| 相场法模拟动力学各向异性对过冷熔体中晶体生长的影响 |
| 赵达文;李金富 |
| 上海交通大学材料科学与工程学院金属基复合材料国家重点实验室; 上海 200240 |
|
| PHASE–FIELD SIMULATION OF THE EFFECT OF KINETIC ANISOTROPY ON CRYSTAL GROWTH IN UNDERCOOLED MELTS |
| ZHAO Dawen; LI Jinfu |
| State Key Laboratory of Metal Matrix Composites; School of Materials Science and Engineering; Shanghai Jiao Tong University; Shanghai 200240 |
引用本文:
赵达文 李金富. 相场法模拟动力学各向异性对过冷熔体中晶体生长的影响[J]. 金属学报, 2009, 45(10): 1237-1241.
,
.
PHASE–FIELD SIMULATION OF THE EFFECT OF KINETIC ANISOTROPY ON CRYSTAL GROWTH IN UNDERCOOLED MELTS[J]. Acta Metall Sin, 2009, 45(10): 1237-1241.
| [1] Langer J S. Directions in Condense Matter. Singapore: World Scientific, 1986: 164
[2] Caginalp G, Fife P. Phys Rev, 1986; 34B: 4940
[3] Karma A, Rappel W J. hys Rev, 1998; 57E: 4323
[4] Karma A, Lee Y H, Plapp M. Phys Rev, 2000; 61E: 3996
[5] Haxhimali T, Karma A, Gonzales F. Nat Mater, 2006; 5: 660
[6] Boettinger W J, Warren J A, Beckermann C. Annu Rev Mater Res, 2002; 32: 163
[7] Li J J, Wang J C, Yang G C. Acta Mater, 2007; 55: 825
[8] Li J J, Wang J C, Yang G C. Acta Phys Sin, 2007; 56: 1514
(李俊杰, 王锦程, 杨根仓. 物理学报, 2007; 56: 1514)
[9] Li J J, Wang J C, Yang G C. J Cryst Growth, 2007; 309: 65
[10] Zhu Y C, Wang J C, Yang G C, Yang Y J. Acta Phys Sin, 2007; 56: 5542
(朱耀产, 王锦程, 杨根仓, 杨玉娟. 物理学报, 2007; 56: 5542)
[11] Zhang R J, Jing T, Liu B C. Acta Mater, 2006; 54: 2235
[12] Cui H B, Guo J J, Su Y Q, Wu S P. Acta Metall Sin, 2007; 43: 907
(崔红保, 郭景杰, 苏彦庆, 吴士平. 金属学报, 2007; 43: 907)
[13] Langer J S. Phys Rev, 1986; 33A: 435
[14] Kessler D A, Levine H. Phys Rev, 1986; 33B: 7867
[15] Amar M B, Pomeau Y. Euro Phys Lett, 1986; 2: 307
[16] Brener E A. Adv Phys, 1991; 40: 53
[17] Zienkiewicz O C, Zhu J Z. Int J Numer Meth Eng, 1987; 24: 337
[18] Zhao D W, Yang G C, Wang J C, Zhu Y C. Prog Nat Sci, 2006; 16: 1009
(赵达文, 杨根仓, 王锦程, 朱耀产. 自然科学进展, 2006; 16: 1009)
[19] Ihle T, Muller–Krumbhaar H. Phys Rev, 1994; 49E: 2972
[20] Mullins W W, Sekerka R F. J Appl Phys, 1963; 34: 323
[21] Mullins W W, Sekerka R F. J Appl Phys, 1964; 35: 444
[22] Langer J S. Rev Mod Phys, 1980; 52: 1 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|