Please wait a minute...
金属学报  2013, Vol. 49 Issue (2): 175-180    DOI: 10.3724/SP.J.1037.2012.00560
  论文 本期目录 | 过刊浏览 |
长期热老化后Z3CN20-09M不锈钢的微观组织与拉伸断裂行为
郑凯1),王艳丽1),李时磊1),吕绪明1),王西涛1),薛飞2)
1)北京科技大学新金属材料国家重点实验室, 北京 100083
2)中国广东核电集团苏州热工研究院, 苏州 215004
THE MICROSTRUCTURE AND TENSILE FRACTURE BEHAVIOR OF LONG TERM THERMAL AGED Z3CN20-09M STAINLESS STEEL
 
ZHENG Kai1), WANG Yanli1), LI Shilei1), LU Xuming1), WANG Xitao1), XUE Fei2)
1) State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083
2)Suzhou Nuclear Power Research Institute, China Guangdong Nuclear Power Group, Suzhou 215004
引用本文:

郑凯,王艳丽,李时磊,吕绪明,王西涛,薛飞. 长期热老化后Z3CN20-09M不锈钢的微观组织与拉伸断裂行为[J]. 金属学报, 2013, 49(2): 175-180.
ZHENG Kai, WANG Yanli, LI Shilei, LU Xuming, WANG Xitao, XUE Fei. THE MICROSTRUCTURE AND TENSILE FRACTURE BEHAVIOR OF LONG TERM THERMAL AGED Z3CN20-09M STAINLESS STEEL[J]. Acta Metall Sin, 2013, 49(2): 175-180.

全文: PDF(2430 KB)  
摘要: 

利用TEM和HRTEM研究了400 ℃热老化2~104 h后Z3CN20--09M不锈钢的微观组织, 用纳米力学探针研究了微区力学性能. 结果表明: 相比于原始状态, 经400 ℃热老化2~104 h后, Z3CN20-09M不锈钢中的铁素体发生了调幅分解并且析出了G相, 导致铁素体的硬度增加和塑性变形能力下降. 利用原位疲劳试验机、SEM和电子探针研究了400 ℃热老化2~10^4 h后Z3CN20-09M不锈钢的微型平板试样拉伸行为. 结果表明: 热老化后, 不锈钢的屈服强度和断裂强度升高, 延伸率下降. 热老化不锈钢中铁素体发生解理断裂, 微裂纹萌生于相界并向铁素体内扩展; 奥氏体主要发生微孔聚集型韧性断裂, 并且在局部区域发生撕裂. 调幅分解是铁素体发生硬脆化和热老化前后Z3CN20-09M不锈钢拉伸断裂行为发生改变的根本原因.

 
关键词 : Z3CN20-09M不锈钢,  热老化,  调幅分解,  G相,  拉伸行为    
Abstract:

Cast austenite stainless steels (CASS) were widely used in the primary circuit piping of pressurized water nuclear reactors (PWRs), for their excellent mechanical behavior, corrosion resistance and good weldability.CASS, however, were known to have a tendency of thermal aging embrittlement after long term service at mid-temperature (about 280-320℃). The microstructures, micro-mechanical properties and tensile fracture behaviors of Z3CN20-09M stainless steels, thermal aged at 400 ℃ for 2~104 h, were studied in this work. TEM was utilized to observe the microstructure. A nano-indenter was used to investigate the micro-mechanical properties. The tensile tests were completed by an in situ fatigue tester. The tensile surface morphology was observed in SEM and the fracture of thermal aged CASS was examined by an electron probe micro-analyzer (EPMA). The results indicated that the spinodal decomposition and G-phase precipitation distributed in ferrite of the aged CASS. The nano-hardness of ferrite increased and the plastic deformation ability of ferrite phase declined. After long-term aging, the yield strength and ultimate strength increased but the elongation declined. Cleavage features were observed in the ferrite phase of thermal aged CASS. It was also found that micro-cracks initiated at phase boundaries and extended toward the ferrite phase. Ductile dimples and tearing at some areas were shown in the austenite phase in the thermal aged CASS. The spinodal decomposition was considered to be the primary mechanism for the change of the tensile fracture behaviors of Z3CN20-09M stainless steel before and after thermal aging.

Key words: Z3CN20-09M stainless steel    thermal aging, spinodal decomposition    G-phase, tensile behavior
收稿日期: 2012-09-23     
基金资助:

国家高技术研究发展计划项目2012AA050901和2012AA03A507资助

作者简介: 凯, 男, 1988年生, 硕士生

[1] Chung H M, Leax T R. Mater Sci Technol, 1990; 6: 249


[2] Hausild P, Berdin C, Bompard P, Verdiere N. Int J Pressure Vessels Piping, 2001; 78: 607

[3] Yukhanov V A, Shur A D. Met Sci Heat Treat, 2006; 48: 295

[4] Miller M K, Hyde J M, Cerezo A, Smith G D W. Appl Surf Sci, 1995; 87--88: 323

[5] Miller M K, Russell K F. Appl Surf Sci, 1996; 94--95: 398

[6] Danoix F, Auger P, Blavette D. Microsc Microanal, 2004; 10: 349

[7] Timofeev B T, Nikolaev Y K. Int J Pressure Vessels Piping, 1999; 76: 849

[8] Ukadgaonker V G, Babu R S. Int J Pressure Vessels Piping, 1996; 69: 135

[9] Haste T J, Birchley J, Richner M. Nucl Eng Des, 2010; 240: 1599

[10] Li S L, Wang Y L, Li S X, Wang X T. Acta Metall Sin, 2010; 46: 1186

 (李时磊, 王艳丽, 李树肖, 王西涛. 金属学报, 2010; 46: 1186)

[11] Xue F, Wang Z X, Shu G G, Yu W W, Shi H J, Ti W X. Nucl Eng Des, 2009; 239: 2217

[12] Mathew M D, Lietzan L M, Murty K L, Shah V N. Mater Sci Eng, 1999; A269: 186

[13] Jayet--Gendrot S, Gilles P, Migne C. Nucl Eng Des, 2000; 197: 141

[14] Vogt J B, Massol K, Foct J. Int J Fatigue, 2002; 24: 627

[15] Nystrom M, Karlsson B. Mater Sci Eng, 1996; A215: 26

[16] Li S L, Wang X T, Wang Y L, Li S X. Acta Metall Sin, 2011; 47: 751

 (李时磊, 王西涛, 王艳丽, 李树肖. 金属学报, 2011; 47: 751)

[17] Wang Z X, Xue F, Guo W H, Shi H J, Zhang G D, Shu G. Nucl Eng Des, 2010; 240: 2538

[18] Sahu J K, Krupp U, Ghosh R N, Christ H J. Mater Sci Eng, 2009; A508: 1

[19] Chopra O K, Chung H M. Nucl Eng Des, 1985; 89: 305

[20] Chung H M. Int J Pressure Vessels Piping, 1992; 50: 179

[21] Kawaguchi S, Sakamoto N, Takano G, Matsuda F, Kikuchi Y, Mraz L.

 Nucl Eng Des, 1997; 174: 273

[22] Yamada T, Okano S, Kuwano H. J Nucl Mater, 2006; 350: 47

[23] Weng K L, Chen H R, Yang J R. Mater Sci Eng, 2004; A379: 119

[24] Yao Y H, Wei J F, Wang Z P. Mater Sci Eng, 2012; A551: 116

[25] Vitek J M. Metall Trans, 1987; 18A: 154

[26] Yu Y N. Fundamentals of Materials Science. Bejing: Higher Education Press,

 (余永宁. 材料科学基础. 北京: 高等教育出版社, 2006: 383)

[27] M'Cirdi L, Lebrun J L, Inal K, Barbier G. Acta Mater, 2001; 49: 3879

 
[1] 项兆龙, 张林, XIN Yan, 安佰灵, NIU Rongmei, LU Jun, MARDANI Masoud, HAN Ke, 王恩刚. Cr含量对FeCrCoSi永磁合金调幅分解组织及其性能的影响[J]. 金属学报, 2022, 58(1): 103-113.
[2] 林晓冬,彭群家,韩恩厚,柯伟. 退火对热老化308L不锈钢焊材显微结构的影响[J]. 金属学报, 2019, 55(5): 555-565.
[3] 刘建学, 席文君, 李能, 李树杰. 界面能调控熔体中纳米颗粒分布铝热合成铁基ODS合金[J]. 金属学报, 2017, 53(8): 1011-1017.
[4] 张海,李时磊,刘刚,王艳丽. 热加工对Z3CN20-09M双相不锈钢组织及热老化冲击断裂行为的影响[J]. 金属学报, 2017, 53(5): 531-538.
[5] 谢君,于金江,孙晓峰,金涛,杨彦红. 温度对高W含量K416B镍基合金拉伸行为的影响*[J]. 金属学报, 2015, 51(8): 943-950.
[6] 王星, 席文君, 崔跃, 李树杰. 铝热合成NiAl共格强化的FeNiCrAl合金的组织演化机理和力学性能[J]. 金属学报, 2015, 51(4): 483-491.
[7] 向红亮, 郭培培, 刘东. 含Ag抗菌双相不锈钢组织及抗菌性能研究[J]. 金属学报, 2014, 50(10): 1210-1216.
[8] 李时磊 王西涛 王艳丽 李树肖. 热老化对Z3CN20-09M不锈钢微区力学性能和冲击断裂行为的影响[J]. 金属学报, 2011, 47(6): 751-756.
[9] 李时磊 王艳丽 李树肖 王西涛. 长期热老化对铸造奥氏体不锈钢组织和性能的影响[J]. 金属学报, 2010, 46(10): 1186-1191.
[10] 王六定; 康沫狂 . 关于Daniel—Lipson调幅波长公式的适用性问题[J]. 金属学报, 2000, 36(8): 793-795 .
[11] 尹钟大;李晓东;李海滨;来忠红. 18Ni马氏体时效钢时效机理的研究[J]. 金属学报, 1995, 31(1): 7-13.
[12] 张喜燕;武小雷;康沫狂;杨延清;孟祥康;韩栋. 含Si钢下贝氏体转变初期碳原子的调幅分解[J]. 金属学报, 1994, 30(7): 327-330.
[13] 任晓兵;王笑天;清水谦一;唯木次男. Fe-1.83C马氏体调幅分解的TEM研究[J]. 金属学报, 1994, 30(7): 289-295.
[14] 张志方;张志东;袁方;王业宁. Mn-Cu合金马氏体相变与沉淀的内耗[J]. 金属学报, 1991, 27(1): 7-10.
[15] 江伯鸿;张美华;魏庆;徐祖耀. 三元系调幅分解的热力学判据[J]. 金属学报, 1990, 26(5): 79-85.