| 弯月面热障涂层方法对结晶器传热及铸坯振痕形貌的影响 |
侯晓光1,2,王恩刚1( ),许秀杰1,邓安元1,王万林3 |
2 宝山钢铁股份有限公司, 上海 201900 3 中南大学冶金与环境学院, 长沙 410083 |
|
| EFFECT OF THERMAL BARRIER COATINGS ABOVE MOULD MENISCUS ON MOULD HEAT TRANSFER AND OSCILLATION MARK MORPHOLOGY OF STRANDS |
Xiaoguang HOU1,2,Engang WANG1( ),Xiujie XU1,Anyuan DENG1,Wanlin WANG3 |
1 Key Laboratory of Electromagnetic Processing of Materials (Ministry of Education), Northeastern University, Shenyang 110819 2 Baoshan Iron & Steel Co., Ltd., Shanghai 201900 3 School of Metallurgy and Environment, Central South University, Changsha 410083 |
引用本文:
侯晓光,王恩刚,许秀杰,邓安元,王万林. 弯月面热障涂层方法对结晶器传热及铸坯振痕形貌的影响[J]. 金属学报, 2015, 51(9): 1145-1152.
Xiaoguang HOU,
Engang WANG,
Xiujie XU,
Anyuan DENG,
Wanlin WANG.
EFFECT OF THERMAL BARRIER COATINGS ABOVE MOULD MENISCUS ON MOULD HEAT TRANSFER AND OSCILLATION MARK MORPHOLOGY OF STRANDS[J]. Acta Metall Sin, 2015, 51(9): 1145-1152.
| [1] | Brimacombe J K, Sorimachi K. Metall Trans, 1977; 8B: 489 | | [2] | Mintz B. ISIJ Int, 1999; 39: 833 | | [3] | Harada S, Tanaka S. ISIJ Int, 1990; 30: 310 | | [4] | Hwang B, Lee H S, Kim Y G, Lee S. Mater Sci Eng, 2005; A402: 177 | | [5] | Sengupta J, Thomas B G, Shin H J, Lee G G, Kim S H. Metall Trans, 2006; 37A: 1597 | | [6] | Takeuchi E, Brimacombe J K. Metall Trans, 1985; 16B: 605 | | [7] | Badri A, Natarajan T T, Snyder C C, Powers K D, Mannion F J, Cramb A W. Metall Trans, 2005; 36B: 360 | | [8] | Badri A, Natarajan T T, Snyder C C, Powers K D, Mannion F J, Cramb A W. Metall Trans, 2005; 36B: 379 | | [9] | Lei Z S, Ren Z M, Zhang B W, Deng K. Acta Metall Sin, 2002; 38: 8 (雷作胜, 任忠鸣, 张邦文, 邓 康. 金属学报, 2002; 38: 8) | | [10] | Gu K Z, Wang W L, Wei J, Matsuura H, Tsukihashi F, Sohn I, Dong J M. Metall Trans, 2012; 43B: 1393 | | [11] | Gu K Z, Wang W L, Zhou L J, Ma F J, Huang D Y. Metall Trans, 2012; 43B: 937 | | [12] | Zhou L J, Wang W L, Ma F J, Li J, Wei J, Matsuura H, Tsukihashi F. Metall Trans, 2012; 43B: 354 | | [13] | Wang W L, Zhou L J, Gu K Z. Met Mater Int, 2010; 16: 913 | | [14] | Wang W L, Gu K Z, Zhou L J, Ma F J, Sohn I, Min D J, Matsuura H, Tsukihashiet F. ISIJ Int, 2011; 51: 1838 | | [15] | Wang W L, Cramb A W. AIST Trans, 2008; 5: 155 | | [16] | Wang W L, Cramb A W. ISIJ Int, 2005; 45: 1864 | | [17] | Zhang H H, Wang W L, Zhou D, Ma F J, Lu B X, Zhou L J. Metall Trans, 2014; 45B: 1038 | | [18] | Zhou D, Wang W L, Zhang H H, Ma F J, Chen K, Zhou L J. Metall Trans, 2014; 45B: 1048 | | [19] | Yin H B, Yao M. Acta Metall Sin, 2005; 41: 638 (尹合壁, 姚 曼. 金属学报, 2005; 41: 638) | | [20] | Wang X D, Zang X Y, Du F M, Kong L W, Yao M. Foundry Technol, 2014; 35: 1474 (王旭东, 臧欣阳, 杜凤鸣, 孔令伟, 姚 曼. 铸造技术, 2014; 35: 1474) | | [21] | Qing L J, Wang X R, Li J, Sun L G. Hebei Enterprise, 2013; (9): 90 (齐力军, 王鑫荣, 李 景, 孙立根. 河北企业, 2013; (9): 90) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|