| 激光立体成形退火态Zr55Cu30Al10Ni5粉末的晶化行为 |
张媛媛,林鑫( ),魏雷,任永明 |
| 西北工业大学凝固技术国家重点实验室 西安 710072 |
|
| Crystallization Behavior of Laser Solid Forming of Annealed Zr55Cu30Al10Ni5 Powder |
Yuanyuan ZHANG,Xin LIN( ),Lei WEI,Yongming REN |
| State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China |
引用本文:
张媛媛,林鑫,魏雷,任永明. 激光立体成形退火态Zr55Cu30Al10Ni5粉末的晶化行为[J]. 金属学报, 2017, 53(7): 824-832.
Yuanyuan ZHANG,
Xin LIN,
Lei WEI,
Yongming REN.
Crystallization Behavior of Laser Solid Forming of Annealed Zr55Cu30Al10Ni5 Powder[J]. Acta Metall Sin, 2017, 53(7): 824-832.
| [1] | Schroers J.Processing of bulk metallic glass[J]. Adv. Mater., 2010, 22: 1566 | | [2] | Inoue A, Takeuchi A.Recent development and application products of bulk glassy alloys[J]. Acta Mater., 2011, 59: 2243 | | [3] | Hu Q, Lin X, Yang G L, et al.Crystallization behavior of Zr55Al10Ni5Cu30 amorphous alloys with different morphologies and thermal history conditions[J]. Acta Metall. Sin., 2012, 48: 1467 | | [3] | (胡桥, 林鑫, 杨高林等. 不同形态和热历史条件下Zr55Al10Ni5Cu30非晶合金的晶化行为[J]. 金属学报, 2012, 48: 1467) | | [4] | Inoue A.Stabilization of metallic supercooled liquid and bulk amorphous alloys[J]. Acta Mater., 2000, 48: 279 | | [5] | Somekawa H, Inoue A, Higashi K.Superplastic and diffusion bonding behavior on Zr-Al-Ni-Cu metallic glass in supercooled liquid region[J]. Scr. Mater., 2004, 50: 1395 | | [6] | Ye X Y, Shin Y C.Synthesis and characterization of Fe-based amorphous composite by laser direct deposition[J]. Surf. Coat. Technol., 2014, 239: 34 | | [7] | Yang G L, Lin X, Liu F C, et al.Laser solid forming Zr-based bulk metallic glass[J]. Intermetallics, 2012, 22: 110 | | [8] | Pauly S, L?ber L, Petters R, et al.Processing metallic glasses by selective laser melting[J]. Mater. Today, 2013, 16: 37 | | [9] | Bai Y W, Bian X F, Lv X Q, et al.Heredity of medium-range order structure from melts to amorphous solids[J]. J. Appl. Phys., 2012, 112: 083524 | | [10] | Balla V K, Bandyopadhyay A.Laser processing of Fe-based bulk amorphous alloy[J]. Surf. Coat. Technol., 2010, 205: 2661 | | [11] | Zhang Y Y, Lin X, Wei L, et al.Influence of powder size on the crystallization behavior during laser solid forming Zr55Cu30Al10Ni5 bulk amorphous alloy[J]. Intermetallics, 2016, 76: 1 | | [12] | Zhang Y Y, Lin X, Yang H O, et al.Influence of powdered state on crystallization during laser solid forming Zr55Cu30Al10Ni5 bulk metallic glasses[J]. Acta Phys. Sin., 2015, 64: 0166402 | | [12] | (张媛媛, 林鑫, 杨海欧等. 粉末状态对激光立体成形Zr55Cu30Al10Ni5块体非晶合金晶化行为的影响[J]. 物理学报, 2015, 64: 0166402) | | [13] | Zhang Y Y, Lin X, Wang L L, et al.Microstructural analysis of Zr55Cu30Al10Ni5 bulk metallic glasses by laser surface remelting and laser solid forming[J]. Intermetallics, 2015, 66: 22 | | [14] | Al-Jaroudi S S, Ul-Hamid A, Mohammed A R I, et al. Use of X-ray powder diffraction for quantitative analysis of carbonate rock reservoir samples[J]. Powder Technol., 2007, 175: 115 | | [15] | Chokethawai K, McCartney D G, Shipway P H. Microstructure evolution and thermal stability of an Fe-based amorphous alloy powder and thermally sprayed coatings[J]. J. Alloys Compd., 2009, 480: 351 | | [16] | Basu A, Samant A N, Harimkar S P, et al.Laser surface coating of Fe-Cr-Mo-Y-B-C bulk metallic glass composition on AISI 4140 steel[J]. Surf. Coat. Technol., 2008, 202: 2623 | | [17] | Zhu W H, Gu Y Q.Fundamentals of Statistical Physics [M]. Beijing: Tsinghua University Press, 1983: 208 | | [17] | (朱文浩, 顾毓沁. 统计物理学基础 [M]. 北京: 清华大学出版社, 1983: 208) | | [18] | Sih S S, Barlow J W.Measurement and prediction of the thermal conductivity of powders at high temperature [A]. Proceedings of the 6th Annual SFF Symposium[C]. Austin: The University of Texas, 1994: 397 | | [19] | Dai K, Shaw L.Thermal and mechanical finite element modeling of laser forming from metal and ceramic powders[J]. Acta Mater., 2004, 52: 69 | | [20] | Mao J, Zhang H F, Fu H M, et al.Influence of casting temperature on the thermal stability of Zr-based metallic glasses[J]. J. Alloys Compd., 2010, 496: 595 | | [21] | Miracle D B.The efficient cluster packing model——An atomic structural model for metallic glasses[J]. Acta Mater., 2006, 54: 4317 | | [22] | Ye S L, Li X Y, Bian X F, et al.Remelting treatment and heredity phenomenon in the formation of Fe78Si9B13 amorphous alloy[J]. J. Alloys Compd., 2013, 562: 143 | | [23] | Lipton J, Kurz W, Trivedi R.Rapid dendrite growth in undercooled alloys[J]. Acta Metall., 1987, 35: 957 | | [24] | Trivedi R, Magnin P, Kurz W.Theory of eutectic growth under rapid solidification conditions[J]. Acta Metall., 1987, 35: 971 | | [25] | Shao G.Thermodynamic and kinetic aspects of intermetallic amorphous alloys[J]. Intermetallics, 2003, 11: 313 | | [26] | Smityhells C J.Metals Reference Book[M]. 5th Ed., London: Butterworth & Ltd., 1976: 186 | | [27] | Schroers J, Johnson W L.History dependent crystallization of Zr41Ti14Cu12Ni10Be23 melts[J]. J. Appl. Phys., 2000, 88: 44 | | [28] | Katakam S, Kumar V, Santhanakrishnan S, et al.Laser assisted Fe-based bulk amorphous coating: Thermal effects and corrosion[J]. J. Alloys Compd., 2014, 604: 266 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|