mo合金显微组织和耐腐蚀性能的影响[J]. 金属学报, 2020, 56: 321
[55] Sun R R, Yao M Y, Lin X D, et al. Effect of Ti on the corrosion behavior of Fe22Cr5Al3Mo alloy in 500 oC superheated steam[J]. Acta Metall. Sin., 2022, 58: 610
[55] 孙蓉蓉, 姚美意, 林晓冬 等. 添加Ti对Fe22Cr5Al3Mo合金在500 ℃过热蒸汽中腐蚀行为的影响[J]. 金属学报, 2022, 58: 610
doi: 10.11900/0412.1961.2021.00200
[56] Sun R R, Yao M Y, Zhang J, et al. Effect of Y on the corrosion behavior of Fe22Cr5Al3Mo alloy in 500 oC super-heated steam[J]. Corros. Sci., 2022, 196: 110022
doi: 10.1016/j.corsci.2021.110022
[57] El Kadiri H, Molins R, Bienvenu Y, et al. Abnormal high growth rates of metastable aluminas on FeCrAl alloys[J]. Oxid. Met., 2005, 64: 63
doi: 10.1007/s11085-005-5715-0
[58] Kim C, Kim H, Heo W, et al. High-temperature steam oxidation behavior of alumina-forming duplex FeNiCrAl and ferritic FeCrAl alloys at 800 oC to 1050 oC[J]. Corros. Sci., 2021, 190: 109658
doi: 10.1016/j.corsci.2021.109658
[59] Berthomé G, N'Dah E, Wouters Y, et al. Temperature dependence of metastable alumina formation during thermal oxidation of FeCrAl foils[J]. Mater. Corros., 2005, 56: 389
doi: 10.1002/(ISSN)1521-4176
[60] Rebak R B, Gupta V K, Larsen M. Oxidation characteristics of two FeCrAl alloys in air and steam from 800 oC to 1300 oC[J]. JOM, 2018, 70: 1484
doi: 10.1007/s11837-018-2979-9
[61] Falaakh D F, Kim S, Bahn C B. Microstructure of aluminium oxide formed on ferritic FeCrAl alloy after high-temperature steam oxidation[J]. Mater. High Temp., 2020, 37: 207
doi: 10.1080/09603409.2020.1742526
[62] Dryepondt S, Unocic K A, Hoelzer D T, et al. Development of low-Cr ODS FeCrAl alloys for accident-tolerant fuel cladding[J]. J. Nucl. Mater., 2018, 501: 59
doi: 10.1016/j.jnucmat.2017.12.035
[63] Pint B A. Performance of FeCrAl for accident-tolerant fuel cladding in high-temperature steam[J]. Corros. Rev., 2017, 35: 167
doi: 10.1515/corrrev-2016-0067
[64] Narukawa T, Kondo K, Fujimura Y, et al. Oxidation and embrittlement behavior of FeCrAl-ODS cladding tube under loss-of-coolant accident conditions[J]. J. Nucl. Mater., 2023, 587: 154736
doi: 10.1016/j.jnucmat.2023.154736
[65] Lipkina K, Hallatt D, Geiger E, et al. A study of the oxidation behaviour of FeCrAl-ODS in air and steam environments up to 1400 oC[J]. J. Nucl. Mater., 2020, 541: 152305
doi: 10.1016/j.jnucmat.2020.152305
[66] McMurray J W, Hu R, Ushakov S V, et al. Solid-liquid phase equilibria of Fe-Cr-Al alloys and spinels[J]. J. Nucl. Mater., 2017, 492: 128
doi: 10.1016/j.jnucmat.2017.05.016
[67] Maeda T, Ukai S, Hayashi S, et al. Effects of zirconium and oxygen on the oxidation of FeCrAl-ODS alloys under air and steam conditions up to 1500 oC[J]. J. Nucl. Mater., 2019, 516: 317
doi: 10.1016/j.jnucmat.2019.01.041
[68] Bye G C, Simpkin G T. Influence of Cr and Fe on formation of α-Al2O3 from γ-Al2O3 [J]. J. Am. Ceram. Soc., 1974, 57: 367
doi: 10.1111/jace.1974.57.issue-8
[69] Yoneda S, Hayashi S, Ukai S. The transition from transient oxide to protective Al2O3 scale on Fe-Cr-Al alloys during heating to 1000 oC[J]. Oxid. Met., 2018, 89: 81
doi: 10.1007/s11085-017-9778-5
[70] Niu Y, Wang S, Gao F, et al. The nature of the third-element effect in the oxidation of Fe-xCr-3at.% Al alloys in 1atm O2 at 1000 oC[J]. Corros. Sci., 2008, 50: 345
doi: 10.1016/j.corsci.2007.06.019
[71] Tang C C, Jianu A, Steinbrueck M, et al. Influence of composition and heating schedules on compatibility of FeCrAl alloys with high-temperature steam[J]. J. Nucl. Mater., 2018, 511: 496
doi: 10.1016/j.jnucmat.2018.09.026
[72] Stott F H, Wood G C, Stringer J. The influence of alloying elements on the development and maintenance of protective scales[J]. Oxid. Met., 1995, 44: 113
doi: 10.1007/BF01046725
[73] Unocic K A, Yamamoto Y, Pint B A. Effect of Al and Cr content on air and steam oxidation of FeCrAl alloys and commercial APMT alloy[J]. Oxid. Met., 2017, 87: 431
doi: 10.1007/s11085-017-9745-1
[74] Pint B A, Terrani K A, Yamamoto Y, et al. Material selection for accident tolerant fuel cladding[J]. Metall. Mater. Trans., 2015, 2E: 190
[75] Pint B A, Unocic K A, Terrani K A. Effect of steam on high temperature oxidation behaviour of alumina-forming alloys[J]. Mater. High Temp., 2015, 32: 28
doi: 10.1179/0960340914Z.00000000058
[76] Chen G, Yang H Y, Sun H Y, et al. Exploring the high-temperature steam oxidation behaviors of the lean-Cr (7-10 wt%) FeCrAl alloys[J]. Corros. Sci., 2022, 194: 109927
doi: 10.1016/j.corsci.2021.109927
[77] Gussev M N, Field K G, Yamamoto Y. Design, properties, and weldability of advanced oxidation-resistant FeCrAl alloys[J]. Mater. Des., 2017, 129: 227
doi: 10.1016/j.matdes.2017.05.009
[78] Zhou X, Guo L P, Wei Y X, et al. Effect of aluminum content on dislocation loops in model FeCrAl alloys[J]. Nucl. Mater. Energy, 2019, 21: 100718
[79] Mao K S, Massey C P, Yamamoto Y, et al. Improved irradiation resistance of accident-tolerant high-strength FeCrAl alloys with heterogeneous structures[J]. Acta Mater., 2022, 231: 117843
doi: 10.1016/j.actamat.2022.117843
[80] Naumenko D, Pint B A, Quadakkers W J. Current thoughts on reactive element effects in alumina-forming systems: In memory of John Stringer[J]. Oxid. Met., 2016, 86: 1
doi: 10.1007/s11085-016-9625-0
[81] Amano T, Hara A, Sakai N, et al. Oxide adherence of Fe-20Cr-4Al alloys with small amounts of sulfur and reactive elements (Y, Hf)[J]. Mater. High Temp., 2000, 17: 117
doi: 10.1179/mht.2000.018
[82] Golightly F A, Stott F H, Wood G C. The influence of yttrium additions on the oxide-scale adhesion to an iron-chromium-aluminum alloy[J]. Oxid. Met., 1976, 10: 163
doi: 10.1007/BF00612158
[83] Yang Z, Pan J, Wang Z X, et al. New insights into the mechanism of yttrium changing high-temperature oxide growth of Fe-13Cr-6Al-2Mo-0.5Nb alloy for fuel cladding[J]. Corros. Sci., 2020, 172: 108728
doi: 10.1016/j.corsci.2020.108728
[84] Yu H, Kondo S, Kasada R, et al. Development of nano-oxide particles dispersed alumina scale formed on Zr-added FeCrAl ODS ferritic alloys[J]. Nucl. Mater. Energy, 2020, 25: 100798
[85] Kim S, Lee C H, Jang J H, et al. High-temperature steam oxidation of (Ti, Mo)C-forming FeCrAlY alloy[J]. J. Nucl. Mater., 2023, 574: 154220
doi: 10.1016/j.jnucmat.2022.154220
[86] Kim S, Lee C H, Kim T, et al. Effects of yttrium on the oxidation behavior of Fe13Cr6AlY alloys under 1200 oC steam[J]. J. Alloys Compd., 2023, 960: 170642
doi: 10.1016/j.jallcom.2023.170642
[87] Liu R, Sun H L, Guo Q Q, et al. A study of the oxidation of Gd-doped FeCrAl in 1000 oC steam environments[J]. J. Mater. Eng. Perform., 2023, 32: 978
doi: 10.1007/s11665-022-07161-0
[88] Li Q, Long D J, Song P, et al. Alumina grain growth and grain boundary segregation of FeCrAl-based oxide dispersion-strengthened alloys at high temperature[J]. Corros. Sci., 2022, 208: 110630
doi: 10.1016/j.corsci.2022.110630
[89] Qi W, Yang K, Wang P, et al. High-temperature steam oxidation behavior of an FeCrAl alloy with controlled addition of Mo[J]. J. Mater. Sci., 2022, 57: 20909
doi: 10.1007/s10853-022-07920-3
[90] Zhang W H, Qian Y, Sun R R, et al. Oxidation characteristics of Fe22Cr5Al3Mo-xNb alloys in high temperature steam[J]. Corros. Sci., 2021, 191: 109722
doi: 10.1016/j.corsci.2021.109722
[91] Huang T H, Naumenko D, Song P, et al. Effect of titanium addition on alumina growth mechanism on yttria-containing FeCrAl-base alloy[J]. Oxid. Met., 2018, 90: 671
doi: 10.1007/s11085-018-9861-6
[92] Hayashi S, Maeda T. Effect of Zr on initial oxidation behavior of FeCrAl alloys[J]. Oxid. Met., 2020, 93: 573
doi: 10.1007/s11085-020-09972-9
[93] Sigler D R. Adherence behavior of oxide grown in air and synthetic exhaust gas on Fe-Cr-Al alloys containing strong sulfide-forming elements: Ca, Mg, Y, Ce, La, Ti, and Zr[J]. Oxid. Met., 1993, 40: 555
doi: 10.1007/BF00666391
[94] Shibata H, Ukai S, Oono N H, et al. Development of accident tolerant FeCrAl-ODS steels utilizing Ce-oxide particles dispersion[J]. J. Nucl. Mater., 2018, 502: 228
doi: 10.1016/j.jnucmat.2018.02.020
[95] Li S, Yuan Y, Zhou R N, et al. Initial oxidation mechanism of FeCrAl thin films with Nb and Si additions[J]. Thin Solid Films, 2023, 782: 140015
doi: 10.1016/j.tsf.2023.140015
[96] Liu Y, Ma H B, Wu L X, et al. Effect of trace Y on mechanical and oxidation properties of FeCrAl alloy cladding[J]. Nucl. Tech., 2023, 46: 060202
[96] 刘 洋, 马海滨, 吴利翔 等. 微量Y对FeCrAl合金包壳力学与氧化性能的影响[J]. 核技术, 2023, 46: 060202
[97] Qu H J, Chikhalikar A S, Abouelella H, et al. Effect of molybdenum on the oxidation resistance of FeCrAl alloy in lower temperature (400 oC) and higher temperature (1200 oC) steam environments[J]. Corros. Sci., 2024, 229: 111870
doi: 10.1016/j.corsci.2024.111870
[98] Ozawa M, Araki K I. Effect of La modification on the stability of coating alumina layer on FeCrAl alloy substrate[J]. Surf. Coat. Technol., 2015, 271: 80
doi: 10.1016/j.surfcoat.2015.01.010
[99] Massey C P, Edmondson P D, Unocic K A, et al. The effect of Zr on precipitation in oxide dispersion strengthened FeCrAl alloys[J]. J. Nucl. Mater., 2020, 533: 152105
doi: 10.1016/j.jnucmat.2020.152105
[100] Jia H D, Zhang R Q, Long D J, et al. Effect of zirconium content on mechanical properties of ODS FeCrAl alloy[J]. Mater. Sci. Eng., 2022, A839: 142824
[101] Niu B, Wang Z H, Wang Q, et al. Effect of Zr addition on the stability of precipitated Laves phase and mechanical properties of Fe-Cr-Al-based alloys at high temperatures[J]. Prog. Nat. Sci. Mater. Int., 2022, 32: 114
doi: 10.1016/j.pnsc.2021.11.007
[102] Jia H D, Zhang R Q, Long D J, et al. Effect of zirconium content on the microstructure of ODS FeCrAl alloys[J]. Int. J. Energy Res., 2021, 45: 10226
doi: 10.1002/er.v45.7
[103] Shi Y N, Lu Z, Yu L, et al. Microstructure and tensile properties of Zr-containing ODS-FeCrAl alloy fabricated by laser additive manufacturing[J]. Mater. Sci. Eng., 2020, A774: 138937
[104] Massey C P, Dryepondt S N, Edmondson P D, et al. Multiscale investigations of nanoprecipitate nucleation, growth, and coarsening in annealed low-Cr oxide dispersion strengthened FeCrAl powder[J]. Acta Mater., 2019, 166: 1
doi: 10.1016/j.actamat.2018.11.062
[105] Naumenko D, Kochubey V, Niewolak L, et al. Modification of alumina scale formation on FeCrAlY alloys by minor additions of group IVa elements[J]. J. Mater. Sci., 2008, 43: 4550
doi: 10.1007/s10853-008-2639-5
[106] Yan Y Q, Ao J Q, Ji Y Q, et al. Cracking inhibition and strengthening of FeCrAlY alloy through addition of TiC nanoparticles during laser melting deposition[J]. Vacuum, 2023, 212: 112014
doi: 10.1016/j.vacuum.2023.112014
[107] Lv W J, Yang X S, Ji Y Q, et al. Effects of TiC nanoparticle additions on microstructure and mechanical properties of FeCrAl alloys prepared by directed energy deposition[J]. J. Nucl. Mater., 2021, 554: 153094
doi: 10.1016/j.jnucmat.2021.153094
[108] Wan H Y, An X G, Kong Q Q, et al. Fabrication of ultrafine grained FeCrAl-0.6wt.%ZrC alloys with enhanced mechanical properties by spark plasma sintering[J]. Adv. Powder Technol., 2021, 32: 1380
doi: 10.1016/j.apt.2021.02.041
[109] Ding R F, Wang H, Jiang Y, et al. Effects of ZrC addition on the microstructure and mechanical properties of Fe-Cr-Al alloys fabricated by spark plasma sintering[J]. J. Alloys Compd., 2019, 805: 1025
doi: 10.1016/j.jallcom.2019.07.181
[110] Wang H, Gao Y X, Sun M, et al. Strengthening mechanism of Nb addition in Fe-13Cr-4.5Al-2Mo alloys assessed by internal friction measurement[J]. J. Nucl. Mater., 2020, 542: 152461
doi: 10.1016/j.jnucmat.2020.152461
[111] Sun ZQ, Bei H B, Yamamoto Y. Microstructural control of FeCrAl alloys using Mo and Nb additions[J]. Mater. Charact., 2017, 132: 126
doi: 10.1016/j.matchar.2017.08.008
[112] Wang H, Gao Y X, Sun M, et al. Effects of Nb addition and heat treatment on the microstructure, mechanical property and internal friction behavior of FeCrAlMo cladding alloys[J]. J. Nucl. Mater., 2022, 572: 154044
doi: 10.1016/j.jnucmat.2022.154044
[113] Wen D H, Jiang B B, Wang Q, et al. Microstructure evolution at elevated temperature and mechanical properties of MoNb-modified FeCrAl stainless steel[J]. Acta Metall. Sin., 2022, 58: 883
doi: 10.11900/0412.1961.2020.00533
[113] 温冬辉, 姜贝贝, 王 清 等. MoNb改性FeCrAl不锈钢高温组织演变和力学性能[J]. 金属学报, 2022, 58: 883
doi: 10.11900/0412.1961.2020.00533
[114] Chen G, Wang H, Sun H Y, et al. Effects of Nb-doping on the mechanical properties and high-temperature steam oxidation of annealing FeCrAl fuel cladding alloys[J]. Mater. Sci. Eng., 2021, A803: 140500
[115] Shi Z L, Pang X Y, Zhang K, et al. Corrosion behavior of Nb-doped FeCrAl alloy in 500 oC steam[J]. Corros. Sci., 2024, 232: 112036
doi: 10.1016/j.corsci.2024.112036
[116] Huang T H, Lü J G, Song P, et al. Effect of Pt doping on oxide scale formation on yttria-dispersion FeCrAl alloy at 1200 oC[J]. Corros. Sci., 2020, 168: 108580
doi: 10.1016/j.corsci.2020.108580
[117] Amano T. High-temperature oxidation of FeCrAl(Y, Pt) alloys in oxygen-water vapour[J]. Mater. High Temp., 2011, 28: 342
doi: 10.3184/096034011X13190156331030
[118] Field K G, Briggs S A. Radiation effects in FeCrAl alloys for nuclear power applications[A]. Comprehensive Nuclear Materials[M]. 2nd Ed., Amsterdam: Elsevier, 2020: 293
[119] Little E A, Stow D A. Void-swelling in irons and ferritic steels: II. An experimental survey of materials irradiated in a fast reactor[J]. J. Nucl. Mater., 1979, 87: 25
doi: 10.1016/0022-3115(79)90123-5
[120] Gelles D S. Microstructural examination of several commercial alloys neutron irradiated to 100 dpa[J]. J. Nucl. Mater., 1987, 148: 136
doi: 10.1016/0022-3115(87)90105-X
[121] Haley J C, Briggs S A, Edmondson P D, et al. Dislocation loop evolution during in-situ ion irradiation of model FeCrAl alloys[J]. Acta Mater., 2017, 136: 390
doi: 10.1016/j.actamat.2017.07.011
[122] Field K G, Hu X X, Littrell K C, et al. Radiation tolerance of neutron-irradiated model Fe-Cr-Al alloys[J]. J. Nucl. Mater., 2015, 465: 746
doi: 10.1016/j.jnucmat.2015.06.023
[123] Field K G, Briggs S A, Sridharan K, et al. Dislocation loop formation in model FeCrAl alloys after neutron irradiation below 1 dpa[J]. J. Nucl. Mater., 2017, 495: 20
doi: 10.1016/j.jnucmat.2017.07.061
[124] Aydogan E, Weaver J S, Maloy S A, et al. Microstructure and mechanical properties of FeCrAl alloys under heavy ion irradiations[J]. J. Nucl. Mater., 2018, 503: 250
doi: 10.1016/j.jnucmat.2018.03.002
[125] Li F, Long Y X, Guo D X, et al. Ion irradiation defects and hardening in FeCrAl alloy[J]. Metals, 2022, 12: 1645
doi: 10.3390/met12101645
[126] Zhou X, Wang H, Guo L P, et al. Effect of niobium content on irradiation microstructure and hardening in FeCrAl-based alloys[J]. J. Mater. Sci. Technol., 2021, 95: 181
doi: 10.1016/j.jmst.2021.04.020
[127] Hernández-Mayoral M, Heintze C, Oñorbe E. Transmission electron microscopy investigation of the microstructure of Fe-Cr alloys induced by neutron and ion irradiation at 300 oC[J]. J. Nucl. Mater., 2016, 474: 88
doi: 10.1016/j.jnucmat.2016.03.002
[128] Xu H X, Stoller R E, Osetsky Y N, et al. Solving the puzzle of <100> interstitial loop formation in bcc Iron[J]. Phys. Rev. Lett., 2013, 110: 265503
doi: 10.1103/PhysRevLett.110.265503
[129] Kondo K, Aoki S, Yamashita S, et al. Ion irradiation effects on FeCrAl-ODS ferritic steel[J]. Nucl. Mater. Energy, 2018, 15: 13
[130] Han X X, Zhang C H, Niu M K, et al. A comparison study of change in hardness and microstructures of a Zr-added FeCrAl ODS steel irradiated with heavy ions[J]. Mater. Sci. Eng., 2022, A841: 143050
[131] Wang R Z, Wang H, Zhu X H, et al. Effects of Fe-ions irradiation on the microstructure and mechanical properties of FeCrAl-1.5wt.%ZrC alloys[J]. Nanomaterials, 2021, 11: 3423
doi: 10.3390/nano11123423
[132] Patki P V, Pownell T J, Bazarbayev Y, et al. Systematic study of radiation-induced segregation in neutron-irradiated FeCrAl alloys[J]. J. Nucl. Mater., 2023, 574: 154205
doi: 10.1016/j.jnucmat.2022.154205
[133] Bonny G, Terentyev D, Malerba L. On the α-α′ miscibility gap of Fe-Cr alloys[J]. Scr. Mater., 2008, 59: 1193
doi: 10.1016/j.scriptamat.2008.08.008
[134] Bachhav M, Robert Odette G, Marquis E A. α′ precipitation in neutron-irradiated Fe-Cr alloys[J]. Scr. Mater., 2014, 74: 48
doi: 10.1016/j.scriptamat.2013.10.001
[135] Field K G, Littrell K C, Briggs S A. Precipitation of α′ in neutron irradiated commercial FeCrAl alloys[J]. Scr. Mater., 2018, 142: 41
doi: 10.1016/j.scriptamat.2017.08.022
[136] Edmondson P D, Briggs S A, Yamamoto Y, et al. Irradiation-enhanced α′ precipitation in model FeCrAl alloys[J]. Scr. Mater., 2016, 116: 112
doi: 10.1016/j.scriptamat.2016.02.002
[137] Briggs S A, Edmondson P D, Littrell K C, et al. A combined APT and SANS investigation of α′ phase precipitation in neutron-irradiated model FeCrAl alloys[J]. Acta Mater., 2017, 129: 217
doi: 10.1016/j.actamat.2017.02.077
[138] Massey C P, Zhang D L, Briggs S A, et al. Deconvoluting the effect of chromium and aluminum on the radiation response of wrought FeCrAl alloys after low-dose neutron irradiation[J]. J. Nucl. Mater., 2021, 549: 152804
doi: 10.1016/j.jnucmat.2021.152804
[139] Zhang D L, Briggs S A, Edmondson P D, et al. Influence of welding and neutron irradiation on dislocation loop formation and α′ precipitation in a FeCrAl alloy[J]. J. Nucl. Mater., 2019, 527: 151784
doi: 10.1016/j.jnucmat.2019.151784
[140] Massey C P, Edmondson P D, Field K G, et al. Post irradiation examination of nanoprecipitate stability and α′ precipitation in an oxide dispersion strengthened Fe-12Cr-5Al alloy[J]. Scr. Mater., 2019, 162: 94
doi: 10.1016/j.scriptamat.2018.10.047
[141] Field K G, Briggs S A, Edmondson P, et al. Evaluation on the effect of composition on radiation hardening and embrittlement in model FeCrAl alloys[R]. Oak Ridge: Oak Ridge National Laboratory, 2015
[142] Shen S K, Wu Z F, Wang Y F, et al. Microstructure and radiation stability of nano-dispersoids in particle-reinforced FeCrAl alloys with different Zr concentrations[J]. J. Alloys Compd., 2022, 925: 166625
doi: 10.1016/j.jallcom.2022.166625
[143] Chen C L, Richter A, Kögler R. The effect of dual Fe+/He+ ion beam irradiation on microstructural changes in FeCrAl ODS alloys[J]. J. Alloys Compd., 2014, 586: S173
doi: 10.1016/j.jallcom.2012.11.113
[144] Ke J H, Reese E R, Marquis E A, et al. Flux effects in precipitation under irradiation—Simulation of Fe-Cr alloys[J]. Acta Mater., 2019, 164: 586
doi: 10.1016/j.actamat.2018.10.063
[145] Xu H, Si S Y, Li Y P, et al. The effect of Laves phase on heavy-ion radiation response of Nb-containing FeCrAl alloy for accident-tolerant fuel cladding[J]. Fundam. Res., 2022, 2: 437
doi: 10.1016/j.fmre.2022.01.028
[146] Li Y P, Ran G, Pei K F, et al. In-situ TEM study on composition change and amorphous transformation of Laves phase precipitates in FeCrAl alloy during Fe+ irradiation[J]. J. Nucl. Mater., 2022, 563: 153620
doi: 10.1016/j.jnucmat.2022.153620
[147] Shen H H, Zhang J M, Peng S M, et al. In situ TEM investigation of amorphization and recrystallization of Zr(Fe, Cr, Nb)2 precipitates under Ne ion irradiation[J]. Vacuum, 2014, 110: 24
doi: 10.1016/j.vacuum.2014.08.002
[148] Jia H D, Wang Y J, Wang Y, et al. Recent progress on creep properties of ODS FeCrAl alloys for advanced reactors[J]. Materials, 2023, 16: 3497
doi: 10.3390/ma16093497
[149] Wu Z F, Xu L D, Chen H Q, et al. Significant suppression of void swelling and irradiation hardening in a nanograined/nanoprecipitated 14YWT-ODS steel irradiated by helium ions[J]. J. Nucl. Mater., 2022, 559: 153418
doi: 10.1016/j.jnucmat.2021.153418
[150] Jia H D, Zhou Z J. Research progress in microstructure and service performance of high-strength and corrosion-resistant ODS FeCrAl alloy[J]. Chin. J. Eng., 2022, 44: 198
[150] 贾皓东, 周张健. 高强度耐腐蚀ODS-FeCrAl合金微观结构、力学性能研究进展[J]. 工程科学学报, 2022, 44: 198
[151] Han X X, Zhang C H, Niu M K, et al. Irradiation hardening of FeCrAl ODS alloys with Zr/Hf addition after high-energy self-ions irradiation[J]. Nucl. Mater. Energy, 2023, 37: 101556
[152] Jung H J, Edwards D J, Kurtz R J, et al. Structural and chemical evolution in neutron irradiated and helium-injected ferritic ODS PM2000 alloy[J]. J. Nucl. Mater., 2017, 484: 68
doi: 10.1016/j.jnucmat.2016.11.022
[153] de Castro V, Briceno M, Jenkins M L, et al. In-situ Fe+ ion irradiation of an oxide dispersion strengthened steel[J]. J. Phys. Conf. Ser., 2014, 522: 012032
[154] Chen T Y, Kim H, Gigax J G, et al. Radiation response of oxide-dispersion-strengthened alloy MA956 after self-ion irradiation[J]. Nucl. Instrum. Methods Phys. Res., 2017, 409B: 259
[155] Wang R Z, Wang H, Zhu X H, et al. Evolution of microstructure and mechanical properties of ZrC reinforced FeCrAl alloy after Fe-ions irradiation[J]. J. Nucl. Mater., 2021, 557: 153243
doi: 10.1016/j.jnucmat.2021.153243
[156] Wharry J P, Swenson M J, Yano K H. A review of the irradiation evolution of dispersed oxide nanoparticles in the b.c.c. Fe-Cr system: Current understanding and future directions[J]. J. Nucl. Mater., 2017, 486: 11
doi: 10.1016/j.jnucmat.2017.01.009
[157] Field K G, Briggs S A, Sridharan K, et al. Mechanical properties of neutron-irradiated model and commercial FeCrAl alloys[J]. J. Nucl. Mater., 2017, 489: 118
doi: 10.1016/j.jnucmat.2017.03.038
[158] Chen X, Field K, Massey C P, et al. Post-irradiation fracture toughness characterization of generation II FeCrAl alloys[A]. Proceedings of 2022 ASME Pressure Vessels and Piping Conference[C]. New York: American Society of Mechanical Engineers, 2022: V04 BT 06A019
[159] Gussev M N, Cakmak E, Field K G. Impact of neutron irradiation on mechanical performance of FeCrAl alloy laser-beam weldments[J]. J. Nucl. Mater., 2018, 504: 221
doi: 10.1016/j.jnucmat.2018.03.036
[160] Yang Y T, Zhang C H, Ding Z N, et al. A correlation between micro- and nano-indentation on materials irradiated by high-energy heavy ions[J]. J. Nucl. Mater., 2018, 498: 129
doi: 10.1016/j.jnucmat.2017.10.025
[161] Busby J T, Hash M C, Was G S. The relationship between hardness and yield stress in irradiated austenitic and ferritic steels[J]. J. Nucl. Mater., 2005, 336: 267
doi: 10.1016/j.jnucmat.2004.09.024
[162] Chen X, Field K G, Campbell A, et al. Fracture toughness characterization of generation II FeCrAl alloys after ~18 dpa irradiation[R]. Oak Ridge: Oak Ridge National Laboratory, 2021
[163] Terrani K A, Karlsen T M, Yamamoto Y. Input correlations for irradiation creep of FeCrAl and SiC based on in-pile Halden test results[R]. Oak Ridge: Oak Ridge National Laboratory, 2016
[164] Yao H, Ye T Z, Wu J M, et al. Creep properties of FeCrAl alloy at high temperature under neutron irradiation[A]. Proceedings of the 29th International Conference on Nuclear Engineering[C]. American Society of Mechanical Engineers, 2022, 86366: V002T02A005
[165] Ehrlich K. Irradiation creep and interrelation with swelling in austenitic stainless steels[J]. J. Nucl. Mater., 1981, 100: 149
doi: 10.1016/0022-3115(81)90531-6
[166] Kammenzind B F, Gruber J A, Bajaj R, et al. Neutron irradiation effects on the corrosion of zircaloy-4 in a pressurized water reactor environment[A]. 18th International Symposium on Zirconium in the Nuclear Industry[C]. West Conshohocken, PA: ASTM International, 2018: 448
[167] Wang P, Was G S. Oxidation of Zircaloy-4 during in situ proton irradiation and corrosion in PWR primary water[J]. J. Mater. Res., 2015, 30: 1335
doi: 10.1557/jmr.2014.408
[168] Lin Y P, Fawcett R M, Desilva S S, et al. Path towards industrialization of enhanced accident tolerant fuel[A]. TopFule 2018[C]. Prague: Czech Republic, 2018
[169] Wu W S, Ran G, Li Y P, et al. Early corrosion behaviour of irradiated FeCrAl alloy in a simulated pressurized water reactor environment[J]. Corros. Sci., 2020, 174: 108824
doi: 10.1016/j.corsci.2020.108824
[170] Wang P, Grdanovska S, Bartels D M, et al. Effect of radiation damage and water radiolysis on corrosion of FeCrAl alloys in hydrogenated water[J]. J. Nucl. Mater., 2020, 533: 152108
doi: 10.1016/j.jnucmat.2020.152108
[171] Wang P, Grdanovska S, Bartels D M, et al. Corrosion behavior of ferritic FeCrAl alloys in simulated BWR normal water chemistry[J]. J. Nucl. Mater., 2021, 545: 152744
doi: 10.1016/j.jnucmat.2020.152744
[172] Qu Z, Xie Y P, Ma J J, et al. Unveiling the dual role of ion irradiation on the corrosion behavior of lean-Cr FeCrAl alloys in a simulated PWR environment[J]. Corros. Sci., 2024, 237: 112344
doi: 10.1016/j.corsci.2024.112344
[173] Little E A. Development of radiation resistant materials for advanced nuclear power plant[J]. Mater. Sci. Technol., 2006, 22: 491
doi: 10.1179/174328406X90998
[174] Du D H, Sun K, Was G S. IASCC of neutron irradiated 316 stainless steel to 125 dpa[J]. Mater. Charact., 2021, 173: 110897
doi: 10.1016/j.matchar.2021.110897
[175] Wang M, Song M, Lear C R, et al. Irradiation assisted stress corrosion cracking of commercial and advanced alloys for light water reactor core internals[J]. J. Nucl. Mater., 2019, 515: 52
doi: 10.1016/j.jnucmat.2018.12.015
[176] Du D H, Sun K, Was G S. Crack initiation of neutron-irradiated 304L stainless steel in PWR primary water[J]. Corros. Sci., 2021, 193: 109902
doi: 10.1016/j.corsci.2021.109902
[177] Ahmedabadi P M, Was G S. Stress corrosion cracking of ferritic-martensitic steels in simulated boiling water reactor environment[J]. Corrosion, 2016, 72: 66
doi: 10.5006/1806
[178] Yu H, Wang H R, Kondo S, et al. Radiation tolerance of alumina scale formed on FeCrAl ODS ferritic alloy[J]. Nucl. Mater. Energy, 2021, 29: 101102
[1] 崔俊峰, 胡晓飞, 陈国新, 李友兵, 柯培玲, 赵宏伟. Nb4AlC3MAX 相单晶纳米线断面自修复原位定量研究[J]. 金属学报, 2026, 62(9): 1478-1486.
[2] 刘泽田, 路伟昭, 徐新宇, 刘旭, 张少游, 王慧远. 均质化温度对3003铝合金微观组织和力学性能的影响规律[J]. 金属学报, 2026, 62(9): 1503-1516.
[3] 苏逸云, 郝晓虎, 黎书华, 崔泽琴, 闫德俊, 李卫国. 瞬态热处理对船用钛/钢接头界面组织和结合性能的影响[J]. 金属学报, 2026, 62(9): 1528-1540.
[4] 刘蓉, 高古辉, 桂晓露, 白秉哲. 贝氏体钢轨的低温疲劳裂纹扩展行为[J]. 金属学报, 2026, 62(9): 1541-1552.
[5] 刘洋, 孙健, 陆善平. Mo含量对1000 MPa级高强钢焊缝金属组织和力学性能的影响[J]. 金属学报, 2026, 62(9): 1553-1565.
[6] 陈园, 宫春波, 王胜刚, 马嵩, 张志东. 纳米晶304不锈钢板材的微观组织、显微硬度与耐腐蚀性能[J]. 金属学报, 2026, 62(9): 1566-1580.
[7] 史显波, 张舒展, 苏元飞, 焦圣轩, 严伟, 戎利建. 铅冷快堆紧固件用高硅奥氏体钢的高温组织稳定性[J]. 金属学报, 2026, 62(8): 1347-1356.
[8] 杨坤, 郭庆伟, 李超, 张高龙, 赵宇宏, 侯华. 冲击加载下60钢的动态力学响应及层裂行为[J]. 金属学报, 2026, 62(8): 1405-1416.
[9] 尹建年, 马英杰, 杨锐, 雷家峰, 齐敏, 周丽. Ti551合金的热变形行为及热加工图构建[J]. 金属学报, 2026, 62(8): 1427-1442.
[10] 陈胜虎, 谢昂, 杨彬彬, 刘涌涛, 陈思含, 赵明久, 姜海昌, 戎利建. Nb稳定化奥氏体不锈钢在第四代核电领域的研究进展[J]. 金属学报, 2026, 62(7): 1175-1188.
[11] 杨何, 侯自勇, 胡兴益, 程金骏, 王亚茹, 范国华, 黄晓旭. 超高强不锈钢微丝表征技术:进展与展望[J]. 金属学报, 2026, 62(7): 1189-1206.
[12] 李瑞雪, 周晨曦, 杨慧敏, 雍兴跃, 刘景军. 流动海水中多重应力耦合作用下B10 Cu-Ni合金的微观结构演变与动态失效机制[J]. 金属学报, 2026, 62(7): 1273-1287.
[13] 王玮, 张宇博, 赵燕, 王同敏, 李廷举. 高熵合金颗粒对选区激光熔化Al12Si合金固溶组织和力学性能的影响[J]. 金属学报, 2026, 62(6): 1009-1020.
[14] 王彬, 赵鹏, 刘家伟, 张春波, 秦志伟, 董红刚, 李鹏. 热处理对FGH96高温合金惯性摩擦焊接头微观组织演变及力学性能的影响[J]. 金属学报, 2026, 62(6): 1043-1058.
[15] 邓尕平, 赵杰, 高凯, 王威, 刘欢, 曹铁山, 程从前. 950 ℃下DZ411镍基高温合金NiCoCrAlY涂层热腐蚀行为[J]. 金属学报, 2026, 62(6): 1059-1068.