| Fe—Cr—Al—Si合金阻尼性能研究 |
| 王卫国;周邦新;郑忠民 |
| 中国核动力研究设计院核燃料及材料重点实验室;成都;610041;中国核动力研究设计院核燃料及材料重点实验室;成都;610041;中国核动力研究设计院核燃料及材料重点实验室;成都;610041 |
|
| DAMPING CAPACITY OF Fe-Cr-Al-Si ALLOYS |
| WANG Weiguo; ZHOU Bangxin; ZHENG Zhongmin(Laboratory for Nuclear Fuel and Materials; Nuclear Power Institute of China; Chengdu 610041)Correspondent: WANG Weiguo; Tel: (028)5582199-88531 |
引用本文:
王卫国;周邦新;郑忠民. Fe—Cr—Al—Si合金阻尼性能研究[J]. 金属学报, 1998, 34(10): 1039-1042.
,
,
.
DAMPING CAPACITY OF Fe-Cr-Al-Si ALLOYS[J]. Acta Metall Sin, 1998, 34(10): 1039-1042.
1Masumoto H, Hinai M, Sawsya S. Trans Jpn Inst Met, 1984; 25: 891 2Karimi A, Giaugue P H, Martin J L. Mater Sci Forum, 1995; 179-181: 679 3Hinai M, Sawaya S, Masumoto H. Trans Jpn Inst Met, 1994; 35: 74 4Yamada T, Takamura T, Hashisume S, Odakei T, Omori T, Hation K. NKK Technical Review, No.65, 1992: 21 5佐藤昭治,砂田晃,渡边敏.热处理, 1992; 32: 340 (Sotoh S, Sunada A, Watanabe S, Heat Treat, 1992; 32: 340) 6Cochart A W.J Appl Mech,1961; 15: 196 7Smith G W, Birchak J R. J Appl Phgs, 1968; 39: 2311 8Astie B, Dugaugue J.J Phys(Paris), 1981; 42: 627 9Lee K H, Vdovenko V A, Cho K K.J Korean Inst Met Mater 1994; 32: 1499 10冯端,王业宁,丘第荣.金属物理.第一版,北京:科学出版社,1964 (Feng D,Wang Y N,Qiu D R.Metal Physics.Beijing:Science Press,1964) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|