| PZT压电陶瓷的应力腐蚀 |
| 王毅; 褚武扬; 宿彦京; 高克玮; 刘辉; 乔利杰 |
| 北京科技大学材料物理系; 北京 100083 |
|
| Stress Corrosion Cracking of PZT Piezoelectric Ceramics |
| WANG Yi; CHU Wuyang; SU Yanjing; GAO Kewei; LIU Hui; QIAO Lijie |
| Department of Materials Physics; University of Science & Technology Beijing; Beijing 100083 |
引用本文:
王毅; 褚武扬; 宿彦京; 高克玮; 刘辉; 乔利杰 . PZT压电陶瓷的应力腐蚀[J]. 金属学报, 2003, 39(2): 182-184 .
,
,
,
,
,
.
Stress Corrosion Cracking of PZT Piezoelectric Ceramics[J]. Acta Metall Sin, 2003, 39(2): 182-184 .
[1] Chen C P, Knapp W J. J Am Ceram Soc, 1977; 60: 87 [2] Ritter J E, Humenik J N. J Mater Sci, 1979; 14: 626 [3] Spearing S M, Zok F W, Evans A G. J Am Ceram Soc,1994; 77: 562 [4] Okabe T, Kido M, Miyahara T. Eng Fract Much, 1994;48: 137 [5] Iskevitch E, Chaim R. Philos Mag, 1990; 61: 209 [6] Michalske T A, Freiman S W. J Am Ceram Soc, 1983; 66:284 [7] Michalske T A, Banker B C. J Appl Phys, 1984; 56: 2666 [8] Yu H H, Suo Z. Ada Mater, 1999; 47: 77 [9] Chu W Y, Hsiao C M, Zhao Y S. Metall Trans, 1988; 19A:1067 [10] Cherepanov G P. Mechanics of Brittle Fracture. New York: McGraw-Hill International Book Company, 1977: 29 [11] Fu C L, Painter G S. J Mater Res, 1991; 6: 719 [12] Sanden P. Pokluda J, Wang L G, Sob M. Mater Sci Eng,1977; A234: 370 [13] Gao H C, Evans A G. J Am Ceram Soc, 1993; 76: 890 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|