|   [1] Mikhail S, Antti S, Vladislav S, Alexander F. Opt Laser Technol, 2012; 44: 2064 [2] Reisgen U, Schleser M, Mokrov O, Ahmed E. Opt Laser Technol, 2012; 44: 255 [3] Ruggiero A, Tricarico L, Olabi A G, Benyounis K Y. Opt Laser Technol, 2011; 43: 82 [4] Yilbas B, Arif A, Abdul A. Opt Laser Technol, 2010; 42: 760 [5] Chang B H, Bai S J, Du D, Zhang H, Zhou Y. J Mater Process Technol, 2010; 210: 885 [6] Mei L F, Chen G Y, Jin X Z, Zhang Y, Wu Q. Opt Lasers Eng, 2009; 47: 1117 [7] Emel T, Eddy D, Alfred D, Erdinc K. Mater Des, 2009; 30: 1193 [8] Zhang X D, Chen W Z, Eiji A, Fukuhisa M. Trans Chin Weld Inst, 2002; 23(6): 51 (张旭东, 陈武柱, 芦田荣次, 松田福久. 焊接学报, 2002; 23(6): 51) [9] Zhao L, Zhang X D, Chen W Z, Bao G. Trans Chin Weld Inst, 2004; 25(1): 29 (赵琳, 张旭东, 陈武柱, 包刚. 焊接学报, 2004; 25(1): 29) [10] Zhang X H, Zhang X D, Chen W Z, Lei H D. Laser Technol, 2007; 31: 419 (张晓红, 张旭东, 陈武柱, 雷华东. 激光技术, 2007; 31: 419) [11] Zhao L, Zhang X D, Chen W Z, Wang J. Appl Laser, 2004; 24: 21 (赵琳, 张旭东, 陈武柱, 王晶. 应用激光, 2004; 24: 21) [12] Wahba M, Kawahitoc Y, Kondohc K, Katayamac S. Mater Sci Eng, 2011; A529: 143 [13] Seto N, Katayama S, Matsunawa A. Q J Jpn Weld Soc, 2001; 19: 600 [14] Zhou J, Tsai H L. Int J Heat Mass Transfer, 2007; 50: 2217 [15] Haboudoua A, Peyrea P, Vannesb A B, Peixc G. Mater Sci Eng, 2003; A363: 40 [16] Hayashi T, Matsubayashi K, Katayama S, Nobuyuki A, Matsunawa A, Omori A. Q J Jpn Weld Soc, 2002; 20: 228 [17] Kawaguchi I, Tsukamoto S, Arakane G, Honda H. Q J Jpn Weld Soc, 2005; 23: 259 [18] Matsunawa A. Sci Technol Weld Join, 2001; 6: 351 [19] Kuo T Y, Jeng S L. J Phys, 2005; 38D: 722 [20] Alessandro A, Alessandro F, Leonardo O, Giampaolo C. Opt Laser Technol, 2012; 44: 1485 [21] Seto N, Katayama S, Matsunawa A. Weld Int, 2002; 16: 451 [22] Matsunawa A, Mizutani M, Katayama S, Seto N. Weld Int, 2003; 17: 431    |