| 低碳钢形变诱导铁素体相中C原子扩散行为与稳定性研究 |
| 赵河山 李殿中 刘朝霞 李依依 |
| 中国科学院金属研究所; 沈阳 110016 |
|
| INVESTIGATION ON DIFFUSION OF CARBON ATOMS AND STABILITY OF DEFORMATION INDUCED FERRITE IN A LOW CARBON STEEL |
| ZHAO Heshan; LI Dianzhong; LIU Zhaoxia; LI Yiyi |
| Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
赵河山; 李殿中; 刘朝霞; 李依依 . 低碳钢形变诱导铁素体相中C原子扩散行为与稳定性研究[J]. 金属学报, 2007, 43(3): 286-290 .
,
,
,
.
INVESTIGATION ON DIFFUSION OF CARBON ATOMS AND STABILITY OF DEFORMATION INDUCED FERRITE IN A LOW CARBON STEEL[J]. Acta Metall Sin, 2007, 43(3): 286-290 .
[1]Yang Z M,Wang R Z.ISIJ Int,2003;43:761 [2]Priestner R,Hodgson P D.Mater Sci Technol,1992;8: 849 [3]Matsumura Y,Yada H.Trans Iron Steel Inst Jpn,1987; 27:492 [4]Hodgson P D,Hickson M R,Gibbs R K.Set Mater,1999; 40:1179 [5]Hurley P J,Hodgson P D,Muddle B C.Scr Mater, 1999;40:433 [6]Hodgson P D,Hickson M R,Gibbs R K.Mater Sci ??Forum,1998;284:63 [7]Choo W Y,Kor J.Inst Met Mater,1998;36:1966 [8]Hong S C,Lim S H,Lee K J,Shin D H,Lee K S.ISIJ Int,2003;43:394 [9]Hong S C,Lee K S.Mater Sci Eng,2002;A323:143 [10]Li C M,Yada H,Yamagata H.ISIJ Int,1999;39:209 [11]Hickson M R,Gibbs R K,Hodgson P D.ISIJ Int,1999; 39:1176 [12]Yang W Y,Qi J J,Sun Z Q,Yang P.Acta Metall Sin, 2004;40:135 (杨王玥,齐俊杰,孙祖庆,杨平.金属学报,2004;40:135) [13]Liu Z X,Tong M M,Huang C J,Li D Z.Acta Metall Sin, 2004;40:930 (刘朝霞,佟铭明,黄成江,李殿中.金属学报,2004;40:930) [14]Christian J W.The Theory of Transformations in Metal and Alloys.Oxford:Pergamon,1981 [15]Hillert M.Metall Trans,1975;6A:5 [16]Lan Y J.Ph.D Theses,Institute of Metal Research,Chi- nese Academy of Sciences,Shenyang,2005: (兰勇军.中国科学院金属研究所博士学位论文,沈阳,2005) [17]Weng Y Q.Ultrafine Grained Steel.Beijing:Metallurgical Industry Press,2003:119 (翁宇庆.超细晶钢.北京:冶金工业出版社,2003:119) |
|