| 磷酸处理对TiAl金属间化合物抗氧化性能的影响 |
| 唐兆麟;王福会;吴维 |
| 中国科学院金属腐蚀与防护研究所金属腐蚀与防护国家重点实验室;沈阳;110015;中国科学院金属腐蚀与防护研究所金属腐蚀与防护国家重点实验室;沈阳;110015;中国科学院金属腐蚀与防护研究所金属腐蚀与防护国家重点实验室;沈阳;110015 |
|
| EFFECT OF SURFACE TREATMENT BY PHOSPHORIC ACID ON OXIDATION RESISTANCE OF TiAl INTERMETALLICS |
| TANG Zhaolin; WANG Fuhui; WU Weitao(State Key Laboratory for Corrosion and Protection; Institute of Corrosion and Protection of Metals; The Chinese Academy of Sciences; Shenyang 110015)Coerespondent: TANG Zhaolin; Tel: (024)23915911; Fax: (024)23894149;E-mail: zltang@icpm.syb.ac.cn |
引用本文:
唐兆麟;王福会;吴维. 磷酸处理对TiAl金属间化合物抗氧化性能的影响[J]. 金属学报, 1998, 34(10): 1084-1088.
,
,
.
EFFECT OF SURFACE TREATMENT BY PHOSPHORIC ACID ON OXIDATION RESISTANCE OF TiAl INTERMETALLICS[J]. Acta Metall Sin, 1998, 34(10): 1084-1088.
1 Tetsui T. In: Nathal M V, Datolia K Liu C L, Martin P L, Miracle D B, Wagner R, Yamaguchi M eds, Stractural Intermetallics 1997, Warrendale, PA: Miner Met Mater Soc, 1997: 489 2 Brady M P, Brindley W J, Smialek J L, Locci I. JOM, 1996; 48: 46 3 Tang Zhaolin, Wang Fuhui, Wu Weitao. In: Nathal M V, Darolia R, Liu C L, Martin P L, Miracle D B,Wagner R, Yamaguchi M eds., Structural Intermetallics 1997, Warrendale,PA: Miner Met Mater Soc, 1997:341 4 Taniguchi S.MRS Bull,1994 ; 10: 31 5 贺跃辉,黄伯云,曲选辉,刘业翔.材料研究学报,1996;10:603(He Y H, Huang B Y, Qu X H, Liu Y X.Chin J Mater Res,1996; 10: 603) 6 Zhang Y, Li X, Chen C. In: Nathal M V, Darolia R, Liu C L, Martin P L, Mircle D B, Wagner R,Yamaguchi M eds., Structural Intermetallics 1997, Warendale, PA: Mine Met Mater Soc, 1997: 411 7 熊谷正树,涉江和久,金 睦淳.日本金属学会志,1993;57:721(Kuwi M, Shibue K, Kim M. J Jpn Inst Met, 1993; 57: 721) 8 辛丽.中国科学院金属腐蚀与防护研究所博士学位论文,1997(Xin L. PhD Thesis, Institute of Corrosion and Protection of Metals, The Chinese Academy of Sclemy of Sciences, 1997) 9 Kawnura H, Nishiuo K, Saito T. In: Nathal M V, Darolia R D, Liu C L, Martin P L, Miracle D B,Wagner R, Yamaguchi M eds., Structural Intermetallics 1997, Warrendale, PA: Miner Met Mater Soc,1997: 377t |
|