| 铁素体不锈钢焊接热影响区晶粒长大过程模拟 |
| 莫春立 李殿中 钱百年 国旭明 |
| 中国科学院金属研究所;沈阳110016 |
|
引用本文:
莫春立; 李殿中; 钱百年; 国旭明 . 铁素体不锈钢焊接热影响区晶粒长大过程模拟[J]. 金属学报, 2001, 37(3): 307-310 .
[1] Anderson M P, Srolovitz D J, Grest G S, Sahni P S. ActaMetall, 1984; 32: 783 [2] Anderson M P, Grest G S, Srolovitz D J. Philos Mag,1989; 59B: 293 [3] Song X Y, Liu G Q. Chin J Mater Res, 1998; 12: 245 (宋晓艳.刘国权.材料研究学报, 1998; 12: 245) [4] Ling S, Andersion M P. J Met, 1992; 44: 30 [5] Grest G S, Glazier J A. Mat Sci Forum, 1992; 39: 94 [6] Gao J H, Thompson R G. Acta mater, 1996; 44: 4565 [7] Shen Y. Master,B Thesis Unversity of Alabama, Birmingham, 1993 [8] Mo C L, Qian B N, Li D Z. Chin J Mater Res, to bepublished (莫春立,钱百年,李殿中.材料研究学报,待发表)- |
|