| 原子氧对金属Ag及其表面TiO2-有机硅热控涂层的侵蚀 |
| 张蕾 严川伟 屈庆 |
| 中国科学院金属研究所金属腐蚀与防护国家重点实验室; 沈阳110016 |
|
引用本文:
张蕾; 严川伟; 屈庆 . 原子氧对金属Ag及其表面TiO2-有机硅热控涂层的侵蚀[J]. 金属学报, 2003, 39(9): 984-988 .
[1] Minton T K, Zhang J, Garton D J. High Perform Polym,2000; 12: 27 [2] Grossman E, Lifshitz Y, Wolan J T. Spacecraft Rockets,1999; 36: 75 [3] Hoflund G B, Weaver J F. Measur Sci Technol, 1994; 53:201 [4] Shen Z G, Wang Z T, Zhao X H. J Beijing Univ AeronautAstronaut, 2000; 26: 676(沈志刚,王忠涛,赵小虎.北京航天航空大学学报,2000;26:676) [5] Zhang L, Yan C W, Qu Q, Cao C N. Trans NonferrorsMet Soc Chin, 2002; 12: 869 [6] Zhang L, Yan C W, Qu Q. Corros Sci Protect Technol,2002; 14: 78(张 蕾,严川伟,屈 庆.腐蚀科学与防护技术,2002;14:781 [7] Sun G, Tong J Y, Li J H. Chin Space Sci Technol, 1999; (6) : 53(孙 刚,童靖宇,李金洪.中国空间科学技术,1999;(6) :53) [8] Zhang L, Yan C W, Qu Q. Chin J Mater Res, 2002; 16: 273(张 蕾,严川伟,屈 庆.材料研究学报, 2002;16:273) [9] Zeng Y B, Zhang L Z, Yu Q. Aerasp Mater Technol, 1997; (3) : 18(曾一兵,张廉正,于 翅.宇航材料工艺, 1997;(3) :18) [10] Harada Y, Mell R J. Inorganic Thermal Control Coatings. AAIA-83-0074, 1983 [11] John W, Philip R, Young, Carol G. The Effect of Low Earth Orbit Exposure on Some Experimental Fluorine and Silicon-Containing Polymers. N95-14074: 157, 1995 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|