| 细观非均质性对多晶材料塑性行为的影响 |
| 耿小亮 张克实 郭运强 秦 亮 |
| 西北工业大学工程力学系; 西安 710072 |
|
| Influence of Microsturcture Hetero--Geneousity on Polycrystallineplastic Behavior |
| GENG Xiaoliang; ZHANG Keshi; GUO Yunqiang; QIN Liang |
| Department of Engineering Mechanics; Northwestern Polytechnical University; Xi'an 710072 |
引用本文:
耿小亮; 张克实; 郭运强; 秦亮 . 细观非均质性对多晶材料塑性行为的影响[J]. 金属学报, 2006, 42(1): 49-53 .
,
,
,
.
Influence of Microsturcture Hetero--Geneousity on Polycrystallineplastic Behavior[J]. Acta Metall Sin, 2006, 42(1): 49-53 .
[1]Taylor G L,Elam C F.Proc R Soc Lond,1925;A108:28 [2]Hill R,Rice J R.J Mech Phys Solid,1972;20:401 [3]Hutchinson J W.Proc R Soc Lond,1976;A348;101 [4]Asaro R J.J Appl Mech,1983;50:924 [5]Peirce D,Asaro R J,Needleman A.Acta Metall,1983;31:1951 [6]Maniatty A M,Dawson P R,Lee Y S.Int J Numberical Methods Eng,1992;35:1565 [7]Rashid M M,Nemat-Nasser S.Comp Methods Appl Mech Eng,1992;94:201 [8]Steinmann P,Stein E.Comput Methods Appl Mech Eng,1996;129:235 [9]Sarma G,Zacharia T.J Mech Phys Solid,1999;47:1219 [10]Zhang K S,Wu M S,Feng R.Int J Plast,2005;4:801 [11]Taylor G L.J Inst Met,1938;62:307 [12]Lin T.H.J Mech Phys Solid,1957;5:143 [13]Toth L S,Molinari A,Zouhai N.Mech Mater,2000;32:99 [14]Turkmen H S,Dawson P R,Miller M P.Int J Plast,2002;18:941z |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|