| 放电等离子烧结过程中粉末颗粒内部温度场的模拟及颈部演变 |
| 刘雪梅;宋晓艳;张久兴 |
| 北京工业大学材料学院新型功能材料教育部重点实验室; 北京100022 |
|
| Temperature Distribution Simulation and Neck Evolution of Powder Particles During Spark Plasma Sintering |
| LIU Xuemei; SONG Xiaoyan; ZHANG Jiuxing |
| College of Materials Science and Engineering; Key Laboratory of Functional Materials of the Education Ministry; Beijing University of Technology; Beijing 100022 |
引用本文:
刘雪梅; 宋晓艳; 张久兴 . 放电等离子烧结过程中粉末颗粒内部温度场的模拟及颈部演变[J]. 金属学报, 2006, 42(7): 757-762 .
,
,
.
Temperature Distribution Simulation and Neck Evolution of Powder Particles During Spark Plasma Sintering[J]. Acta Metall Sin, 2006, 42(7): 757-762 .
[1] Angerer P,Yu L G,Khor K A,Korb G,Zalite I. Eur Ceram Soc, 2005; 25: 1919 [2] Zhou A G, Wang C A, Huang Y. Mater Sci Eng, 2003;A352: 333 [3] Zavaliangos A, Zhang J, Krammer M,Groza J R.Mater Sci Eng, 2004; A379: 218 [4] Zhang J X, Liu K G, Zhou M L. Powder Metall Technol,2002; 20(3): 129 (张久兴,刘科高,周美玲.粉末冶金技术,2002;20(3):129) [5] Mamedov V. Powder Metall, 2002; 45: 322 [6] Tokita M. In:Kosuge K,Nagai H.Nagai eds.,Proc of the 2000 Powder Metallurgy World Congress,Japan:Japanese Society of Powder and Powder Metallurgy, 2001;729 [7] Khor K A, Yu L G, Chan S H, Chen X J. Eur Ceram Soc,2003; 23: 1855 [8] Kim Y H, Kang J H, Kim J S, Kim W T, Kwon Y S. In:Proc NEDO Int Symp on Functionally Graded Materials,Kyoto, Japan, 1999: 123 [9] Omori M. Mater Sci Eng, 2000; A287:183 [10] Guo S J. The Sintering Theory of Powders (Ⅱ). Beijing:Metallurgical Industry Press, 1998: 4 (果世驹.粉末烧结理论,(Ⅱ).北京:冶金工业出版社,1998: 4) [11] Song X Y, Liu X M, Zhang J X. J Am Ceram Soc, 2006; 89: 494 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|