| 基于分形的金属材料海水腐蚀形貌图像分析诊断系统 |
| 王守琰;宋诗哲 |
| 天津大学材料学院 |
|
| Corrosion Morphology Diagnosing Syste Of Metallic Materials In Seawater Based On Fractal |
| WANG Shouyan;SONG Shizhe |
| School of Materials; Tianjin University |
引用本文:
王守琰; 宋诗哲 . 基于分形的金属材料海水腐蚀形貌图像分析诊断系统[J]. 金属学报, 2004, 40(1): 94-98 .
,
.
Corrosion Morphology Diagnosing Syste Of Metallic Materials In Seawater Based On Fractal[J]. Acta Metall Sin, 2004, 40(1): 94-98 .
[1] Zhang K H, Wang J R, Zhang Q H. Opto-Electronic Eng, 2001; 28: 52(张坤华,王敬儒,张启衡.光电工程,2001;28:52) [2] Mandelbrot B B, Passoja D E, Paullay A J. Nature, 1984; 308: 721 [3] Costa J M, Sagues F, Vilarrasa M. Corrs Sci, 1991; 32: 665 [4] Chen J, Long Q Y, Chen J Z, Long Q W. J Chin Soc Corros Protect, 1991; 4: 344(陈军,龙起易,陈继志,龙期威.中国腐蚀与防护学报,1991;4:344) [5] Jiang X G, Chu W Y, Xiao J M. J Chin Soc Corros Protect, 1995; 15: 57(蒋兴钢,褚武扬,肖纪美.中国腐蚀与防护学报,1995;15:57) [6] Dong S H, Lv Y M: J Chin Soc Corros Protect, 2001; 2: 106(董绍华,吕英民.中国腐蚀与防护学报,2001;21:106) [7] Dong L K. Theory and Application of Fractal. Shengyang: Liaoning Science and Technology Press, 1990: 174(董连科.分形理论及其应用,沈阳:辽宁科学技术出版社,1990:174) [8] Niruparm S, Chaudhuri B B. Sign Process, 1995; 42: 181 [9] Li K H, Liu Z K, Lin F. J Remot Sens, 2001; 5: 353(李厚强,刘政凯,林峰.遥感学报,1995,5:353) [10] Chaudhuri B, Sarkar N. IEEE Trans Pattern Anal Mach Intellig, 1995; 17: 72 [11] Wang S Y, Kong D Y, Song S Z. Acta Metall Sin, 2001; 37: 517(王守琰,孔德英,宋诗哲.金属学报,2001;37:517) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|