| 电磁场对金属凝固界面前沿颗粒行为及分布的影响 |
| 孙秋霞;钟云波;任忠鸣;楼磊;邓康;徐匡迪 |
| 上海大学上海市现代冶金与材料制备重点实验室; 上海 200072 |
|
| Effect of electromagnetic field on the behavior and distribution of the particles in front of metallic solidification interface |
| SUN Qiuxia; ZHONG Yunbo; REN Zhongming; LOU Lei; DENG Kang; XU Kuangdi |
| Shanghai Enhanced Laboratory of Modern Metallurgy & Materials Processing; Shanghai University; Shanghai 200072 |
引用本文:
孙秋霞; 钟云波; 任忠鸣; 楼磊; 邓康; 徐匡迪 . 电磁场对金属凝固界面前沿颗粒行为及分布的影响[J]. 金属学报, 2005, 41(3): 321-325 .
,
,
,
,
,
.
Effect of electromagnetic field on the behavior and distribution of the particles in front of metallic solidification interface[J]. Acta Metall Sin, 2005, 41(3): 321-325 .
[1] Uhlmann D R, Chalmers B, Jackson K A. J Appl Phys, 1964; 35: 2986 [2] Omenyi S N, Neumann A W. J Appl Phys, 1976; 47: 3956 [3] Boiling G F, Cisse J. J Cryst Growth, 1971; 10: 56 [4] Cisse J, Boiling G F. J Cryst Growth, 1971; 10: 67 [5] Korber C, Rau G. J Cryst Growth, 1985; 72: 649 [6] Stefanescu D M, Dhindaw B K, Kacar S A. Metall Trans, 1988; 19A: 2847 [7] Garvin J W, Udaykumar H S. J Cryst Growth, 2003; 252: 451 [8] Hadji L. Scr Mater, 2003; 48: 665 [9] Shangguan D, Ahuja S, Stefanescu D M. Metall Trans, 1992; 23A: 669 [10] Wu S S, Nakae Hideo. Spec Found Nonferrous Alloy, 1998; (3):34 (吴树森,中江秀雄.特种铸造及有色合金, 1998;(3):34) [11] Zhong Y B, Ren Z M, Sun Q X, Deng K, Xu K D. Acta Metall Sin, 2003; 39: 1269 (钟云波,任忠鸣,孙秋霞,邓康,徐匡迪.金属学报,2003; 39:1269) [12] Marty P, Alemany A. In: Moffatt H K, Proctor M R E, eds., Proc Symp Int Union of Theoretical and Applied Mechanics (IUTAM), London: The Metals Society, 1982: 245 [13] Taniguchi S, Brimacombe J K. In: Asoi A, ed., Int Symp Electromagnetic Processing Materials, Nagoya, Iron and Steel Institute of Japan, 1994: 429 [14] Zhong Y B, Sun Q X, Ren Z M, Deng K, Xu K D. In: Asai S, Fautrelle Y, Gillon P, eds., Proc 4th Int Conf on Electromagnetic Processing of Materials (EPM 2003), Nagoya, Iron and Steel Institute of Japan, 2003: 404 [15] Han Q, Hunt J D. ISIJ Int, 1995; 35: 693 [16] Leenov D, Kolin A. J Chem Phys, 1954; 22: 683 [17] Kolin A. Science, 1953; 117: 134 [18] Han Q Y, Hunt J D. Acta Metall Sin, 1996: 32: 363 (韩青有,Hunt J D.金属学报,1996;32:363) [19] Li Q C. Theory of Cast Forming. Beijing: China Machine Press, 1982: 89 (李庆春.铸件形成理论.北京:机械工业出版社, 1982:89)f |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|