Fe-C-Mn-Si钢中奥氏体共格孪晶界对贝氏体铁素体变体选择的影响 |
王西霞,郭晖, 王鼎, 白银, 杨善武, 贺信莱 |
北京科技大学材料科学与工程学院, 北京 100083 |
|
INFLUENCE OF COHERENT AUSTENITE TWIN BOUNDARIES ON THE VARIANT SELECTION OF BAINITIC FERRITE IN Fe-C-Mn-Si STEELS |
WANG Xixia, GUO Hui, WANG Ding, BAI Yin, YANG Shanwu, HE Xinlai |
School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
王西霞,郭晖, 王鼎, 白银, 杨善武, 贺信莱. Fe-C-Mn-Si钢中奥氏体共格孪晶界对贝氏体铁素体变体选择的影响[J]. 金属学报, 2012, 48(4): 385-392.
,
,
,
,
,
.
INFLUENCE OF COHERENT AUSTENITE TWIN BOUNDARIES ON THE VARIANT SELECTION OF BAINITIC FERRITE IN Fe-C-Mn-Si STEELS[J]. Acta Metall Sin, 2012, 48(4): 385-392.
[1] Guo Z, Lee C S, Morris J W. Acta Mater, 2004; 52: 5511
[2] Kitahara H, Ueji R, Ueda M, Tsuji N, Minamino Y. Mater Charact,2005; 54: 378
[3] Kitahara H, Ueji R, Tsuji N, Minamino Y. Acta Mater, 2006; 54: 1279
[4] Kitahara H, Ueda M, Tsuji N, Minamino Y. Mater Sci Forum, 2006; 512: 117
[5] Sandvik B P J. Metall Trans, 1982; 13A: 77
[6] Furuhara T, Kawata H, Morito S, Maki T. Mater Sci Eng, 2006; A431: 228
[7] Pancholi V, Krishnan M, Samajdar I S, Yadav V, Ballal N B. Acta Mater, 2008; 56: 2037
[8] Furuhara T, Kawata H, Morito S, Miyamoto G, Maki T. Metall Mater Trans, 2008; 39A: 1003
[9] Furuhara T, Maki T. Mater Sci Eng, 2001; A312: 146
[10] Babu S S, Bhadeshia H K D H. Mater Sci Eng, 1991; A142: 209
[11] Cho J Y, Suh D W, Kang J H, Lee H C. ISIJ Int, 2002; 42: 1321
[12] Suh D W, Kang J H, Oh K H, Lee H C. Scr Mater, 2002; 46: 375
[13] Kim D W, Suh D W, Qin R S, Bhadeshia H K D H. J Mater Sci,2010; 45: 4126
[14] Cui G B, Guo H, Yang S W, He X L. Acta Metall Sin,2009; 45: 680
(崔桂彬, 郭晖, 杨善武, 贺信莱. 金属学报, 2009; 45: 680)
[15] Guo H, Bai Y, Yang S W, He X L. Mater Sci Forum,2010; 654-656: 2326
[16] Hackenber R E, Nordstrom D P, Shiflet G J. Scr Mater,2002; 47: 357
[17] Hackenber R E, Shiflet G J. Philos Mag, 2003; 83: 3367
[18] Hackenberg R E, Shiflet G J. Acta Mater, 2003; 51: 2131
[19] Miyamoto G, Takayama N, Furuhara T. Scr Mater,2009; 60: 1113
[20] Luo C P, Liu J W, Xiao X L. Acta Metall Sin, 1998; 34: 1009
(罗承萍, 刘江文, 肖晓玲. 金属学报, 1998; 34: 1009)
[21] Liu Z C, Wang H Y. Heat Treat Technol Equip, 2009; 30(5); 1
(刘宗昌, 王海燕. 热处理技术与装备, 2009; 30(5): 1)
[22] Fang H S, Bo X Z, Zheng Y K, Huang J F. Heat Treat Met,1998; 11: 1
(方鸿生, 薄祥正, 郑燕康, 黄进峰. 金属热处理, 1998; 11: 1)
[23] Yang P. EBSD Technique and its Application. Beijing: Metallurgy Industry Press, 2007: 55
(杨 平. 电子背散射衍射技术及其应用. 北京: 冶金工业出版社, 2007: 55)
[24] Lee J K, Aaronson H I. Acta Metall, 1979; 23: 799
[25] Lee J K, Aaronson H I. Acta Metall, 1979; 23: 809
[26] Ameyama K, Maki T, Tamura I. J Jpn Inst Met, 1986; 50: 602
[27] Furuhara T, Takage S, Watanabe H, Maki T. Metall Mater Trans, 1996; 27A: 1635 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|