| Fe中刃型位错及其掺杂体系的电子结构 |
| 牛原 赵栋梁 王崇愚 |
| 钢铁研究总院功能材料所;北京100081 |
|
引用本文:
牛原; 赵栋梁; 王崇愚 . Fe中刃型位错及其掺杂体系的电子结构[J]. 金属学报, 2001, 37(3): 239-242 .
[1] Gehlen P C, Rosenfield A R, Than G T. J Appl Phys,1968; 39: 5246 [2] Gavrilyuk VG, Dekhtyar AI, ProkopenkO VG. FizikaMetallov-i-Metallovedenie, 1981; 52: 1091 [3] Rotthier R, Scheire L, Phariseau P. Physica, 1981; 108A:605 [4] De-Hosson-JThM. Int J Quant Chem, 1980; 18: 575 [5] Gesari S, Irigoyen B, Juan A. J Phys D: Appl Phys, 1998;31: 2179 [6] Delley B. J Chem Phys, 1991; 94: 7245 [7] Kohn W, Sham L J. Phys Rev, 1965; 140: A1133 [8] Wang C Y, Zeng Y P. Science in China, 1992; 35A: 107 [9] Companion A L. J Less-Common Met, 1985; 107: 131$ |
|