| 活度、活度相互作用系数数据库软件开发 |
| 罗利华;丁学勇;郭丹;曹文斌;邹宗树;王文忠 |
| 东北大学材料与冶金学院;沈阳;110006;东北大学材料与冶金学院;沈阳;110006;东北大学材料与冶金学院;沈阳;110006;北京科技大学特种陶瓷中心;北京;100083;东北大学材料与冶金学院;沈阳;110006;东北大学材料与冶金学院;沈阳;110006 |
|
| DATABASE SOFTWARE DEVELOPMENT FOR ACTIVITY AND INTERACTION MRAMETER OF ALLOY SYSTEMS |
| LUO Lihua; DING Xueyong; GUO Dan; CAO Wenbin; ZOU Zongshu; WANG Wenzhong (School of Materials and Metallurgy; Northeastern University; Shenyang 110006)( University of Science and Technology Beijing; Beijing 1100083) |
引用本文:
罗利华;丁学勇;郭丹;曹文斌;邹宗树;王文忠. 活度、活度相互作用系数数据库软件开发[J]. 金属学报, 1998, 34(4): 388-392.
,
,
,
,
,
.
DATABASE SOFTWARE DEVELOPMENT FOR ACTIVITY AND INTERACTION MRAMETER OF ALLOY SYSTEMS[J]. Acta Metall Sin, 1998, 34(4): 388-392.
1 Wagner C.Thermodynamics of Alloys.Reading,Massachusetts:Addlson-Wesley,1952:1 2制钢第19委员会编制钢反应推奖平衡值(改订增补).日本学术振兴会,1984:255(Steelmaking Committee No.19.Recommended Equilibrium Data of Steelmaking Reactions(Revised and Supplemented). Science Promotion Committee of Japan; 1984: 255) 3 Eiji Ichise ,Akira Moro-Oka. Trans Iron Steel Inst Jpn, 1988;28:153 4丁学勇,王文忠,韩其勇.金属学报,19931 29:B527(Ding Xueyong, Wang Wenzhong, Han Qiyong. Acta Metall Sin、 1993 29: B527) 5丁学勇,范 鹏,韩其勇.金属学报,19942 30:B49(Ding Xueyong,Fan Peng,Han Qiyong Acta Metall Sin,1994; 30:B49) 6 Miedema A Rt de Chatel P F, de Boer F R. Physica, 1980 100B: 1 7 Tanaka T, Gokcen N A, Morita Z Z Metallkunde, 1990 81: 49 8 丁学勇,王文忠.1994年全国冶金物理化学学术会议论文集.广州,1994:97 (Ding Xueyong,Wang Wenzhong. Proceedings of National Symposium on Meallurgical Physico-Chemistry, Guangzhou, 1994: 97) 9 魏寿昆. 冶金过程热力学.上海:上海科学技术出版社,1980:382Wei Shoukun. Thermodynamics of Metallurgical Processes. Shanghai: Shanghai Science & Technology Press,1980:382 10 魏寿昆. 活度在冶金物理化学中的应用. 北京:中国工业出版社,1964:12 (Wei Shoukun. Activity Application in Metallurgical Physico-Chemistry. Beijing:China Idustry Press,1964:12) 11魏寿昆.从实验数据求活度相互作用系数中的某些问题讲授提纲.北京:北京科技大学,1991:1(Wei Shoukun. Some Problems of Calculating Activity Interaction Parameters from Experimental Data.Beijing: University of Science and Technology Beijing, 1991:1) |
|