| 321奥氏体不锈钢单晶应力腐蚀断口的研究 |
| 高克玮;乔利杰;褚武扬;骆静利 |
| 北京科技大学材料物理系;100083;北京科技大学材料物理系;100083;北京科技大学材料物理系;100083;加拿大阿尔伯特大学化学与材料工程系;加拿大阿尔伯特;T6G2G6 |
|
| FRACTOGRAPHIC STUDY OF SCC OF 321 AUSTENITIC STAINLESS STEEL SINGLE CRYSTAL |
| GAO Kewei; QIAO Lijie; CHU Wuyang(Department of Materials Physics; University of Science and Technology Beijing; Beijing 100083)LUO Kingli(Department of Chemical and Materials Engineering; University of Alberta; Alberta; Canada; T6G; 2G6)Correspondent: GAO Kewei; associate professor Tel. (010)62332906; Fax: (010)62327283;E-mail: ljqiao public.bta.net.cn |
引用本文:
高克玮;乔利杰;褚武扬;骆静利. 321奥氏体不锈钢单晶应力腐蚀断口的研究[J]. 金属学报, 1998, 34(8): 888-891.
,
,
,
.
FRACTOGRAPHIC STUDY OF SCC OF 321 AUSTENITIC STAINLESS STEEL SINGLE CRYSTAL[J]. Acta Metall Sin, 1998, 34(8): 888-891.
1 Li S X, Smith D J. Scr Metall Mater 1995; 33: 711 2 Antolovich B F, Saxena A, Antolovich S D. J Mater Eny Performace, 1993; 2: 489 3 Lichter B D, Flanagan W F, Kim J S, Elkenbracht J C, Van Hunen M. Corrosion, 1996; 52: 453 4 Lukas P, Cadek J, Sustek V, Kunz L. Mater Sci Eng, 1996; 208A: 149 5 Stroh A N. Philos Mag, 1956; 1: 489 6 Mimaki T, Nakazawa Y, Hashimoto S, Miuram S. Metall Trans, 1990; 21A: 2355 7 Meletis E I, Hochman R F. Corros Sci, 1984; 24: 843 8 Dickson J I, Li S Q, Bailon J P, Tromans D. The Minerals, Metals Mater Soc, 1992 9 Stroh A N. Proc R Soc London, 1954; 223A: 404 10 Magnin T, Chambreuil A, Bayle B. Acta Mater 1996; 44: 1457u |
|