| 不同酸溶液中制备纳米结构MnO2单晶 |
| 陈永1, 2),洪玉珍1, 2),马艳平1, 2),杨昊1, 2),李健保1, 2) |
1) 海南大学硅锆钛资源综合开发与利用海南省重点实验室, 海口 570228
2) 海南大学海南优势资源化工材料应用技术教育部重点实验室, 海口 570228 |
|
| PREPARATION OF NANOSTRUCTURE MnO$_{\bf 2}$ SINGLE CRYSTAL IN VARIOUS ACID SOLUTION |
| CHEN Yong1, 2), HONG Yuzhen1, 2), MA Yanping1, 2), YANG Hao1, 2), LI Jianbao1, 2) |
1) Hainan Provincial Key Laboratory of Research on Utilization of Si--Zr--Ti Resources, Hainan University, Haikou 570228
2) Ministry of Education Key Laboratory of Application Technology of Hainan Superior Resources Chemical Materials, Hainan University, Haikou 570228 |
引用本文:
陈永 洪玉珍 马艳平 杨昊 李健保. 不同酸溶液中制备纳米结构MnO2单晶[J]. 金属学报, 2010, 46(7): 857-861.
,
,
,
,
.
PREPARATION OF NANOSTRUCTURE MnO$_{\bf 2}$ SINGLE CRYSTAL IN VARIOUS ACID SOLUTION[J]. Acta Metall Sin, 2010, 46(7): 857-861.
| [1] Liao M Y, Lin J M, Wang J H, Yang C T, Chou T L, Mok B H. Electrochem Commun, 2003; 5: 312
[2] Reddy R N, Reddy R G. J Power Sources, 2004; 132: 315
[3] Ataherian F, Zolfaghari A, Jafari S M, Ghaemi M. Electrochim Acta, 2008; 53: 4607
[4] Park M S, Yoon W Y. J Power Sources, 2003; 114: 237
[5] Manickam M, Singh P, Issa T B, Thurgate S, Marco R D. J Power Sources, 2004; 130: 254
[6] Sugantha M, Ramakrishnan P A, Hermann A M, Warmsingh C P, Ginley D S. Int J Hydrogen Energy, 2003; 28: 597
[7] Ghaemi M, Gholami A, Moghaddam R B. Electrochim Acta, 2008; 53: 3250
[8] Reddy A L M, Shaijumon M M, Gowda S R, Ajayan P M. Nano Lett, 2009; 9: 1002
[9] Devaraj S, Munichandraiah N. J Phys Chem, 2008; 112C: 4406
[10] Wang X, Li Y D. J Am Chem Soc, 2002; 124: 2880
[11] Wang X, Li Y D. Chem Eur J, 2003; 9: 300
[12] Xiao T D, Bokhimi X, Benaissa M, Perez R, Strutt P R, Yacaman M J. Acta Mater, 1997; 45: 1685
[13] Yuan Z Y, Zhang Z, Du G, Ren T Z, Su B L. Chem Phys Lett, 2003; 378: 349
[14] Wang X, Li Y. J Am Chem Soc, 2002; 124: 2880
[15] Zhang Y, Chen L, Zheng Z, Yang F. Solid State Sci, 2009; 11: 1265
[16] Huang X, Lv D, Yue H, Attia A, Yang Y. Nanotechnology, 2008; 19: 225606
[17] Wei M, Konishi Y, Zhou H, Sugihara H, Aiakawa H. Nanotechnology, 2005; 16: 245
[18] Chen Y, Liu C, Li F, Cheng H M. J Alloys Compd, 2005; 397: 282
[19] Chen Y, Hong Y, Ma Y, Li J. J Alloys Compd, 2010; 490: 331
[20] Kijima N, Yasuda H, Sato T, Yoshimura Y. J Solid State Chem, 2001; 159: 94
[21] Muraoka Y, Chiba H, Atou T, Kikuchi M, Hiraga K, Syono Y. J Solid State Chem, 1999; 144: 136 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|