| 快凝合金Zr(Ni0.55Mn0.3V0.1Cr0.05)2.1的相结构与储氢性能 |
| 吕光烈 舒康颖 胡秀荣 顾建明 宋雪雁 雷永泉 王启东 |
| 浙江大学分析测试中心;杭州 310028 |
|
引用本文:
吕光烈; 舒康颖; 胡秀荣; 顾建明; 宋雪雁; 雷永泉; 王启东 . 快凝合金Zr(Ni0.55Mn0.3V0.1Cr0.05)2.1的相结构与储氢性能[J]. 金属学报, 1999, 35(5): 453-457 .
[1] Tang W, Sun G. J Alloys Comp, 1994; 203: 195 [2] Ovshinsy S R, Fetcenko M A. J Russ Set, 1993; 176. 260 [3] Hu X R, Gu J M, Chen L S, Lu G L. J Mat Res, 1999; 13:129(胡秀荣,顾建明,陈林深,吕光烈.材料研究学报,1999; 13:129) [4] Zhang W K. Dissertation Submitted to Zhejiang Universityjob the Degree Of Doctor, 1997. 76(张文魁,浙江大学博士学位论文,1997: 76) [5] Louer D, Langford J I. J Appl Cryst, 1988; 21: 430 [6] Lutterotti L, Scardi R. J Appl Cryst, 1990; 23: 246 [7] Lutterotti L, Scardi R. J Appl Cryst, 1992; 25: 459 [8] Prince E. In' YOung R A ed, The Rietveld Method, Oxford:Oxford University Press, 1993: 21 |
|