| 金属间化合物Al5Fe2液固两相结构的相关性 |
| 边秀房 秦敬玉 |
| 山东工业大学材料科学与工程学院; 济南 250061 |
|
引用本文:
边秀房; 秦敬玉 . 金属间化合物Al5Fe2液固两相结构的相关性[J]. 金属学报, 1999, 35(1): 19-22 .
| [1]EnderbyJE,BarnesAC.RepProgPhys,1990;53:85[2]PriceDL,MossSC,ReijersR,SaboungiM-L,SusmanS.JPhys:CondenMater,1989;1:1005[3]McKameyCG,DeVanJH,TortoreliPF,SikkaVK.JMaterRes,1991;6:1779[4]NguyenMD,MayuD,PastureA,Cyrot-LackmanF.JPhysF:MetPhys,1985;15:1911[5]QinJY,BianXF,WangWM,SliousarenkoSI,XuCY,MaJJ.SciChin,1998;41E:182[6]WasedaY.TheStructureofNon-CrystalineMaterials,NewYork:McGraw-Hil,1980:27[7]PowderDiffractionFileAlphabeticalIndex:InorganicPhases,ParkLane:JCPDC,1983:10[8]BlétryJ.ZNaturforsch,1978;33A:327[9]QinJY,BianXF,SliousarenkoSI,WangWM.JPhys:CondenMater,1998;10:1211[10]EliotSR.Nature,1991;354:445[11]BlackPJ,CundalJA.ActaCrystalogr,1966;20:417[12]HomtovaEV,SluhofskiOI,RomanovaAV.JPhys(Ukraine),1986;31:1045(ХомутоваЗВ,СлуховскийОИ,РомановаАВ.Укрфизж,1986;31:1045)[13]EgamiT.JNon-CrystSolids,1996;205-207:575[14]TurnbulD.ActaMetalMater,1990;38:243[15]IsonoN,SimithPM,TurnbulD,AzizMJ.MetalMaterTrans,1996;27A:725" |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|