| 低碳钢过冷奥氏体形变过程中的组织及取向变化 |
| 齐俊杰 杨王玥 孙祖庆 |
| 北京科技大学材料科学与工程学院;北京100083 |
|
引用本文:
齐俊杰; 杨王玥; 孙祖庆 . 低碳钢过冷奥氏体形变过程中的组织及取向变化[J]. 金属学报, 2002, 38(6): 629-634 .
[1] Yang W Y, Hu A M, Qi J J, Sun Z Q. Acta Metall Sin. 2000; 36:1192 (杨王玥.胡安民.齐俊杰.孙祖庆.金属学报.2000;36:1192) [2] Yang W Y, Hu A M. Qi J J, Sun Z Q. Chin J Mater Res, 2001; 15; 171 (杨王玥,胡安民. 齐俊杰.孙祖庆.材料研究学报、2001;15:171) [3] Hu A M, Master Thesis, Univ Sci Technol Beijing, 2000(胡安民. 北京科技大学硕士学位论文.2000) [4] Lewis J. Jonas J J, Mintz B. ISIJ International, 1998: 38:300 [5] Mintz B. Jonas J J. Mater Sci Technol, 1994: 10: 721 [6] Mintz B. Lewis H. Jonas J J.Mater Sci Technol. 1997;13: 379 [7] Pristner R, Ali L. Mater Sci Technol, 1993: 9: 135 [8] Priestner R.Hodgson P D.Mater Sci Technol.1992; 8:849 [9] Beynon J H. Gloss R. Hodgson P D. Mater Forum, 1992;16: 37 [10] Hodgson P D, Hickson M R, Gibbs R K. Scr Mater. 1999;40:1179 [11] Hurley P J, Kelly G L, Hodgson P D. Mater Sci Technol,2000: 16: 1273 [12] Fu Y Y, Yang P, Yang W Y, Sun Z Q. J Univ Sci Technol Beijing. 2000; 22: 170 (傅云义.杨 平. 杨王玥.孙祖庆.北京科技大学学报.2000;22:170) [13] Li L F. Master Thesis. Univ Sci Technol Beijing, 2001(李龙飞.北京科技大学硕士学位论文.2001) [14] Hirosuke I. ISIJ Inter. 1994: 34: 313 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|