| 颗粒尺寸对金刚石/Al封装基板热物性的影响 |
周洪宇1, 冉珉瑞1, 李亚强2, 张卫冬1, 刘俊友3, 郑文跃1( ) |
1.北京科技大学 国家材料服役安全科学中心 北京 100083 2.北京科技大学 新材料技术研究院 北京 100083 3.北京科技大学 材料科学与工程学院 北京 100083 |
|
| Effect of Diamond Particle Size on the Thermal Properties of Diamond/Al Composites for Packaging Substrate |
ZHOU Hongyu1, RAN Minrui1, LI Yaqiang2, ZHANG Weidong1, LIU Junyou3, ZHENG Wenyue1( ) |
1.National Center for Materials Service Safety, University of Science and Technology Beijing, Beijing 100083, China 2.Institute for Advanced Materials and Technology, University of Science and Technology Beijing, Beijing 100083, China 3.School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China |
引用本文:
周洪宇, 冉珉瑞, 李亚强, 张卫冬, 刘俊友, 郑文跃. 颗粒尺寸对金刚石/Al封装基板热物性的影响[J]. 金属学报, 2021, 57(7): 937-947.
Hongyu ZHOU,
Minrui RAN,
Yaqiang LI,
Weidong ZHANG,
Junyou LIU,
Wenyue ZHENG.
Effect of Diamond Particle Size on the Thermal Properties of Diamond/Al Composites for Packaging Substrate[J]. Acta Metall Sin, 2021, 57(7): 937-947.
| 1 |
Suh D, Moon C M, Kim D, et al. Ultrahigh thermal conductivity of interface materials by silver-functionalized carbon nanotube phonon conduits [J]. Adv. Mater., 2016, 28: 7220
|
| 2 |
Li T, Li J Q, Wang W G, et al. A discussion on the main factors affecting thermal conductivity of carbon/metal matrix composites [J]. Mater. Rev., 2018, 32: 2640
|
| 2 |
李 通, 李金权, 王文广等. 影响碳/金属复合材料导热性能的主要因素探讨 [J]. 材料导报, 2018, 32: 2640
|
| 3 |
Zhang D, Yuan M Y, Tan Z Q, et al. Progress in interface modification and nanoscale study of diamond/Cu composites [J]. Acta Metall. Sin., 2018, 54: 1158
|
| 3 |
张 荻, 苑孟颖, 谭占秋等. 金刚石/Cu复合界面导热改性及其纳米化研究进展 [J]. 金属学报, 2018, 54: 1158
|
| 4 |
Janicki M, Napieralski A. Modelling electronic circuit radiation cooling using analytical thermal model [J]. Microelectron. J., 2000, 31: 781
|
| 5 |
Ma R L, Peng C Q, Wang R C, et al. Research progress of diamond/aluminum composites for electronic packaging [J]. Chin. J. Nonferrous Met., 2014, 24: 689
|
| 5 |
马如龙, 彭超群, 王日初等. 电子封装用diamond/Al复合材料研究进展 [J]. 中国有色金属学报, 2014, 24: 689
|
| 6 |
Liu X Y, Wang W G, Wang D, et al. Effect of nanometer TiC coated diamond on the strength and thermal conductivity of diamond/Al composites [J]. Mater. Chem. Phys., 2016, 182: 256
|
| 7 |
Zhang L, Wei Q P, An J J, et al. Construction of 3D interconnected diamond networks in Al-matrix composite for high-efficiency thermal management [J]. Chem. Eng. J., 2020, 380: 122551
|
| 8 |
Chu K, Jia C C, Liang X B, et al. Effect of particle size on the microstructure and thermal conductivity of Al/diamond composites prepared by spark plasma sintering [J]. Rare Met., 2009, 28: 646
|
| 9 |
Tan Z Q, Chen Z Z, Fan G L, et al. Effect of particle size on the thermal and mechanical properties of aluminum composites reinforced with SiC and diamond [J]. Mater. Des., 2016, 90: 845
|
| 10 |
Kwon H, Leparoux M, Heintz J M, et al. Fabrication of single crystalline diamond reinforced aluminum matrix composite by powder metallurgy route [J]. Met. Mater. Int., 2011, 17: 755
|
| 11 |
Zhang W X, Xu S S, Wang Y Z, et al. Diamond/Ti3AlC2 composite prepared by spark plasma sintering [J]. Superhard Mater. Eng., 2017, 29(1): 11
|
| 11 |
张旺玺, 徐世帅, 王艳芝等. 放电等离子烧结制备金刚石/钛铝碳复合材料 [J]. 超硬材料工程, 2017, 29(1): 11
|
| 12 |
Mizuuchi K, Inoue K, Agari Y, et al. Bimodal and monomodal diamond particle effect on the thermal properties of diamond-particle-dispersed Al-matrix composite fabricated by SPS [J]. Microelectron. Reliab., 2014, 54: 2463
|
| 13 |
Sun Y H, Zhang C, He L K, et al. Enhanced bending strength and thermal conductivity in diamond/Al composites with B4C coating [J]. Sci. Rep., 2018, 8: 11104
|
| 14 |
Ji G, Tan Z Q, Lu Y G, et al. Heterogeneous interfacial chemical nature and bonds in a W-coated diamond/Al composite [J]. Mater. Charact., 2016, 112: 129
|
| 15 |
Che Z F, Li J W, Wang Q X, et al. The formation of atomic-level interfacial layer and its effect on thermal conductivity of W-coated diamond particles reinforced Al matrix composites [J]. Composites, 2018, 107A: 164
|
| 16 |
Yang W L, Sang J Q, Zhou L P, et al. Overcoming selective interfacial bonding and enhancing thermal conductivity of diamond/aluminum composite by an ion bombardment pretreatment [J]. Diam. Relat. Mater., 2018, 81: 127
|
| 17 |
Ma S D, Zhao N Q, Shi C S, et al. Mo2C coating on diamond: Different effects on thermal conductivity of diamond/Al and diamond/Cu composites [J]. Appl. Surf. Sci., 2017, 402: 372
|
| 18 |
Wang P P, Xiu Z Y, Jiang L T, et al. Enhanced thermal conductivity and flexural properties in squeeze casted diamond/aluminum composites by processing control [J]. Mater. Des., 2015, 88: 1347
|
| 19 |
Liang X B, Jia C C, Chu K, et al. Thermal conductivity and microstructure of Al/diamond composites with Ti-coated diamond particles consolidated by spark plasma sintering [J]. J. Compos. Mater., 2012, 46: 1127
|
| 20 |
Tan Z Q, Li Z Q, Fan G L, et al. Fabrication of diamond aluminium composites by vacuum hot: Pressing process optimization and thermal properties [J]. Composites, 2013, 47B: 173
|
| 21 |
Xin L, Tian X, Yang W S, et al. Enhanced stability of the diamond/Al composites by W coatings prepared by the magnetron sputtering method [J]. J. Alloys Compd., 2018, 763: 305
|
| 22 |
Li N, Wang L H, Dai J J, et al. Interfacial products and thermal conductivity of diamond/Al composites reinforced with ZrC-coated diamond particles [J]. Diam. Relat. Mater., 2019, 100: 107565
|
| 23 |
Zhou H Y, Liu X, Yin Z, et al. The fabrication of functional gradient hypereutectic Al-Si composites by liquid-solid separation technology [J]. J. Alloys Compd., 2018, 763: 49
|
| 24 |
Zhou H Y, Yin Y L, Shi Z L, et al. The fabrication of Al-diamond composites for heat dissipation by liquid-solid separation technology [J]. J. Mater. Sci.: Mater. Electron., 2017, 28: 721
|
| 25 |
Zhou H Y, Yin Y L, Wu C J, et al. Microstructures and properties of diamond/Al composites prepared by liquid-solid separation technology [J]. Chin. J. Nonferrous. Met., 2017, 27: 1855
|
| 25 |
周洪宇, 尹衍利, 吴春京等. 液固分离法制备金刚石/铝封装材料的组织与性能 [J]. 中国有色金属学报, 2017, 27: 1855
|
| 26 |
Yamamoto Y, Imai T, Tanabe K, et al. The measurement of thermal properties of diamond [J]. Diam. Relat. Mater., 1997, 6: 1057
|
| 27 |
Yang W L, Peng K, Zhou L P, et al. Finite element simulation and experimental investigation on thermal conductivity of diamond/aluminium composites with imperfect interface [J]. Comput. Mater. Sci., 2014, 83: 375
|
| 28 |
Ren S B, He X B, Qu X H, et al. Effect of Mg and Si in the aluminum on the thermo-mechanical properties of pressureless infiltrated SiCp/Al composites [J]. Compos. Sci. Technol., 2007, 67: 2103
|
| 29 |
Yin S, Cizek J, Chen C Y, et al. Metallurgical bonding between metal matrix and core-shelled reinforcements in cold sprayed composite coating [J]. Scr. Mater., 2020, 177: 49
|
| 30 |
Tan Z Q, Li Z Q, Xiong D B, et al. A predictive model for interfacial thermal conductance in surface metallized diamond aluminum matrix composites [J]. Mater. Des., 2014, 55: 257
|
| 31 |
Yan Y W, Geng L. Effects of particle size on the thermal expansion behavior of SiCp/Al composites [J]. J. Mater. Sci., 2007, 42: 6433
|
| 32 |
Geiger A L, Jackson M. Low-expansion MMC's boost avionics [J]. Adv. Mater. Process., 1989, 136: 23
|
| 33 |
Turner P S. Thermal-expansion stress in reinforced plastics [J]. J. Res. Nat. Bur. Stand., 1946, 37: 250
|
| 34 |
Kerner E H. The elastic and thermo-elastic properties of composite media [J]. Proc. Phys. Soc., 1956, 69B: 808
|
| 35 |
Edtmaier C, Segl J, Koos R, et al. Characterization of interfacial bonding strength at Al(Si)/diamond interfaces by neutron diffraction: Effect of diamond surface termination and processing conditions [J]. Diam. Relat. Mater., 2020, 106: 107842
|
| 36 |
Vetterli M, Tavangar R, Weber L, et al. Influence of the elastic properties of the phases on the coefficient of thermal expansion of a metal matrix composite [J]. Scr. Mater., 2011, 64: 153
|
| 37 |
Fan T X, Liu Y, Yang K M, et al. Recent progress on interfacial structure optimization and their influencing mechanism of carbon reinforced metal matrix composites [J]. Acta Metall. Sin., 2019, 55: 16
|
| 37 |
范同祥, 刘 悦, 杨昆明等. 碳/金属复合材料界面结构优化及界面作用机制的研究进展 [J]. 金属学报, 2019, 55: 16
|
| 38 |
Yang W S, Chen G Q, Wang P P, et al. Enhanced thermal conductivity in diamond/Aluminum composites with tungsten coatings on diamond particles prepared by magnetron sputtering method [J]. J. Alloys Compd., 2017, 726: 623
|
| 39 |
Monje I E, Louis E, Molina J M. On critical aspects of infiltrated Al/diamond composites for thermal management: Diamond quality versus processing conditions [J]. Composites, 2014, 67A: 70
|
| 40 |
Caccia M, Rodríguez A, Narciso J. Diamond surface modification to enhance interfacial thermal conductivity in Al/diamond composites [J]. JOM, 2014, 66: 920
|
| 41 |
Maxwell J C. A Treatise on Electricity and Magnetism [M]. Oxford: Oxford University Press, 1937: 1
|
| 42 |
Tavangar R, Molina J M, Weber L. Assessing predictive schemes for thermal conductivity against diamond-reinforced silver matrix composites at intermediate phase contrast [J]. Scr. Mater., 2007, 56: 357
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|