| 轧制-重熔SIMA法制备ZCuSn10合金半固态坯料 |
王佳1,2, 肖寒1( ), 吴龙彪1, 卢德宏1, 周荣锋1,3, 周荣1 |
1 昆明理工大学材料科学与工程学院, 昆明 650093 2 四川理工学院机械工程学院, 自贡 643000 3 昆明理工大学分析测试研究中心, 昆明 650093 |
|
| STUDY OF ROLLING-REMELTING SIMA PROCESS FOR PREPARING THE SEMI-SOLID BILLET OF ZCuSn10 ALLOY |
WANG Jia1,2, XIAO Han1( ), WU Longbiao1, LU Dehong1, ZHOU Rongfeng1,3, ZHOU Rong1 |
1 Faculty of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093 2 College of Mechanical Engineering, Sichuan University of Science and Engineering, Zigong 643000 3 Research Center for Analysis and Measurement, Kunming University of Science and Technology, Kunming 650093 |
引用本文:
王佳, 肖寒, 吴龙彪, 卢德宏, 周荣锋, 周荣. 轧制-重熔SIMA法制备ZCuSn10合金半固态坯料[J]. 金属学报, 2014, 50(5): 567-574.
Jia WANG,
Han XIAO,
Longbiao WU,
Dehong LU,
Rongfeng ZHOU,
Rong ZHOU.
STUDY OF ROLLING-REMELTING SIMA PROCESS FOR PREPARING THE SEMI-SOLID BILLET OF ZCuSn10 ALLOY[J]. Acta Metall Sin, 2014, 50(5): 567-574.
| [1] |
Spencer D B, Mehrabia R, Flemings M C. Metall Trans, 1972; 3: 1925
|
| [2] |
Flemings M C. Metall Trans, 1991; 22A: 957
|
| [3] |
Chen Q, Luo S J, Zhao Z D. J Alloys Compd, 2009; 447: 726
|
| [4] |
Kiuchi M, Kopp R. CIRP Ann-Manuf Technol, 2002; 51: 653
|
| [5] |
Kirkwood D H. Int Mater Rev, 1994; 39: 173
|
| [6] |
Zhao J W, Wu S S, Wan L, Chen Q H, An P. Acta Metall Sin, 2009; 45: 314
|
| [6] |
(赵君文, 吴树森, 万 里, 陈启华, 安 萍. 金属学报, 2009; 45: 314)
|
| [7] |
Luo S J, Chen Q, Zhao Z D. Mater Sci Eng, 2009; A501: 146
|
| [8] |
Liu Z, Mao W M, Zhao Z D. Acta Metall Sin, 2009; 45: 507
|
| [8] |
(刘 政, 毛卫民, 赵振铎. 金属学报, 2009; 45: 507)
|
| [9] |
Young K P, Kyonka C P, Courtois J A. US Pat, 4415374, 1983
|
| [10] |
Lin H Q, Wang J G, Wang H Y, Jiang Q C. J Alloys Compd, 2007; 431: 141
|
| [11] |
Dong J, Cui J Z, Le Q C, Lu G M. Mater Sci Eng, 2003; A345: 234
|
| [12] |
Hassas-Irani S B, Zarei-Hanzaki A, Bazaz B, Roostaei A A. Mater Des, 2013; 46: 579
|
| [13] |
Alipour M, Aghdam B G, Rahnoma H E, Emamy M. Mater Des, 2013; 46: 766
|
| [14] |
Jiang J F, Wang Y, Qu J J. Mater Sci Eng, 2013; A560: 473
|
| [15] |
Dodangeh A, Kazeminezhad M, Aashuri H. Mater Sci Eng, 2012; A558: 371
|
| [16] |
Tao J Q, Cheng Y S, Huang S D, Peng F F, Yang W X, Lu M Q, Zhang Z M, Jin X. Trans Nonferrous Metall, 2012; 22(suppl 2): 428
|
| [17] |
Chen Q, Zhao Z D, Zhao Z X, Hu C K, Shu D Y. J Alloys Compd, 2011; 509: 7303
|
| [18] |
Tian R Z,Wang Z T. Handbook of Copper Alloy and its Processing. Changsha: Central South University Press, 2002: 259
|
| [18] |
(田荣璋,王祝堂. 铜合金及其加工手册. 长沙: 中南大学出版社, 2002: 259)
|
| [19] |
Metallographic Experiment Group of Central Laboratory of Luoyang Copper Processing Factory. Metallographic Atlas of Copper and Copper Alloy. Beijing: Metallurgical Industry Press, 1983: 74
|
| [19] |
(洛阳铜加工厂中心试验室金相组. 铜及铜合金金相图谱. 北京: 冶金工业出版社, 1983: 74)
|
|