| 人造金刚石单晶铁基金属包膜的精细结构 |
| 许 斌; 崔建军;王淑华;李木森;李成美;冯立明 |
| 山东建筑工程学院材料科学与工程系; 济南 250014 |
|
| Fine Structures Of The Fe--Based Metal Film Covering Synthetic Diamond Single Crystal |
| XU Bin; CUI Jianjun; WANG Shuhua;LI Musen; LI Chengmei; FENG Liming |
| Department of Materials Science & Engineering; Shandong Institute of Architecture and Engineering; Jinan 250014 |
引用本文:
许斌; 崔建军; 王淑华; 李木森; 李成美; 冯立明 . 人造金刚石单晶铁基金属包膜的精细结构[J]. 金属学报, 2005, 41(4): 444-448 .
,
,
,
,
,
.
Fine Structures Of The Fe--Based Metal Film Covering Synthetic Diamond Single Crystal[J]. Acta Metall Sin, 2005, 41(4): 444-448 .
[1]Sung J. J Mater Sci, 2000; 35: 6041 [2]Lin Q Y, Zhu Y Y, Zhang Y Z, Wu B Q, Zhang X L. J Iron Steel Res, 1999; 11(2): 51 (林清英,朱衍勇,张燕征,吴伯群,张秀林.钢铁研究学报, 1999;11(2):51) [3]Strong H M, Hanneman R E. J Chem Phys, 1967; 46: 3668 [4]Hao Z Y, Chen Y F, Zou G T. Synthetic Diamond. Changchun: Jilin University Press, 1996: 74 (郝兆印,陈宇飞,邹广田.人工合成金刚石.长春:吉林大学 出版社, 1996:74) [5]Shen Z T. Diamond Ind, 2000; 5: 1 (沈主同.工业金刚石, 2000;5:1) [6]Xu B, Li M S, Gong J H, Yin L W, Cui J J, Cheng K J. J Synth Cryst, 2002; 31(1): 75 (许斌,李木森,宫建红,尹龙卫,崔建军,程开甲.人工晶 体学报,2002;31(1):75) [7]Yin L W, Li M S, Gong Z G, Bai Y J, Li F Z, Hao Z Y. Appl Phys A, 2003; 76: 1061 [8]Zhang K C, Zhang L H. Science and Technology in Crystal Growth. Beijing: Science Press, 1997: 197 (张克丛,张乐漶.晶体生长科学与技术.北京:科学出版社, 1997:197) [9]Xu B, Li M S, Yin L W, Cui J J, Liu Y X, Gong J H. Chin Sci Bull, 2002; 47: 1258 [10]Chattarji D. Theory of Auger Transition. London: Academic Press, 1979: 132 [11]Yin L W. Ph.D Dissertation, Shandong University, Jinan, 2001 (尹龙卫.山东大学博士论文,济南, 2001) [12]Hua Z Y, Luo W A. Analysis for Surface. Shanghai: Fu dan University Press, 1989: 89 (华中一,罗维昂.表面分析.上海;复旦大学出版社. 1989: 89) [13]Li X. Ph.D Dissertation, Jilin University, Changchun, 2002 (李迅.吉林大学博士学位论文,长春, 2002) |
|